Deformation and Corrosion Behavior of A High Purity Manganese Free AZ31 Magnesium Alloy

被引:1
|
作者
Kakutani, Eigo [1 ]
Jotoku, Masahiro [1 ]
Yamamoto, Atsushi [2 ]
Tsubakino, Harushige [2 ]
机构
[1] Univ Hyogo, Materials Sci & Chem, 2167 Shosha, Himeji, Hyogo 6712201, Japan
[2] Univ Hyogo, Grad Sch Engn, Himeji, Hyogo 6712201, Japan
来源
关键词
recrystallization; cold-rolling; low impurity; magnesium alloy; AZ31; alloy; room temperature; corrosion resistance; TEM;
D O I
10.4028/www.scientific.net/AMR.26-28.1283
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A low impurity magnesium alloy has bean prepared. Deformation behavior in cold-rolling and corrosion behavior of the alloy were compared with those of a commercial alloy. The specimens were cold-rolled at room temperature with reduction rates of 0 similar to 80 %. Transmission electron microscopic observations on the cold-rolled specimens were carried out. In the case of the low impurity magnesium alloy, recrystallization easily occurred. Analyses of microstructures in the deformed specimens were carried out by means of EBSP, and the recrystallization phenomena have been discussed. Another effect of lowering the impurities is to improve a corrosion resistance with changing the corrosion morphology.
引用
收藏
页码:1283 / +
页数:5
相关论文
共 50 条
  • [21] Corrosion Behavior of AZ31 Magnesium Alloy in Highly Alkaline Environment
    Doja, Somi
    Bichler, Lukas
    Fan, Simon
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2017, 30 (04) : 367 - 375
  • [22] Cavitation behavior during superplastic deformation of AZ31 magnesium alloy
    Zhang, KF
    Yin, DL
    Wang, GF
    Han, WB
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2005, 21 (04) : 510 - 514
  • [23] Corrosion Behavior of AZ31 Magnesium Alloy in Highly Alkaline Environment
    Somi Doja
    Lukas Bichler
    Simon Fan
    ActaMetallurgicaSinica(EnglishLetters), 2017, 30 (04) : 367 - 375
  • [24] Constitutive Analysis for Superplasic Deformation Behavior of AZ31 Magnesium Alloy
    Lee, H. S.
    Bang, W.
    Kim, D. W.
    Semiatin, S. L.
    Chang, Y. W.
    THERMEC 2006 SUPPLEMENT: 5TH INTERNATIONAL CONFERENCE ON PROCESSING AND MANUFACTURING OF ADVANCED MATERIALS, 2007, 15-17 : 507 - 512
  • [25] Corrosion Behavior of AZ31 Magnesium Alloy in Highly Alkaline Environment
    Somi Doja
    Lukas Bichler
    Simon Fan
    Acta Metallurgica Sinica (English Letters), 2017, 30 : 367 - 375
  • [26] The high strain rate deformation behavior of high purity magnesium and AZ31B magnesium alloy
    Livescu, Veronica
    Cady, Carl M.
    Cerreta, Ellen K.
    Henrie, Benjamin L.
    Gray, George T., III
    MAGNESIUM TECHNOLOGY 2006, PROCEEDINGS, 2006, : 153 - +
  • [27] Surface modification of AZ31 magnesium alloy by deposition coating with high purity magnesium
    Fukumoto, S
    Sugahara, K
    Yamamoto, A
    Tsubakino, H
    PROCESSING AND FABRICATION OF ADVANCED MATERIALS XI, 2003, : 360 - 370
  • [28] CYCLIC DEFORMATION RESPONSE OF AZ31 MAGNESIUM ALLOY AFTER CORROSION DEGRADATION
    Dolezal, Pavel
    Zapletal, Josef
    Horynova, Miroslava
    Gejdos, Pavel
    Celko, Ladislav
    CHEMICKE LISTY, 2011, 105 : S787 - S789
  • [29] High temperature deformation and microstructural instability in AZ31 magnesium alloy
    Spigarelli, S.
    Ruano, O. A.
    El Mehtedi, M.
    del Valle, J. A.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 570 : 135 - 148
  • [30] High temperature deformation Behavior of AZ31 Mg alloy
    Lee, BH
    Shin, KS
    Lee, CS
    PRICM 5: THE FIFTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, PTS 1-5, 2005, 475-479 : 2927 - 2930