摘要
Samples of a polypropylene homopolymer have been degraded and analysed with regard to chemical composition, molecular weight distribution and chemical composition distribution. FTIR shows the progress of degradation and a decrease in molecular weight can be observed from SEC. CRYSTAF shows that the chemical heterogeneity of the samples broadens with continuing degradation. SEC-FTIR reveals that the degraded species are mainly found in the low molecular end of the molecular weight distribution. The spatial heterogeneity of the degradation process has been proven by the analysis of abrased layers.
引用
收藏
页码:35 / 43
页数:9
相关论文
共 50 条
  • [22] Mechanism of thermo-oxidative degradation of polyamide
    Li, RF
    Hu, XZ
    ACTA POLYMERICA SINICA, 2000, (02) : 136 - 141
  • [23] Pyrolysis and thermo-oxidative degradation of polycyclopentadiene
    Radhakrishnan, TS
    JOURNAL OF APPLIED POLYMER SCIENCE, 2000, 76 (05) : 635 - 641
  • [24] CHARACTERIZATION OF POLYESTERS - THERMO-OXIDATIVE DEGRADATION
    UGLEA, C
    CORDUNEANU, I
    NEGULESCU, I
    MONATSHEFTE FUR CHEMIE, 1984, 115 (03): : 349 - 356
  • [25] Monitoring thermo-oxidative degradation in elastomers by NMR relaxation measurements.
    Assink, RA
    Lang, DP
    Celina, M
    Sanderson, B
    Gillen, KT
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2001, 221 : U330 - U330
  • [26] Monitoring the chemical heterogeneity of metallocene-catalysed copolymers of ethylene and higher 1-olefins using CRYSTAF and SEC-FTIR -: art. no. 005
    Graef, SM
    Brüll, R
    Pasch, H
    Wahner, UM
    E-POLYMERS, 2003,
  • [27] Long term thermo-oxidative degradation and stabilization of polypropylene (PP) and the implications for its recyclability
    Gijsman, Pieter
    Fiorio, Rudinei
    POLYMER DEGRADATION AND STABILITY, 2023, 208
  • [28] The influence of thermo-oxidative degradation on the measured interface strength of glass fibre-polypropylene
    Yang, L.
    Thomason, J. L.
    Zhu, W.
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2011, 42 (10) : 1293 - 1300
  • [29] Thermo-oxidative degradation of isotactic polypropylene at high temperatures: phenolic antioxidants versus HAS
    Gensler, R
    Plummer, CJG
    Kausch, HH
    Kramer, E
    Pauquet, JR
    Zweifel, H
    POLYMER DEGRADATION AND STABILITY, 2000, 67 (02) : 195 - 208
  • [30] The thermo-oxidative stability and flammability of wood/polypropylene composites
    Slawomir Borysiak
    Journal of Thermal Analysis and Calorimetry, 2015, 119 : 1955 - 1962