Fatigue behavior of Y-TZP ceramic after surface treatments

被引:39
|
作者
Amaral, Marina [1 ]
Cesar, Paulo Francisco [2 ]
Bottino, Marco Antonio [1 ]
Lohbauer, Ulrich [3 ]
Valandro, Luiz Felipe [4 ]
机构
[1] Sao Paulo State Univ, Sch Dent, Dept Dent Mat & Prosthesis, Ave Eng Franscisco Jose Longo, Sao Jose Dos Campos, Brazil
[2] Univ Sao Paulo, Sch Dent, Dept Dent Mat, Ave Prof Lineu Prestes 2227, Sao Paulo, Brazil
[3] Univ Erlangen Nurnberg, Dent Clin Operat Dent & Periodontol 1, Lab Biomat Res, Gluedstr 11, Erlangen, Germany
[4] Univ Fed Santa Maria, Prosthodont Unit, Sch Dent, Dept Restorat Dent, Rua Marechal Floriano Peixoto 1184, BR-97015372 Santa Maria, RS, Brazil
基金
巴西圣保罗研究基金会;
关键词
Zirconia ceramic; Fatigue; Surface treatments; Strength; Weibul analysis; DENTAL CERAMICS; ZIRCONIA CERAMICS; TETRAGONAL ZRO2; HEAT-TREATMENT; BOND STRENGTH; TRANSFORMATION; RESTORATIONS; SYSTEMS; CROWNS;
D O I
10.1016/j.jmbbm.2015.11.042
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Objectives: The aim of this study was to evaluate the effect of three surface treatments on the biaxial flexural strength before and after mechanical cycling, and fatigue limit of a Y-TZP ceramic. Methods: Disc-shaped specimens were produced and three surface conditions were tested: CT (as-sintered, untreated), GL (thin layer of porcelain glaze), and AA (air abrasion with 30 mu m silica particles). Profilometric and phase transformation analyses were performed. Disks were submitted to biaxial flexural strength (BFS) before and after mechanical cycling (100 N, 2 x 10(6) cycles) and staircase approach (n=20). The flexural fatigue limits (FFLs) were obtained at 10(2), 10(3), 10(4) and 10(5) cycles. Results: Tetragonal to monoclinic transformation was only observed for AA group (9.46% of monoclinic phase). Glazed group presented the highest Ra values. Flexural strength was higher for AA group; CT and GL groups were similar. The reliability was similar between groups. The mechanical cycling at 100 N did not affected flexural strength. FFLs were higher for AA group, and the three surface treatments presented decrease in strength according to the increase in number o cycles. (C) 2015 Elsevier Ltd. All rights reserved.
引用
下载
收藏
页码:149 / 156
页数:8
相关论文
共 50 条
  • [31] Fracture of a Y-TZP ceramic femoral head
    Maccauro, G
    Piconi, C
    Burger, W
    Pilloni, L
    De Santis, E
    Muratori, E
    Learmonth, ID
    JOURNAL OF BONE AND JOINT SURGERY-BRITISH VOLUME, 2004, 86B (08): : 1192 - 1196
  • [32] The effect of surface treatment on the friction and wear behavior of dental Y-TZP ceramic against human enamel
    Buciumeanu, M.
    Queiroz, J. R. C.
    Martinelli, A. E.
    Silva, F. S.
    Henriques, B.
    TRIBOLOGY INTERNATIONAL, 2017, 116 : 192 - 198
  • [33] Damage and Reliability of Y-TZP after Cementation Surface Treatment
    Guess, P. C.
    Zhang, Y.
    Kim, J. -W.
    Rekow, E. D.
    Thompson, V. P.
    JOURNAL OF DENTAL RESEARCH, 2010, 89 (06) : 592 - 596
  • [34] Wear behavior of dental Y-TZP ceramic against natural enamel after different finishing procedures
    Mitov, Gergo
    Heintze, Siegward D.
    Walz, Stephanie
    Woll, Karsten
    Muecklich, Frank
    Pospiech, Peter
    DENTAL MATERIALS, 2012, 28 (08) : 909 - 918
  • [35] Efficacy of Surface Roughness and Bond Strength of Y-TZP Zirconia After Various Pre-Treatments
    Kirmali, Omer
    Kustarci, Alper
    Kapdan, Alper
    Er, Kursat
    PHOTOMEDICINE AND LASER SURGERY, 2015, 33 (01) : 15 - 21
  • [36] Effect of surface topography and wettability on shear bond strength of Y-TZP ceramic
    Suriyakul Wongsue
    Ornnicha Thanatvarakorn
    Taweesak Prasansuttiporn
    Piyarat Nimmanpipug
    Thanapat Sastraruji
    Keiichi Hosaka
    Richard M. Foxton
    Masatoshi Nakajima
    Scientific Reports, 13
  • [37] Effect of surface topography and wettability on shear bond strength of Y-TZP ceramic
    Wongsue, Suriyakul
    Thanatvarakorn, Ornnicha
    Prasansuttiporn, Taweesak
    Nimmanpipug, Piyarat
    Sastraruji, Thanapat
    Hosaka, Keiichi
    Foxton, Richard M.
    Nakajima, Masatoshi
    SCIENTIFIC REPORTS, 2023, 13 (01)
  • [38] LCMAS glass-ceramic /Y-TZP composite
    Zhang, Yufeng
    Yang, Hanmei
    Guo, Jingkun
    Wuji Cailiao Xuebao/Journal of Inorganic Materials, 1994, 9 (02): : 156 - 160
  • [39] Low temperature degradation of a Y-TZP dental ceramic
    Cattani-Lorente, Maria
    Scherrer, Susanne S.
    Ammann, Patrick
    Jobin, Marc
    Wiskott, H. W. Anselm
    ACTA BIOMATERIALIA, 2011, 7 (02) : 858 - 865
  • [40] Fatigue Resistance of Y-TZP/Porcelain Crowns is Not Influenced by the Conditioning of the Intaglio Surface
    Anami, L. C.
    Lima, J. M. C.
    Valandro, L. F.
    Kleverlaan, C. J.
    Feilzer, A. J.
    Bottino, M. A.
    OPERATIVE DENTISTRY, 2016, 41 (01) : E1 - E12