Study on the acoustic and thermal response characteristics of coal samples with various prefabricated crack angles during loaded failure under uniaxial compression

被引:23
|
作者
Li, Zhonghui [1 ,2 ,3 ]
Tian, He [1 ,2 ]
Niu, Yue [1 ,2 ]
Wang, Enyuan [1 ,2 ]
Zhang, Xin [1 ,2 ]
He, Shun [1 ,2 ]
Wang, Fengzhi [1 ,2 ]
Zheng, Anqi [1 ,2 ]
机构
[1] China Univ Min & Technol, Key Lab Coal Mine Gas & Fire Prevent & Control, Minist Educ, Xuzhou 221116, Jiangsu, Peoples R China
[2] China Univ Min & Technol, Sch Safety Engn, Xuzhou 221116, Jiangsu, Peoples R China
[3] China Univ Min & Technol, State Key Lab Coal Resources & Safe Min, Xuzhou 221116, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
Prefabricated crack; Angle; Mechanical properties; Failure mode; Infrared radiation; Acoustic emission; ROCK; COALESCENCE; FRACTURE; FIELD;
D O I
10.1016/j.jappgeo.2022.104618
中图分类号
P [天文学、地球科学];
学科分类号
07 ;
摘要
In this study, uniaxial compression tests were conducted on coal samples with different-angle prefabricated cracks. Based on the test results, the effects of prefabricated crack angles on the mechanical properties, failure modes and acoustic and thermal characteristics of the samples during loaded failure were analyzed. The following research results were obtained: the prefabricated crack angle significantly influences the mechanical properties of coal samples. Both the peak stress and the peak strain increase with the increase of the prefabricated crack angle, and the relationships between them and the prefabricated crack angle satisfy quadratic functions. The fracture types of prefabricated fracture coal samples are wing-shaped cracks, inverse wing-shaped cracks and split fracture. For example, when alpha=90 degrees, the coal sample experiences splitting failure. The infrared radiation temperature (IRT) and acoustic emission (AE) responses exhibit obviously distinct characteristics in different stages. The states of crack propagation in the loaded failure process can be clearly obtained by means of infrared thermal images and AE location. With the increase of the prefabricated crack angle, the change in average infrared radiation temperature and the peak AE counts vary in a similar trend, both decreasing first and increasing later.
引用
收藏
页数:10
相关论文
共 50 条
  • [11] Acoustic emission response characteristics and numerical simulation of soil failure under uniaxial compression
    Li, Xiangchun
    Li, Yi
    Yang, Chunli
    Zhang, Liang
    Li, Zhongbei
    Huang, Tao
    JOURNAL OF APPLIED GEOPHYSICS, 2024, 222
  • [12] Experimental study on crack propagation process and macroscopic failure mode of prefabricated-crack fine sandstone under uniaxial compression
    Yang D.
    Zhang D.
    Niu S.
    Ge S.
    Liu S.
    Chen X.
    Wang T.
    Li X.
    Caikuang yu Anquan Gongcheng Xuebao/Journal of Mining and Safety Engineering, 2019, 36 (04): : 786 - 793
  • [13] Characteristics of self-potential of coal samples under uniaxial compression
    Yang, Cai
    Liu, Shengdong
    Liu, Jing
    Yang, Haiping
    Xie, Jingyan
    JOURNAL OF APPLIED GEOPHYSICS, 2019, 168 : 1 - 11
  • [14] Experimental Study on Infrared Temperature Characteristics and Failure Modes of Marble with Prefabricated Holes under Uniaxial Compression
    Peng, Yanyan
    Lin, Qunchao
    He, Manchao
    Zhu, Chun
    Zhang, Haijiang
    Guo, Pengfei
    ENERGIES, 2021, 14 (03)
  • [15] Study of the Acoustic Characteristics and Evolution of the Failure Mode of Yellow Sandstone Under Uniaxial Compression
    Li, Shijie
    Huang, Zhen
    Yang, Daoxue
    Zeng, Wei
    Zhao, Kui
    ROCK MECHANICS AND ROCK ENGINEERING, 2024, 57 (02) : 1059 - 1078
  • [16] Study of the Acoustic Characteristics and Evolution of the Failure Mode of Yellow Sandstone Under Uniaxial Compression
    Shijie Li
    Zhen Huang
    Daoxue Yang
    Wei Zeng
    Kui Zhao
    Rock Mechanics and Rock Engineering, 2024, 57 : 1059 - 1078
  • [17] Study of Strength and Deformation Evolution in Raw and Briquette Coal Samples under Uniaxial Compression via Monitoring Their Acoustic Emission Characteristics
    Meng, Han
    Yang, Yuzhong
    Wu, Liyun
    Wang, Fei
    Peng, Lei
    ADVANCES IN CIVIL ENGINEERING, 2020, 2020
  • [18] Investigation of the acoustic emission and fractal characteristics of coal with varying water contents during uniaxial compression failure
    Ali, Muhammad
    Wang, Enyuan
    Li, Zhonghui
    Khan, Naseer Muhammad
    Sabri, Mohanad Muayad Sabri
    Ullah, Barkat
    SCIENTIFIC REPORTS, 2023, 13 (01):
  • [19] Investigation of the acoustic emission and fractal characteristics of coal with varying water contents during uniaxial compression failure
    Muhammad Ali
    Enyuan Wang
    Zhonghui Li
    Naseer Muhammad Khan
    Mohanad Muayad Sabri Sabri
    Barkat Ullah
    Scientific Reports, 13 (1)
  • [20] Influence of heterogeneity on the failure characteristics of coal under uniaxial compression condition
    Song H.
    Zhao Y.
    Jiang Y.
    Zhang X.
    Meitan Xuebao/Journal of the China Coal Society, 2017, 42 (12): : 3125 - 3132