Hydrogen embrittlement sensitivity of X100 pipeline steel under different pre-strain

被引:54
|
作者
Han, Y. D. [1 ,2 ]
Wang, R. Z. [1 ,2 ]
Wang, H. [1 ,2 ]
Xu, L. Y. [1 ,2 ,3 ]
机构
[1] Tianjin Univ, Sch Mat Sci & Engn, Tianjin 300072, Peoples R China
[2] Tianjin Key Lab Adv Joining Technol, Tianjin 300072, Peoples R China
[3] Tianjin Univ, State Key Lab Engines, Tianjin 300050, Peoples R China
基金
中国国家自然科学基金;
关键词
X100 pipeline steel; Pre-strain; Hydrogen embrittlement sensitivity; Hydrogen permeation; INDUCED CRACKING; BEHAVIOR; STRESS; MICROSTRUCTURE; TEXTURE; GROWTH; IRON;
D O I
10.1016/j.ijhydene.2019.06.054
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In the present study, the influences of hydrogen on the mechanical properties as well as the pre-strain on the HE susceptibility of X100 pipeline steel were investigated by combining electrochemical hydrogen charging and tensile experiments. Both the yield and tensile strength decrease with the increasing hydrogen charging time no matter the values of pre-strain. When the charging time is 12 h, the yield strength and tensile strength was reduced by 3% and 9%, respectively. The longer the charging time, the stronger the HE damage of the steel. Besides, when the hydrogen charging time is same, HE sensitivity increases with the pre-strain values. When the charging time is 6 h, the HE sensitivity coefficient is 40.24% without pre-strain, and it increases to 49.26% with the pre-strain value increases to the 2%. The hydrogen effective diffusion coefficient reduces gradually with the increasing pre-strain values. The coefficient is 5.45 x 10(-7) cm(2)/s without pre-strain and it reduces to 1.21 x 10(-7) cm(2)/s with the pre-strain value increases to the 3%. When the hydrogen charging time is same, HE sensitivity increases with the pre-strain values. (C) 2019 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:22380 / 22393
页数:14
相关论文
共 50 条
  • [21] Modeling the fatigue crack growth of X100 pipeline steel in gaseous hydrogen
    Amaro, Robert L.
    Rustagi, Neha
    Findley, Kip O.
    Drexler, Elizabeth S.
    Slifka, Andrew J.
    INTERNATIONAL JOURNAL OF FATIGUE, 2014, 59 : 262 - 271
  • [22] Characteristics of hydrogen embrittlement in high-pH stress corrosion cracking of X100 pipeline steel in carbonate/bicarbonate solution
    Song, Longfei
    Liu, Zhiyong
    Li, Xiaogang
    Du, Cuiwei
    CONSTRUCTION AND BUILDING MATERIALS, 2020, 263
  • [23] Characteristics of hydrogen embrittlement in high-pH stress corrosion cracking of X100 pipeline steel in carbonate/ bicarbonate solution
    Song L.
    Liu Z.
    Li X.
    Du C.
    Construction and Building Materials, 2020, 263
  • [24] Analysis of enhanced hydrogen embrittlement fracture for pre-strain hardening 2205 duplex stainless steel
    Tao, Ping
    Ye, Fei
    Cen, Weiwei
    Zhao, Jiaxi
    Wang, Yanfei
    Gong, Jianming
    RESULTS IN PHYSICS, 2020, 16
  • [25] Effect of pre-strain on susceptibility of Indian Reduced Activation Ferritic Martensitic Steel to hydrogen embrittlement
    Sonak, Sagar
    Tiwari, Abhishek
    Jam, Uttam
    Keskar, Nachiket
    Kumar, Sanjay
    Singh, Ram N.
    Dey, Gautam K.
    JOURNAL OF NUCLEAR MATERIALS, 2015, 465 : 78 - 82
  • [26] The Effect of Pre-Strain on the Resistance to Hydrogen Embrittlement in 316L Austenitic Stainless Steel
    Park, Il-Jeong
    Jung, Jae-Gil
    Jo, Seo Yeon
    Lee, Sang-Min
    Lee, Young-Kook
    MATERIALS TRANSACTIONS, 2014, 55 (06) : 964 - 970
  • [27] Investigation of hydrogen embrittlement behavior in X65 pipeline steel under different hydrogen charging conditions
    Wang, D.
    Hagen, A. B.
    Fathi, P. U.
    Lin, M.
    Johnsen, R.
    Lu, X.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 860
  • [28] Study on the weldability of X100 pipeline steel on scene
    Wang Pinyi
    Mou Zongyuan
    MATERIALS PROCESSING AND MANUFACTURING III, PTS 1-4, 2013, 753-755 : 343 - 352
  • [29] CTOA MEASUREMENTS OF WELDS IN X100 PIPELINE STEEL
    Drexler, Elizabeth
    Darcis, Philippe
    McCowan, Christopher
    Treinen, J. Matthew
    Shtechman, Avigdor
    Reuven, Rony
    Siewert, Thomas
    Smith, Robert
    Merritt, James
    McColskey, J. David
    IPC2008: PROCEEDINGS OF THE ASME INTERNATIONAL PIPELINE CONFERENCE - 2008, VOL 3, 2009, : 287 - 292
  • [30] Cold cracking susceptibility of X100 pipeline steel
    严春妍
    姜心怡
    元媛
    纪秀林
    张可召
    China Welding, 2019, 28 (03) : 25 - 33