共 50 条
Biomechanical Study in Polyurethane Mandibles of Different Metal Plates and Internal Fixation Techniques, Employed in Mandibular Angle Fractures
被引:4
|作者:
Semeghini Guastaldi, Fernando Pozzi
[1
]
Hochuli-Vieira, Eduardo
[2
]
Guastaldi, Antonio Carlos
[3
]
机构:
[1] Sao Paulo State Univ, Aracatuba Dent Sch, Dept Surg & Integrated Clin, Sao Paulo, Brazil
[2] Araraquara Dent, Dept Diag & Surg, Sao Paulo, Brazil
[3] Sao Paulo State Univ, Inst Chem Araraquara, Dept Phys Chem, Sao Paulo, Brazil
关键词:
Mandible;
fracture fixation;
internal;
bone plates;
titanium;
molybdenum;
TI-MO ALLOYS;
PLATING TECHNIQUES;
IN-VITRO;
BIOMEDICAL APPLICATIONS;
RIGID FIXATION;
STABILITY;
MINIPLATE;
REPAIR;
SYSTEM;
MODEL;
D O I:
10.1097/SCS.0000000000001157
中图分类号:
R61 [外科手术学];
学科分类号:
摘要:
The aim of this study was to perform a physicochemical and morphological characterization and compare the mechanical behavior of an experimental Ti-Mo alloy to the analogous metallic Ti-based fixation system, for mandibular angle fractures. Twenty-eight polyurethane mandibles were uniformly sectioned on the left angle. These were divided into 4 groups: group Eng 1P, one 2.0-mm plate and 4 screws 6 mm long; group Eng 2P, two 2.0-mm plates, the first fixed with 4 screws 6 mm long and the second with 4 screws 12 mm long. The same groups were created for the Ti-15Mo alloy. Each group was subjected to linear vertical loading at the first molar on the plated side in a mechanical testing unit. Means and standard deviations were compared with respect to statistical significance using ANOVA. The chemical composition of the Ti-15Mo alloy was close to the nominal value. The mapping of Mo and Ti showed a homogeneous distribution. SEM of the screw revealed machining debris. For the plates, only the cpTi plate undergoes a surface treatment. The metallographic analysis reveals granular microstructure, from the thermomechanical trials. A statistically significant difference was found (P < 0.05) when the comparison between both internal fixation techniques was performed. The 2P technique showed better mechanical behavior than 1P.
引用
收藏
页码:2246 / 2250
页数:5
相关论文