Study on the acoustic and thermal response characteristics of coal samples with various prefabricated crack angles during loaded failure under uniaxial compression

被引:23
|
作者
Li, Zhonghui [1 ,2 ,3 ]
Tian, He [1 ,2 ]
Niu, Yue [1 ,2 ]
Wang, Enyuan [1 ,2 ]
Zhang, Xin [1 ,2 ]
He, Shun [1 ,2 ]
Wang, Fengzhi [1 ,2 ]
Zheng, Anqi [1 ,2 ]
机构
[1] China Univ Min & Technol, Key Lab Coal Mine Gas & Fire Prevent & Control, Minist Educ, Xuzhou 221116, Jiangsu, Peoples R China
[2] China Univ Min & Technol, Sch Safety Engn, Xuzhou 221116, Jiangsu, Peoples R China
[3] China Univ Min & Technol, State Key Lab Coal Resources & Safe Min, Xuzhou 221116, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
Prefabricated crack; Angle; Mechanical properties; Failure mode; Infrared radiation; Acoustic emission; ROCK; COALESCENCE; FRACTURE; FIELD;
D O I
10.1016/j.jappgeo.2022.104618
中图分类号
P [天文学、地球科学];
学科分类号
07 ;
摘要
In this study, uniaxial compression tests were conducted on coal samples with different-angle prefabricated cracks. Based on the test results, the effects of prefabricated crack angles on the mechanical properties, failure modes and acoustic and thermal characteristics of the samples during loaded failure were analyzed. The following research results were obtained: the prefabricated crack angle significantly influences the mechanical properties of coal samples. Both the peak stress and the peak strain increase with the increase of the prefabricated crack angle, and the relationships between them and the prefabricated crack angle satisfy quadratic functions. The fracture types of prefabricated fracture coal samples are wing-shaped cracks, inverse wing-shaped cracks and split fracture. For example, when alpha=90 degrees, the coal sample experiences splitting failure. The infrared radiation temperature (IRT) and acoustic emission (AE) responses exhibit obviously distinct characteristics in different stages. The states of crack propagation in the loaded failure process can be clearly obtained by means of infrared thermal images and AE location. With the increase of the prefabricated crack angle, the change in average infrared radiation temperature and the peak AE counts vary in a similar trend, both decreasing first and increasing later.
引用
收藏
页数:10
相关论文
共 50 条
  • [21] Acoustic emission fractal characteristics of different prefabricated fractured sandstone under uniaxial compression tests
    Deng, Min
    Zhang, Zizheng
    Xin, Jinlin
    Yu, Weijian
    Yu, Xianyang
    GEOTECHNICAL AND GEOLOGICAL ENGINEERING, 2021, 39 (04) : 3161 - 3170
  • [22] Acoustic emission fractal characteristics of different prefabricated fractured sandstone under uniaxial compression tests
    Min Deng
    Zizheng Zhang
    Jinlin Xin
    Weijian Yu
    Xianyang Yu
    Geotechnical and Geological Engineering, 2021, 39 : 3161 - 3170
  • [23] Acoustic emission characteristics of thermal cracking of marble under uniaxial compression
    Zhai, S.-T. (zhaisongtao@sjtu.edu.cn), 2013, Chinese Society of Civil Engineering (35):
  • [24] Experimental study of charge induction of coal samples under uniaxial compression
    Zhao, Yangfeng
    Pan, Yishan
    Liu, Yuchun
    Luo, Hao
    Yanshilixue Yu Gongcheng Xuebao/Chinese Journal of Rock Mechanics and Engineering, 2011, 30 (02): : 306 - 312
  • [25] Experimental Study on Creep Characteristics of Coal Under Uniaxial Compression
    Yang, Yongjie
    Guo, Mingfu
    Chen, Dongwei
    ADVANCES IN INDUSTRIAL AND CIVIL ENGINEERING, PTS 1-4, 2012, 594-597 : 290 - +
  • [26] Acoustic Emission Waveform Characteristics of Red Sandstone Failure under Uniaxial Compression after Thermal Damage
    Zhang, Herui
    Guo, Weihong
    SUSTAINABILITY, 2022, 14 (20)
  • [27] Study on acoustic-electric-heat effect of coal and rock failure processes under uniaxial compression
    Li, Zhong-Hui
    Lou, Quan
    Wang, En-Yuan
    Liu, Shuai-Jie
    Niu, Yue
    JOURNAL OF GEOPHYSICS AND ENGINEERING, 2018, 15 (01) : 71 - 80
  • [28] Discrete element study on mesomechanical behavior of crack propagation in coal samples with two prefabricated fissures under biaxial compression
    Xu, Hao
    Qin, Yueping
    Wang, Gang
    Fan, Cheng
    Wu, Mengmeng
    Wang, Rui
    POWDER TECHNOLOGY, 2020, 375 (375) : 42 - 59
  • [29] Crack Propagation and AE/EMR Response Characteristics of Pre-Holed Coal Specimens under Uniaxial Compression
    Feng, Xiaojun
    Hu, Qinjing
    Ding, Zeng
    Wang, Dongming
    Zhao, Xue
    Wei, Qilei
    SUSTAINABILITY, 2022, 14 (22)
  • [30] Failure characteristics and the law of the energy evolution of granite with different pre-crack inclination angles under uniaxial compression loading
    Zhao, Ercheng
    Li, Juhong
    Zhang, Xiongtian
    Zhang, Chunyang
    Ren, Qinglin
    Tan, Tao
    Wang, Yixian
    FRONTIERS IN EARTH SCIENCE, 2023, 11