Skin effect of WC-8 wt% Co alloy by microwave sintering

被引:8
|
作者
Bao, Rui [1 ,2 ]
Yi, Jian-Hong [1 ,2 ]
Peng, Yuan-Dong [2 ]
Li, Feng-Xian [1 ]
Li, Shang [1 ]
Li, Shao-Yu [1 ]
机构
[1] Kunming Univ Sci & Technol, Sch Mat Sci & Engn, Kunming 650093, Yunnan, Peoples R China
[2] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
基金
中国国家自然科学基金;
关键词
Microwave sintering; Tungsten carbide; Microstructure; Solubility; Skin effect; MECHANICAL-PROPERTIES; TUNGSTEN CARBIDE; DENSIFICATION; POWDERS; FE;
D O I
10.1007/s12598-015-0488-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To investigate the microwave effect on the WC-Co alloys, WC-8 wt% Co alloy was fabricated by microwave sintering (MWS) in this paper. The results show that decarburization layer forms on the surface of the microwave-sintered samples. WC grain coarsening in the core area is strongly suppressed by the decarburization effect. In addition, the microstructure of the MWS-fabricated alloy was compared to that of the alloy sintered by vacuum sintering (VS). Microstructural investigations by transmission electron microscopy (TEM) and energy dispersive spectroscopy (EDS) show that more tungsten (29.50 wt%) is dissolved in the cobalt binder phase in microwave-sintered alloy than that in the vacuum-sintered samples. Finally, the formation mechanism of the surface layer by skin effect was discussed.
引用
收藏
页码:1364 / 1368
页数:5
相关论文
共 50 条
  • [41] Microwave sintering of nanocrystalline WC-12Co: Challenges and perspectives
    Sunil, B. Ratna
    Sivaprahasam, D.
    Subasri, R.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2010, 28 (02): : 180 - 186
  • [42] Preparation of WC-10Co cemented carbide by microwave sintering
    Shi, Xiao-Liang
    Yang, Hua
    Shao, Gang-Qin
    Duan, Xing-Long
    Xiong, Zhen
    Yi, Zhong-Lai
    Zhongnan Daxue Xuebao (Ziran Kexue Ban)/Journal of Central South University (Science and Technology), 2006, 37 (04): : 665 - 669
  • [43] Gelcasting of WC-8wt%Co tungsten cemented carbide
    Li, Yan
    Guo, Zhimeng
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2008, 26 (05): : 472 - 477
  • [44] Cold Isostatic Pressing Effect on the WC-15 wt.% Co Hard Alloy Strength
    Sheremet, V. I.
    Akimov, G. Ya.
    Andreev, I. V.
    Trosnikova, I. Yu.
    Loboda, P. I.
    STRENGTH OF MATERIALS, 2024, 56 (03) : 551 - 558
  • [45] INFLUENCE OF PROCESS VARIABLES ON SINTERING OF WC-25 WT-PERCENT CO
    LEE, JW
    JAFFREY, D
    BROWNE, JD
    POWDER METALLURGY, 1980, 23 (02) : 57 - 64
  • [46] Preparation and sintering of WC-Co composite powders for coarse grained WC-8Co hardmetals
    Su, Wei
    Sun, Yexi
    Wang, Huifeng
    Zhang, Xianqi
    Ruan, Jianming
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2014, 45 : 80 - 85
  • [47] Effect of the sintering parameters on the liquid Co migration in WC-Co
    Emanuelli, L.
    Molinari, A.
    Arrighetti, G.
    Garoli, G.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2018, 70 : 202 - 209
  • [48] 低压烧结温度对WC-8%Co硬质合金性能影响的研究
    辛海艳
    吴翔
    稀有金属与硬质合金, 2015, 43 (03) : 54 - 56+66
  • [49] 不同粒度WC配比对WC-8%Co-4%Ni硬质合金组织与性能影响
    阳建宏
    杨开明
    刘海军
    夏艳萍
    汤郡
    龙坚战
    硬质合金, 2022, 39 (01) : 37 - 42
  • [50] Influence of the process temperature of spark plasma sintering on micorsturcture and nanoindentation hardness/Young's modulus of WC-8wt%Co
    Zhang, Jianfeng
    Burkel, Eberhard
    ADVANCED CERAMICS AND NOVEL PROCESSING, 2014, 616 : 56 - 61