Comparison between microwave and conventional sintering of WC/Co composites

被引:192
|
作者
Breval, E [1 ]
Cheng, JP
Agrawal, DK
Gigl, P
Dennis, A
Roy, R
Papworth, AJ
机构
[1] Penn State Univ, Mat Res Inst, University Pk, PA 16802 USA
[2] Dennis Tool Co, Houston, TX USA
[3] Univ Liverpool, Dept Engn & Mfg, Liverpool L693 GHG, Merseyside, England
关键词
microwave sintering; tungsten carbide; cobalt binder; microstructure; properties;
D O I
10.1016/j.msea.2004.08.085
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
WC/Co samples sintered in a microwave field differ radically in terms of phases, chemistry, and microstructure when compared with conventionally sintered samples. Microstructural investigations by TEM showed that in microwave sintered material the cobalt phase dissolved nearly no tungsten, whereas in conventionally sintered samples up to 20 wt.% tungsten was dissolved in the cobalt binder phase. Besides, smaller WC grains and finer and more uniform distribution of cobalt binder were observed in microwave sintered samples. This resulted in a harder material, which also exhibited better resistance towards both corrosion and erosion. Microwave sintered samples also have a three-dimensional uniform shrinkage, whereas conventionally sintered samples showed a greater vertical shrinkage. It is possible to microwave sinter WC/Co at lower surface temperature and in much shorter times than normally needed in a conventional furnace to obtain the same degree of densification. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:285 / 295
页数:11
相关论文
共 50 条
  • [31] Comparison Study in Consolidation of Yttria Reinforced Iron-Chromium Composites using Conventional and Microwave Sintering Technique
    Marina, M.
    Zamzuri, M. Z. M.
    Derman, M. N.
    Selamat, M. A.
    Nooraizedfiza, Z.
    ADVANCED MATERIALS ENGINEERING AND TECHNOLOGY II, 2014, 594-595 : 832 - +
  • [32] Skin effect of WC-8 wt% Co alloy by microwave sintering
    Bao, Rui
    Yi, Jian-Hong
    Peng, Yuan-Dong
    Li, Feng-Xian
    Li, Shang
    Li, Shao-Yu
    RARE METALS, 2022, 41 (04) : 1364 - 1368
  • [33] Skin effect of WC-8 wt% Co alloy by microwave sintering
    Rui Bao
    Jian-Hong Yi
    Yuan-Dong Peng
    Feng-Xian Li
    Shang Li
    Shao-Yu Li
    Rare Metals, 2022, 41 (04) : 1364 - 1368
  • [34] Comparison between Microwave and Microwave Plasma Sintering of Nickel Powders
    Breen, Aidan P.
    Twomey, Barry
    Byrne, Greg
    Dowling, Denis P.
    RESEARCHES IN POWDER METALLURGY, 2011, 672 : 289 - 292
  • [35] Spark plasma sintering of Co-WC cubic boron nitride composites
    Yaman, Bilge
    Mandal, Hasan
    MATERIALS LETTERS, 2009, 63 (12) : 1041 - 1043
  • [36] Spark Plasma Sintering of Fine-Grained WC-Co Composites
    Wachowicz, Joanna
    Dembiczak, Tomasz
    Fik, Joanna
    Balaga, Zbigniew
    Kruzel, Robert
    Naprstkova, Natasa
    Kusmierczak, Sylvia
    MATERIALS, 2023, 16 (24)
  • [37] Conventional sintering of WC with nano-sized Co binder: Characterization and mechanical behavior
    Raihanuzzaman, Rumman Md.
    Han, Seung-Taek
    Ghomashchi, Reza
    Kim, Hyo-Seob
    Hong, Soon-Jik
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2015, 53 : 2 - 6
  • [38] Sintering of WC-Co powder with nanocrystalline WC by spark plasma sintering
    O. Van der Biest
    J. Vleugels
    Rare Metals, 2006, (03) : 246 - 252
  • [39] Sintering of WC-Co powder with nanocrystalline WC by spark plasma sintering
    Wang Xingqing
    Xie Yingang
    Guo Hailiang
    Van der Biest, O.
    Vleuge, J.
    RARE METALS, 2006, 25 (03) : 246 - 252
  • [40] The effect of microwave sintering on the properties of electroless Ni plated WC-Fe-Ni composites
    Yönetken, Ahmet
    Erol, Ayhan
    Science and Engineering of Composite Materials, 2010, 17 (03): : 191 - 198