Effect of microstructure on fracture behavior of freestanding plasma sprayed 7 wt.% Y2O3 stabilized ZrO2

被引:10
|
作者
Lal, Devi [1 ]
Kumar, Praveen [1 ]
Bathe, Ravi [2 ]
Sampath, Sanjay [3 ]
Jayaram, Vikram [1 ]
机构
[1] Indian Inst Sci, Mat Engn, Bangalore 56012, Karnataka, India
[2] Int Adv Res Ctr Powder Met & New Mat ARCI, Ctr Laser Proc Mat, Hyderabad 50005, India
[3] SUNY Stony Brook, Ctr Thermal Spray Res, Stony Brook, NY 11790 USA
关键词
Air plasma spray; Yttria-stabilized zirconia; Fracture; Crack tortuosity; Microstructure-fracture relationship; THERMAL-BARRIER COATINGS; TOUGHNESS; YSZ; CONDUCTIVITY; PERFORMANCE; DEPOSITS;
D O I
10.1016/j.jeurceramsoc.2021.02.038
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Air plasma sprayed (APS) 7 wt.% yttria-stabilized zirconia (7YSZ) coatings have a multitude of microstructural defects, at various length scales, such as pores, intra-splat and inter-splat micro-cracks, which cumulatively affect the mechanical properties and fracture behavior of the material. This microstructure is also susceptible to changes including sintering during high temperature operation. The kinetics of ?healing? of these microstructural defects are widely different, such that the smallest defects heal at significantly lower temperatures and in shorter periods. Here, the effect of thermal exposure-induced change in the microstructure on the fracture behavior, in terms of crack path and apparent fracture energy, of free-standing APS 7YSZ has been examined using miniaturized cantilever samples. Femto-second laser ablation technique was used to fabricate a sharp notch in the sample. Apparent fracture toughness in Mode I increased with the bending modulus of the material, revealing a monotonic effect of the density, which directly affects the modulus of the coating, on the overall fracture resistance of the coating. The relative density, crack tortuosity and the average apparent fracture energy of the as-deposited coating were 0.82, 2.1 and 62 ? 15 J/m2, respectively, which evolved to 0.94, 1.2 and 170 ? 30 J/ m2, respectively, after a heat treatment at 1300 ?C for 100 h. The detailed microstructural characterization and fractography revealed that the healing of inter-splat and intra-splat cracks led to the transition from fracture along the splat interface to quasi-cleavage fracture through the splats, thereby increasing the fracture resistance of these coatings toward monolithic fully-dense 7YSZ. The work readily reveals the relative importance of defects at various length scales on the overall energy absorbed during fracture of the coating.
引用
收藏
页码:4294 / 4301
页数:8
相关论文
共 50 条
  • [11] Electron microscopy and diffraction studies of suspension-plasma-sprayed ZrO2+8 wt.% Y2O3 coatings
    Podlesak, Harry
    Latka, Leszek
    Dietrich, Dagmar
    Pawlowski, Lech
    Wielage, Bernhard
    Lampke, Thomas
    SURFACE & COATINGS TECHNOLOGY, 2013, 220 : 67 - 73
  • [12] COMPRESSIVE CREEP OF PLASMA-SPRAYED Y2O3-STABILIZED ZRO2
    FIRESTONE, RF
    LOGAN, WR
    TAYLOR, TA
    BILL, RC
    AMERICAN CERAMIC SOCIETY BULLETIN, 1979, 58 (03): : 357 - 357
  • [13] Nanophase decomposition in plasma sprayed ZrO2(Y2O3)/Al2O3 coatings
    Liu, FD
    Cosandey, F
    Zhou, XZ
    Kear, BH
    CERAMIC NANOMATERIALS AND NANOTECHNOLOGY II, 2004, 148 : 91 - 100
  • [14] Analysis of tensile strength of Y2O3 stabilized ZrO2
    Nakayama, Y
    Kakita, S
    ADVANCES IN ENGINEERING PLASTICITY, PTS 1-2, 2000, 177-1 : 467 - 472
  • [15] THERMAL-DIFFUSIVITY OF PLASMA-SPRAYED COATINGS OF ZRO2 WITH 8 WT-PERCENT Y2O3 AND ZRO2 WITH 25 WT-PERCENT CEO2
    RUDAJEVOVA, A
    THIN SOLID FILMS, 1993, 223 (02) : 248 - 252
  • [17] Influence of Plasma Spray Parameters on the Microstructure and Property of ZrO2-7 wt%Y2O3 Coating
    Li Hui
    Wang Benpeng
    Wei Qi
    Ji Xiaojian
    Li Zhuoxin
    RARE METAL MATERIALS AND ENGINEERING, 2012, 41 : 291 - 295
  • [18] Effect of Microstructure on the Thermal Conductivity of Plasma Sprayed Y2O3 Stabilized Zirconia (8% YSZ)
    Hu, Ningning
    Khan, Matiullah
    Wang, Yongzhe
    Song, Xuemei
    Lin, Chucheng
    Chang, Chengkang
    Zeng, Yi
    COATINGS, 2017, 7 (11):
  • [19] Microstructure and fracture behaviour of ZrO2 (2 mol% Y2O3) reinforced with SiC whiskers
    F Ye
    T. C Lei
    Y. C Zhao
    Y Zhou
    Journal of Materials Science, 1997, 32 : 3249 - 3255
  • [20] Yttria stabilized zirconia solid electrolyte surface modification with ZrO2, Y2O3, and ZrO2 + 9 mol % Y2O3 films
    L. A. Dunyushkina
    A. I. Vshivkova
    A. A. Pankratov
    B. D. Antonov
    V. P. Gorelov
    Russian Journal of Electrochemistry, 2010, 46 : 767 - 773