Rail rolling contact fatigue formation and evolution with surface defects

被引:47
|
作者
Zhang, S. Y. [1 ,2 ]
Spiryagin, M. [2 ]
Ding, H. H. [1 ]
Wu, Q. [2 ]
Guo, J. [1 ]
Liu, Q. Y. [1 ]
Wang, W. J. [1 ]
机构
[1] Southwest Jiaotong Univ, Tribol Res Inst, State Key Lab Tract Power, Chengdu 610031, Peoples R China
[2] Cent Queensland Univ, Ctr Railway Engn, Rockhampton, Qld, Australia
基金
中国国家自然科学基金; 澳大利亚研究理事会;
关键词
Surface defect; Rolling contact fatigue; Microstructure evolution; Critical size; WHITE ETCHING LAYER; MICROSTRUCTURE EVOLUTION; CRACK-PROPAGATION; SQUAT FORMATION; BEHAVIOR;
D O I
10.1016/j.ijfatigue.2022.106762
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Surface defects can induce serious rolling contact fatigue (RCF) damage at wheel/rail interfaces and even cause fracture failure of rail material. This study aims to explore the formation mechanism of surface defects on rails, and to trace the evolution process of RCF behavior of material around the surface defect. Experimental studies were conducted on a wheel/rail twin-disc machine considering two forms of defects: indentation defects caused by ballast impacts (IDBs) and indentation defects caused by cone penetration head impacts (IDCs). Results indicate that IDB can cause RCF cracks that propagate downward deep into the subsurface of rail due to the formation of a material hardening layer (MHL), causing severe damage. IDCs with different sizes and angles were grouped into an affected group and a non-affected group by considering a critical size dividing line and whether the MHLs existed on the defect surface or not. The evolution process of a crack in the affected group includes four main periods: fracture of the MHL, crack initiation, the rail steel matrix filling up the MHL gap and crack propagation downward. Further, the increase in both the angle and the depth of the IDC would lead to severe RCF damage.
引用
收藏
页数:13
相关论文
共 50 条
  • [21] Evolution of rail rolling contact fatigue on heavy-haul curves and treatment optimization
    Zhang, Xin
    Zhao, Xin
    Peng, Feng
    Li, Jinwei
    Zhang, Kai
    Li, Tao
    Journal of Railway Science and Engineering, 2024, 21 (08) : 3153 - 3165
  • [22] Effects of dent size on the evolution process of rolling contact fatigue damage on defective rail
    Zhang, S. Y.
    Zhao, X. J.
    Ding, H. H.
    Spiryagin, M.
    Guo, J.
    Liu, Q. Y.
    Wang, W. J.
    Zhou, Z. R.
    WEAR, 2021, 477
  • [23] Rail rolling contact fatigue research by the European Rail Research Institute
    British Rail Research, Derby, United Kingdom
    Wear, 1-2 (1-13):
  • [24] Rail rolling contact fatigue - Research by the European Rail Research Institute
    Cannon, DF
    Pradier, H
    WEAR, 1996, 191 (1-2) : 1 - 13
  • [25] Impact of wheel profile evolution on wheel-rail dynamic interaction and surface initiated rolling contact fatigue in turnouts
    Chen, Rong
    Chen, Jiayin
    Wang, Ping
    Fang, Jiasheng
    Xu, Jingmang
    WEAR, 2019, 438
  • [26] Overview of phenomena rolling contact fatigue of wheel/rail
    Jin, Xuesong
    Zhang, Jiye
    Wen, Zefeng
    Li, Fu
    Journal of Mechanical Strength, 2002, 24 (02)
  • [27] Effect of Liquid on Rolling Contact Fatigue Cracks in Rail
    Zhou Y.
    Wang Z.
    Lu Z.
    Li J.
    Tongji Daxue Xuebao/Journal of Tongji University, 2022, 50 (02): : 253 - 263
  • [28] Effect of wheel/rail friction on rolling contact fatigue
    Wang Jianxi
    Xiao Wei
    Zhang Xiaodong
    MATERIALS SCIENCE AND ENGINEERING APPLICATIONS, PTS 1-3, 2011, 160-162 : 1636 - +
  • [29] FAILURE PREDICTION OF RAIL CONSIDERING ROLLING CONTACT FATIGUE
    Patra, Ambika Prasad
    Bidhar, Sujit
    Kumar, Uday
    INTERNATIONAL JOURNAL OF RELIABILITY QUALITY AND SAFETY ENGINEERING, 2010, 17 (03) : 167 - 177
  • [30] Rolling contact fatigue assessment of repair rail welds
    Kabo, Elena
    Ekberg, Anders
    Maglio, Michele
    WEAR, 2019, 436