Low temperature degradation of a Y-TZP dental ceramic

被引:174
|
作者
Cattani-Lorente, Maria [1 ]
Scherrer, Susanne S. [1 ]
Ammann, Patrick [2 ]
Jobin, Marc [3 ]
Wiskott, H. W. Anselm [1 ]
机构
[1] Univ Geneva, Sch Dent, Lab Biomat, CH-1205 Geneva, Switzerland
[2] Univ Geneva, HUG, Fac Med, Div Bone Dis, CH-1211 Geneva 14, Switzerland
[3] Univ Appl Sci Western Switzerland, EPIA, CH-1202 Geneva, Switzerland
关键词
Zirconia; Low temperature degradation; Tetragonal-to-monoclinic transformation; Dental ceramics; Mechanical properties; ATOMIC-FORCE MICROSCOPY; MONOCLINIC PHASE-TRANSFORMATION; TETRAGONAL ZIRCONIA; STABILIZED ZIRCONIA; MARTENSITIC-TRANSFORMATION; MECHANICAL-PROPERTIES; HYDROTHERMAL DEGRADATION; AGING SENSITIVITY; ZRO2; POLYCRYSTALS; FLEXURAL STRENGTH;
D O I
10.1016/j.actbio.2010.09.020
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Bars of Y-TZP ceramic for dental restorations were subjected to hydrothermal degradation via in vitro exposure to water steam at 140 degrees C for 7 days. X-ray diffraction, atomic force microscopy and scanning electron microscopy techniques were applied to observe and quantify the tetragonal-monoclinic (t-m) phase transformation associated with the process. Nanoindentation was used to assess the ceramic's mechanical properties before and after hydrothermal degradation. Texture associated with martensitic t-m transformation was observed at the grain surface. The t-m transformation followed nucleation-and-growth kinetics, with predominance of the nucleation process. The transformation occurred within a layer of 6 gm below the surface. Mechanical properties deteriorated with hydrothermal degradation, resulting in a 30% reduction of Young's modulus and hardness. A strong correlation was found between the increasing monoclinic fraction and the decline in mechanical response. It was thus concluded that the emergence of the monoclinic phase and the associated microcracking were the most likely causes for the degradation of mechanical properties. (C) 2010 Published by Elsevier Ltd. on behalf of Acta Materialia Inc.
引用
收藏
页码:858 / 865
页数:8
相关论文
共 50 条
  • [1] Low Temperature Degradation of Y-TZP Ceramic for Dental Applications
    Wu, Zhi-kai
    Li, Ning
    Zhao, Wan-qian
    Yan, Jia-zhen
    EIGHTH CHINA NATIONAL CONFERENCE ON FUNCTIONAL MATERIALS AND APPLICATIONS, 2014, 873 : 241 - 249
  • [2] Low-temperature degradation of a Y-TZP ceramic after surface treatments
    Amaral, Marina
    Valandro, Luiz Felipe
    Bottino, Marco A.
    Souza, Rodrigo O. A.
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2013, 101 (08) : 1387 - 1392
  • [3] LOW-TEMPERATURE DEGRADATION OF Y-TZP MATERIALS
    SWAB, JJ
    JOURNAL OF MATERIALS SCIENCE, 1991, 26 (24) : 6706 - 6714
  • [4] The effect of a high strength electric field on the low temperature degradation of a Y-TZP ceramic
    Zhao, ZB
    Liu, C
    Northwood, DO
    27TH INTERNATIONAL COCOA BEACH CONFERENCE ON ADVANCED CERAMICS AND COMPOSITES: B, 2003, 24 (04): : 163 - 168
  • [5] LOW TEMPERATURE DEGRADATION AND BIOMEDICAL PROPERTIES OF Y-TZP CERAMICS
    Tanaka, Yumi
    Ukai, Nami
    Nishio, Keishi
    Yamashita, Kimihiro
    ADVANCES IN BIOCERAMICS AND POROUS CERAMICS, 2009, 29 (07): : 239 - +
  • [6] Effect of Copper Oxide and Manganese Oxide on Properties and Low Temperature Degradation of Sintered Y-TZP Ceramic
    M. M. Khan
    S. Ramesh
    L. T. Bang
    Y. H. Wong
    S. Ubenthiran
    C. Y. Tan
    J. Purbolaksono
    H. Misran
    Journal of Materials Engineering and Performance, 2014, 23 : 4328 - 4335
  • [7] Effect of Copper Oxide and Manganese Oxide on Properties and Low Temperature Degradation of Sintered Y-TZP Ceramic
    Khan, M. M.
    Ramesh, S.
    Bang, L. T.
    Wong, Y. H.
    Ubenthiran, S.
    Tan, C. Y.
    Purbolaksono, J.
    Misran, H.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2014, 23 (12) : 4328 - 4335
  • [8] Influence of relative humidity and low temperature hydrothermal degradation on fretting wear of Y-TZP dental ceramics
    Borrell, Amparo
    Gil, Lorena
    Presenda, Alvaro
    Salvador, Maria D.
    Vleugels, Jozef
    Moreno, Rodrigo
    WEAR, 2019, 428 : 1 - 9
  • [9] Study on preparation of Y-TZP ceramic matrix for dental prosthesis
    Xi'an Jiaotong University, Xi'an 710049, China
    不详
    Xiyou Jinshu Cailiao Yu Gongcheng, 2007, 2 (313-317): : 313 - 317
  • [10] Study on preparation of Y-TZP ceramic matrix for dental prosthesis
    Yang Sefei
    Jin Zhihao
    Guo Tianwen
    RARE METAL MATERIALS AND ENGINEERING, 2007, 36 (02) : 313 - 317