Effect of microstructure on fracture behavior of freestanding plasma sprayed 7 wt.% Y2O3 stabilized ZrO2

被引:10
|
作者
Lal, Devi [1 ]
Kumar, Praveen [1 ]
Bathe, Ravi [2 ]
Sampath, Sanjay [3 ]
Jayaram, Vikram [1 ]
机构
[1] Indian Inst Sci, Mat Engn, Bangalore 56012, Karnataka, India
[2] Int Adv Res Ctr Powder Met & New Mat ARCI, Ctr Laser Proc Mat, Hyderabad 50005, India
[3] SUNY Stony Brook, Ctr Thermal Spray Res, Stony Brook, NY 11790 USA
关键词
Air plasma spray; Yttria-stabilized zirconia; Fracture; Crack tortuosity; Microstructure-fracture relationship; THERMAL-BARRIER COATINGS; TOUGHNESS; YSZ; CONDUCTIVITY; PERFORMANCE; DEPOSITS;
D O I
10.1016/j.jeurceramsoc.2021.02.038
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Air plasma sprayed (APS) 7 wt.% yttria-stabilized zirconia (7YSZ) coatings have a multitude of microstructural defects, at various length scales, such as pores, intra-splat and inter-splat micro-cracks, which cumulatively affect the mechanical properties and fracture behavior of the material. This microstructure is also susceptible to changes including sintering during high temperature operation. The kinetics of ?healing? of these microstructural defects are widely different, such that the smallest defects heal at significantly lower temperatures and in shorter periods. Here, the effect of thermal exposure-induced change in the microstructure on the fracture behavior, in terms of crack path and apparent fracture energy, of free-standing APS 7YSZ has been examined using miniaturized cantilever samples. Femto-second laser ablation technique was used to fabricate a sharp notch in the sample. Apparent fracture toughness in Mode I increased with the bending modulus of the material, revealing a monotonic effect of the density, which directly affects the modulus of the coating, on the overall fracture resistance of the coating. The relative density, crack tortuosity and the average apparent fracture energy of the as-deposited coating were 0.82, 2.1 and 62 ? 15 J/m2, respectively, which evolved to 0.94, 1.2 and 170 ? 30 J/ m2, respectively, after a heat treatment at 1300 ?C for 100 h. The detailed microstructural characterization and fractography revealed that the healing of inter-splat and intra-splat cracks led to the transition from fracture along the splat interface to quasi-cleavage fracture through the splats, thereby increasing the fracture resistance of these coatings toward monolithic fully-dense 7YSZ. The work readily reveals the relative importance of defects at various length scales on the overall energy absorbed during fracture of the coating.
引用
收藏
页码:4294 / 4301
页数:8
相关论文
共 50 条
  • [21] Metastable phase formation in plasma-sprayed ZrO2 (Y2O3)-Al2O3
    Zhou, XZ
    Shukla, V
    Cannon, WR
    Kear, BH
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2003, 86 (08) : 1415 - 1420
  • [22] Effect of heat-treatment on stress relaxation behavior of plasma-sprayed 7 wt.% Y2O3-ZrO2 stand-alone coatings
    Petorak, Christopher
    Trice, Rodney W.
    SURFACE & COATINGS TECHNOLOGY, 2011, 205 (10): : 3218 - 3225
  • [23] Preparation and properties of Y2O3 partially stabilized ZrO2 crystals
    M. A. Borik
    M. A. Vishnyakova
    V. P. Voitsitskii
    A. V. Kulebyakin
    E. E. Lomonova
    V. A. Myzina
    V. V. Osiko
    V. A. Panov
    Inorganic Materials, 2007, 43 : 1223 - 1229
  • [24] Preparation and properties of Y2O3 partially stabilized ZrO2 crystals
    Borik, M. A.
    Vishnyakova, M. A.
    Voitsitskii, V. P.
    Kulebyakin, A. V.
    Lomonova, E. E.
    Myzina, V. A.
    Osiko, V. V.
    Panov, V. A.
    INORGANIC MATERIALS, 2007, 43 (11) : 1223 - 1229
  • [26] SINTERING OF GRANULAR MASSES OF ZRO2 STABILIZED WITH CAO AND Y2O3
    KARAULOV, AG
    RUDYAK, IN
    INORGANIC MATERIALS, 1977, 13 (06) : 867 - 872
  • [27] INFLUENCE OF TRANSPARENCY AND GRINDING ON THE THERMAL-DIFFUSIVITY OF PLASMA SPRAYED ZRO2 WITH 8WT.PERCENT Y2O3 COATINGS
    RUDAJEVOVA, A
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1992, 151 (01): : L23 - L26
  • [28] Design of 7 wt.% Y2O3-ZrO2/mullite plasma-sprayed composite coatings for increased creep resistance
    Withey, Elizabeth
    Petorak, Christopher
    Trice, Rodney
    Dickinson, Graeme
    Taylor, Thomas
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (16) : 4675 - 4683
  • [29] W-2 wt.%Y2O3 composite: Microstructure and mechanical properties
    Battabyal, M.
    Schaeublin, R.
    Spaetig, P.
    Baluc, N.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 538 : 53 - 57
  • [30] Sintering densification, microstructure and transformation behavior of Al2O3/ZrO2(Y2O3) composites
    Ma Weimin
    Wen Lei
    Guan Renguo
    Sun Xudong
    Li Xikun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 477 (1-2): : 100 - 106