Skin effect of WC-8 wt% Co alloy by microwave sintering

被引:8
|
作者
Bao, Rui [1 ,2 ]
Yi, Jian-Hong [1 ,2 ]
Peng, Yuan-Dong [2 ]
Li, Feng-Xian [1 ]
Li, Shang [1 ]
Li, Shao-Yu [1 ]
机构
[1] Kunming Univ Sci & Technol, Sch Mat Sci & Engn, Kunming 650093, Yunnan, Peoples R China
[2] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
基金
中国国家自然科学基金;
关键词
Microwave sintering; Tungsten carbide; Microstructure; Solubility; Skin effect; MECHANICAL-PROPERTIES; TUNGSTEN CARBIDE; DENSIFICATION; POWDERS; FE;
D O I
10.1007/s12598-015-0488-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To investigate the microwave effect on the WC-Co alloys, WC-8 wt% Co alloy was fabricated by microwave sintering (MWS) in this paper. The results show that decarburization layer forms on the surface of the microwave-sintered samples. WC grain coarsening in the core area is strongly suppressed by the decarburization effect. In addition, the microstructure of the MWS-fabricated alloy was compared to that of the alloy sintered by vacuum sintering (VS). Microstructural investigations by transmission electron microscopy (TEM) and energy dispersive spectroscopy (EDS) show that more tungsten (29.50 wt%) is dissolved in the cobalt binder phase in microwave-sintered alloy than that in the vacuum-sintered samples. Finally, the formation mechanism of the surface layer by skin effect was discussed.
引用
收藏
页码:1364 / 1368
页数:5
相关论文
共 50 条
  • [1] Skin effect of WC-8 wt% Co alloy by microwave sintering
    Rui Bao
    Jian-Hong Yi
    Yuan-Dong Peng
    Feng-Xian Li
    Shang Li
    Shao-Yu Li
    Rare Metals, 2022, 41 (04) : 1364 - 1368
  • [2] Skin effect of WC–8 wt% Co alloy by microwave sintering
    Rui Bao
    Jian-Hong Yi
    Yuan-Dong Peng
    Feng-Xian Li
    Shang Li
    Shao-Yu Li
    Rare Metals, 2022, 41 : 1364 - 1368
  • [3] Densification and alloying of microwave sintering WC-8 wt.%Co composites
    Bao, Rui
    Yi, Jianhong
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2014, 43 : 269 - 275
  • [4] Effect of WC nanoparticle size on the sintering temperature, density, and microhardness of WC-8 wt % Co alloys
    Kurlov, A. S.
    Rempel, A. A.
    INORGANIC MATERIALS, 2009, 45 (04) : 380 - 385
  • [5] Effect of WC nanoparticle size on the sintering temperature, density, and microhardness of WC-8 wt % Co alloys
    A. S. Kurlov
    A. A. Rempel
    Inorganic Materials, 2009, 45 : 380 - 385
  • [6] Effect of sintering temperature on the phase composition and microhardness of WC-8 wt % Co cemented carbide
    A. S. Kurlov
    A. A. Rempel’
    Inorganic Materials, 2007, 43 : 602 - 607
  • [7] Effect of sintering temperature on the phase composition and microhardness of WC-8 wt % co cemented carbide
    Kurlov, A. S.
    Rempel, A. A.
    INORGANIC MATERIALS, 2007, 43 (06) : 602 - 607
  • [8] Vacuum sintering of WC-8 wt.% Co hardmetals from WC powders with different dispersity
    Kurlov, A. S.
    Gusev, A. I.
    Rempel, A. A.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2011, 29 (02): : 221 - 231
  • [9] Fabrication of WC-8 wt.%Co hard materials by two rapid sintering processes
    Kim, Hwan Cheol
    Jeong, In Kyoon
    Shon, In Jin
    Ko, In Yong
    Doh, Jung Mann
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2007, 25 (04): : 336 - 340
  • [10] Effect of sintering atmosphere on microwave prepared WC-8wt.%Co cemented carbide
    Bao, Rui
    Yi, Jianhong
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2013, 41 : 315 - 321