摘要
The creep behavior of an Al-8.5Fe-1.3V-1.7Si alloy processed by rapid solidification is investigated at three temperatures ranging from 623 to 723 K. The measured minimum creep strain rates cover seven orders of magnitude. The creep behavior is associated with the true threshold stress, decreasing with increasing temperature more strongly than the shear modulus of aluminum. The minimum creep strain rate is controlled by the lattice diffusion in the alloy matrix, and the true stress exponent is close to 5. The apparent activation energy of creep depends strongly on both applied stress and temperature and is generally much higher than the activation enthalpy of lattice self-diffusion in aluminum. Also, the apparent stress exponent of minimum creep strain rate depends on applied stress as well as on temperature and is generally much higher than the true stress exponent. This behavior of both the apparent activation energy and apparent stress exponent is accounted for by the strong temperature dependence of the threshold stress-to-shear modulus ratio. The true threshold creep behavior of the alloy is interpreted in terms of athermal detachment of dislocations from fine incoherent Al-12(Fe,V)(3)Si phase particles, admitting a temperature dependence of the relaxation factor characterizing the strength of the attractive dislocation/particle interaction.
引用
收藏
页码:2229 / 2237
页数:9
相关论文
共 50 条
  • [31] Elevated temperature mechanical properties of Al-8.5Fe-1.3V-1.7Si/SiCP composite prepared by multi-layer spray deposition
    He, Yiqiang
    Qiao, Bin
    Feng, Lichao
    FRONTIER OF NANOSCIENCE AND TECHNOLOGY, 2011, 694 : 708 - 712
  • [32] Structure, properties and fracture of friction stir welds in a high-temperature Al-8.5Fe-1.3V–1.7Si alloy (AA-8009)
    W. A. Baeslack
    K. V. Jata
    T. J. Lienert
    Journal of Materials Science, 2006, 41 : 2939 - 2951
  • [33] Al-8.5Fe-1.3V-1.7Si/SiCP复合材料热加工工艺的研究
    徐政坤
    贺毅强
    陈振华
    尹显觉
    郝亮
    热加工工艺, 2007, (10) : 17 - 20+24
  • [34] SiCP/Al-8.5Fe-1.3V-1.7Si composites prepared by multi-layer spray co-deposition
    He, Yiqiang
    Fuhe Cailiao Xuebao/Acta Materiae Compositae Sinica, 2012, 29 (02): : 109 - 114
  • [35] 快凝Al-8.5Fe-1.3V-1.7Si合金高温下的相稳定性
    曾欲晓,黎文献,李松瑞,肖于德
    中南工业大学学报, 1996, (04)
  • [36] 喷射沉积SiCP/Al-8.5Fe-1.3V-1.7Si热暴露过程的显微组织演变
    贺毅强
    屠宏
    冯立超
    杨建明
    陈振华
    航空材料学报, 2012, 32 (05) : 54 - 59
  • [37] Tribological properties improvement of conventionally-cast Al-8.5Fe-1.3V-1.7Si alloy by multi-pass friction stir processing
    Nouri, Z.
    Taghiabadi, R.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2021, 31 (05) : 1262 - 1275
  • [38] Transition from athermal to thermally activated detachment of dislocations from small incoherent particles in creep of an Al-8.5Fe-1.3V-1.7Si alloy reinforced with silicon carbide particulates
    Cadek, J
    Kucharová, K
    Zhu, SJ
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 297 (1-2): : 176 - 184
  • [39] Threshold stress and load transfer effects in creep of an Al-9.5Fe-1.3V-1.7Si alloy reinforced with silicon carbide particulates-an Al-8.5Fe-1.3V-1.7Si-15SiCp composite
    Cadek, J
    Kucharová, K
    Zhu, SJ
    INTERNATIONAL JOURNAL OF MATERIALS & PRODUCT TECHNOLOGY, 2003, 18 (1-3): : 178 - 198
  • [40] 锻造对喷射成形Al-8.5Fe-1.3V-1.7Si合金组织和性能的影响
    张荣华
    刘雅政
    张永安
    朱宝宏
    王锋
    稀有金属, 2006, (02) : 255 - 258