Monitoring thermo-oxidative degradation of polypropylene by CRYSTAF and SEC-FTIR

被引:11
|
作者
de Goede, S
Brüll, R
Pasch, H
Marshall, N
机构
[1] SASOL Polymers, ZA-1645 Modderfontein, South Africa
[2] German Inst Polymers, D-64289 Darmstadt, Germany
[3] Schumann SASOL, ZA-1947 Sasolburg, South Africa
关键词
D O I
10.1002/masy.200390062
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Samples of a polypropylene homopolymer have been degraded and analysed with regard to chemical composition, molecular weight distribution and chemical composition distribution. FTIR shows the progress of degradation and a decrease in molecular weight can be observed from SEC. CRYSTAF shows that the chemical heterogeneity of the samples broadens with continuing degradation. SEC-FTIR reveals that the degraded species are mainly found in the low molecular end of the molecular weight distribution. The spatial heterogeneity of the degradation process has been proven by the analysis of abrased layers.
引用
收藏
页码:35 / 43
页数:9
相关论文
共 50 条
  • [41] THERMO-OXIDATIVE DEGRADATION OF FATS - METHYLOLEATE AS AN EXAMPLE
    LECKER, G
    INDUSTRIE ALIMENTARI, 1983, 22 (06): : 498 - 498
  • [42] Thermo-oxidative degradation of polypropylene by selective labeling and 13C NMR spectroscopy.
    Assink, RA
    Derzon, DK
    Clough, RL
    Mowery, D
    Bernstein, R
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2003, 226 : U378 - U378
  • [43] THERMO-OXIDATIVE DEGRADATION OF ISOTACTIC POLYPROPYLENE FILM - STRUCTURAL-CHANGES AND ITS CORRELATION WITH PROPERTIES
    MATHUR, AB
    MATHUR, GN
    POLYMER, 1982, 23 (01) : 54 - 56
  • [44] Kinetics of thermo-oxidative degradation of polypropylene/aluminum trihydroxide/organo Fe-montmorillonite nanocomposites
    Qinghong Kong
    Yuan Hu
    Lei Song
    Yuwen Tang
    Journal of Thermal Analysis and Calorimetry, 2011, 104 : 1145 - 1151
  • [45] Kinetics of thermo-oxidative degradation of polypropylene/aluminum trihydroxide/organo Fe-montmorillonite nanocomposites
    Kong, Qinghong
    Hu, Yuan
    Song, Lei
    Tang, Yuwen
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2011, 104 (03) : 1145 - 1151
  • [46] Influence of polypropylene and nanoclay on thermal and thermo-oxidative degradation of poly(lactide acid): TG-FTIR, TG-DSC studies and kinetic analysis
    Karimpour-Motlagh, Navid
    Khonakdar, Hossein Ali
    Jafari, Seyed Mohammad Ali
    Mahjub, Alireza
    Panahi-Sarmad, Mahyar
    Kasbi, Sina Farahani
    Shojaei, Shahrokh
    Goodarzi, Vahabodin
    Arjmand, Mohammad
    THERMOCHIMICA ACTA, 2020, 691
  • [47] The impact of cupric ion on thermo-oxidative degradation of chitosan
    Ou, Chun-Yan
    Li, Si-Dong
    Yang, Lei
    Li, Cheng-Peng
    Hong, Peng-Zhi
    She, Xiao-Dong
    POLYMER INTERNATIONAL, 2010, 59 (08) : 1110 - 1115
  • [48] Thermo-oxidative degradation during sintering of polyethylene particles
    Pircheraghi, Gholamreza (pircheraghi@sharif.ir), 1600, John Wiley and Sons Inc (138):
  • [49] Thermo-oxidative degradation during sintering of polyethylene particles
    Salehi, Amirmehdi
    Pircheraghi, Gholamreza
    JOURNAL OF APPLIED POLYMER SCIENCE, 2021, 138 (19)
  • [50] Thermo-oxidative Degradation of Natural Rubber Coagulated by Microorganisms
    Liao, Shuang-Quan
    She, Xiao-Dong
    Li, Si-Dong
    Zhong, Jie-Ping
    Yang, Lei
    He, Can-Zhong
    JOURNAL OF POLYMER MATERIALS, 2010, 27 (04): : 303 - 311