Deformation and Corrosion Behavior of A High Purity Manganese Free AZ31 Magnesium Alloy

被引:1
|
作者
Kakutani, Eigo [1 ]
Jotoku, Masahiro [1 ]
Yamamoto, Atsushi [2 ]
Tsubakino, Harushige [2 ]
机构
[1] Univ Hyogo, Materials Sci & Chem, 2167 Shosha, Himeji, Hyogo 6712201, Japan
[2] Univ Hyogo, Grad Sch Engn, Himeji, Hyogo 6712201, Japan
来源
关键词
recrystallization; cold-rolling; low impurity; magnesium alloy; AZ31; alloy; room temperature; corrosion resistance; TEM;
D O I
10.4028/www.scientific.net/AMR.26-28.1283
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A low impurity magnesium alloy has bean prepared. Deformation behavior in cold-rolling and corrosion behavior of the alloy were compared with those of a commercial alloy. The specimens were cold-rolled at room temperature with reduction rates of 0 similar to 80 %. Transmission electron microscopic observations on the cold-rolled specimens were carried out. In the case of the low impurity magnesium alloy, recrystallization easily occurred. Analyses of microstructures in the deformed specimens were carried out by means of EBSP, and the recrystallization phenomena have been discussed. Another effect of lowering the impurities is to improve a corrosion resistance with changing the corrosion morphology.
引用
收藏
页码:1283 / +
页数:5
相关论文
共 50 条
  • [41] Hot deformation behavior of a spray-deposited AZ31 magnesium alloy
    LI Yongbinga
    RareMetals, 2009, 28 (01) : 91 - 97
  • [42] Influence of Grain Orientation on the Corrosion Behavior of Rolled AZ31 Magnesium Alloy
    Yan-Chun Zhao
    Guang-Sheng Huang
    Guan-Gang Wang
    Ting-Zhuang Han
    Fu-Sheng Pan
    Acta Metallurgica Sinica(English Letters), 2015, 28 (11) : 1387 - 1393
  • [43] Corrosion behavior of AZ31 magnesium alloy in simulated acid rain solution
    Liu Feng
    Song Ying-wei
    Shan Da-yong
    Han En-hou
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 : S638 - S642
  • [44] Influence of Grain Orientation on the Corrosion Behavior of Rolled AZ31 Magnesium Alloy
    Yan-Chun Zhao
    Guang-Sheng Huang
    Guan-Gang Wang
    Ting-Zhuang Han
    Fu-Sheng Pan
    Acta Metallurgica Sinica (English Letters), 2015, 28 : 1387 - 1393
  • [45] Adsorption and Corrosion Inhibition Behavior of Sodium Dodecylbenzenesulfonate on AZ31 Magnesium Alloy
    Li Ling-Jie
    Yao Zhi-Ming
    Lei Jing-Lei
    Xu Hui
    Zhang Sheng-Tao
    Pan Fu-Sheng
    ACTA PHYSICO-CHIMICA SINICA, 2009, 25 (07) : 1332 - 1336
  • [46] Deformation behavior of AZ31 magnesium alloy at different strain rates and temperatures
    谭成文
    胥珊娜
    王鲁
    陈志永
    王富耻
    才鸿年
    马红磊
    TransactionsofNonferrousMetalsSocietyofChina, 2007, (S1) : 347 - 352
  • [47] Corrosion and degradation behavior of MCSTE-Processed AZ31 magnesium alloy
    Abdelfattah, Khaled B.
    Abbas, Marwa A.
    El-Garaihy, Waleed H.
    Mohamed, Adel M. A.
    Salem, Hanadi G.
    SCIENTIFIC REPORTS, 2025, 15 (01):
  • [48] Hot deformation behavior of a spray-deposited AZ31 magnesium alloy
    Li Yongbing
    Chen Yunbo
    Cui Hua
    Ding Jie
    Zuo Lingli
    Zhang Jishan
    RARE METALS, 2009, 28 (01) : 91 - 97
  • [49] Isochronal annealing behavior of magnesium alloy AZ31 after hot deformation
    Yang, XY
    Miura, H
    Sakai, T
    MATERIALS TRANSACTIONS, 2005, 46 (12) : 2981 - 2987
  • [50] Deformation Behavior of AZ31 Magnesium Alloy During Tension at Moderate Temperatures
    Junwei Liu
    Ding Chen
    Zhenhua Chen
    Hongge Yan
    Journal of Materials Engineering and Performance, 2009, 18 : 966 - 972