Fusion Welding of T23 and T91 Steel Joints for Advanced Thermal Power Plant Application

被引:2
|
作者
Chatterjee, Suvam [1 ]
Mondal, Manas Kumar [1 ]
Maity, Joydeep [1 ]
机构
[1] Natl Inst Technol Durgapur, Dept Met & Mat Engn, Durgapur 713209, W Bengal, India
关键词
failure analysis; fusion welding; high strength and reasonable ductility; high-temperature tensile test; T23 to T91 joining; HEAT-TREATMENT; MECHANICAL-PROPERTIES; WELDED-JOINTS; P91; STEEL; MICROSTRUCTURE;
D O I
10.1007/s11665-021-05884-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The unresolved decisive aspect of joining T23 steel to T91 steel in a supercritical boiler is hereby taken up with reasonable success by adopting a cost-effective GTAW process with an iron-based filler wire (ER90S-B9). Quite a reasonable joint strength (UTS = 319 MPa) coupled with a considerable ductility (%elongation = 8) is ascertained by carrying out tensile test at boiler operation temperature (571 degrees C), known as one of the most critical tasks; and subsequently performing advanced characterization keeping all the significant regions of the weldment intact. Being pushed along with grain boundary sliding, Cr23C6 particles are clustered around the cavity evolved therein under tensile load applied at the boiler service temperature. The dimples originated through microvoid coalescence in the soft alpha-ferrite matrix eventually negate the cleavage mode of failure initiated at the segregated Cr23C6 particles around cavity so as to maintain a considerable level of ductility. Furthermore, the defect accumulation in the form of dislocation wall around Cr23C6 particle appears to be responsible for providing significant high-temperature strength so as to justify the success of the adopted joining route.
引用
收藏
页码:7655 / 7667
页数:13
相关论文
共 50 条
  • [21] Welding performance analysis of ultra (ultra) supercritical thermal power units T91 and TP347H
    Zheng, Kai
    Xu, Desheng
    Zhang, Xuelian
    Xie, Fang
    Hanjie Xuebao/Transactions of the China Welding Institution, 2010, 31 (06): : 53 - 55
  • [22] INFLUENCE OF THE ANNEALING TIME AFTER WELDING ON THE MECHANICAL PROPERTIES OF WELDED JOINT OF T91 STEEL
    Wojsyk, K.
    Golanski, G.
    Jasak, J.
    Slania, J.
    Zielinski, A.
    Urbanczyk, P.
    ARCHIVES OF METALLURGY AND MATERIALS, 2016, 61 (03) : 1079 - 1083
  • [23] Aging Behavior of T91/10CrMo910 Dissimilar Steel Welded Joints
    Yao, Yuhong
    Wei, Jianfeng
    Liu, Jiangnan
    Wang, Zhengpin
    Jin, Yaohua
    ADVANCES IN SUPERALLOYS, PTS 1 AND 2, 2011, 146-147 : 156 - +
  • [24] T23、T91、TP347H钢管长时服役后的显微组织和拉伸性能
    郭赉佳
    谷树超
    段鹏
    丁宪飞
    王松
    刘宇哲
    机械工程材料, 2020, 44 (09) : 56 - 61+66
  • [25] T23和T91高温过热器短时超温爆管的组织性能分析
    史志刚
    马红
    崔雄华
    王飞
    王碧磊
    热力发电, 2014, (09) : 129 - 132
  • [26] Experimental Analysis of T23-T91 Dissimilar Steel Joining in Supercritical Boiler by a Cost-Effective Fusion Welding Route
    Chatterjee, Suvam
    Mondal, Manas Kumar
    Maity, Joydeep
    STEEL RESEARCH INTERNATIONAL, 2021, 92 (09)
  • [27] Influence of temperature on the oxide spallation of T91 alloy superheater tubes in power plant
    Qi, Jing
    Zhou, Keyi
    Huang, Junlin
    Si, Xiaodong
    APPLIED THERMAL ENGINEERING, 2018, 128 : 244 - 252
  • [28] Fireside corrosion degradation of 15Mo3, T22, T23 & T91 in simulated coal-biomass co-fired environment
    Dudziak, T.
    Hussain, T.
    Orlicka, D.
    Pokrywa, A.
    Simms, N. J.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2015, 66 (09): : 839 - 850
  • [29] Microstructures and Properties of Laser Hybrid Welded T91 Steel Joints after High Temperature Aging
    Hu Lianhai
    Liu Xiaolin
    Hou Debin
    Xu Changling
    Zhao Yang
    Fu Kun
    Wang Changcai
    CHINESE JOURNAL OF LASERS-ZHONGGUO JIGUANG, 2018, 45 (09):
  • [30] 长时服役后的T23管与T91新管焊接接头组织与性能研究
    李晋刚
    朱建强
    栾高灿
    景江峰
    夏咸喜
    张向前
    热加工工艺, 2023, 52 (09) : 66 - 71