CTOA MEASUREMENTS OF WELDS IN X100 PIPELINE STEEL

被引:0
|
作者
Drexler, Elizabeth [1 ]
Darcis, Philippe [1 ]
McCowan, Christopher [1 ]
Treinen, J. Matthew [1 ]
Shtechman, Avigdor [1 ]
Reuven, Rony [1 ]
Siewert, Thomas [1 ]
Smith, Robert
Merritt, James
McColskey, J. David [1 ]
机构
[1] NIST, Boulder, CO USA
关键词
SPECIMEN;
D O I
暂无
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
A suite of tests characterizing X100 pipeline steels was initiated at the National Institute of Standards and Technology (NIST) in Boulder. Part of the test matrix included testing the toughness of the base metal, welds, and heat-affected zones (HAZ) by use of modified double cantilever beam specimens for crack tip opening angle (CTOA) testing. The thickness of the test section was either 3 mm or 8 mm. Girth welds perpendicular to the growing crack, and seam welds and their HAZ parallel with the crack, were tested with a crosshead displacement rate of 0.02 mm/s (with the exception of one girth weld specimen for each thickness, which were tested at 0.002 mm/s). Analysis of the data revealed some general differences among the weld specimens. The tests where the crack ran perpendicular to the girth weld demonstrated changes in CTOA and crack growth rate as the crack moved through the base metal, HAZ, and weld material. We observed the values for CTOA increasing and the crack propagation slowing as the crack moved through the weld and approached the fusion line. The stress field appeared to be strongly influenced by the thin HAZ, the fusion line, and the tougher base material. Consequently, the CTOA of the HAZ associated with the girth weld was larger than that of the seam-weld HAZ. It was not possible to obtain CTOA data for the seam weld, with the crack parallel within the weld, because the crack immediately diverted out of the stronger weld material into the weaker HAZ. CTOA values from both girth welds and seam-weld HAZ were smaller than those of the base material. The 8 mm thick specimens consistently produced larger CTOA values than their 3 mm counterparts, introducing the possibility that there may be limitations to CTOA as a material property. Further tests are needed to determine whether a threshold thickness exists below which the constraints and stress field are sufficiently changed to affect the CTOA value.
引用
收藏
页码:287 / 292
页数:6
相关论文
共 50 条
  • [1] Ductile-Fracture Resistance in X100 Pipeline Welds Measured with CTOA
    Drexler, E.
    Darcis, P.
    McCowan, C. N.
    Sowards, J. W.
    McColskey, D.
    Siewert, T. A.
    [J]. WELDING JOURNAL, 2011, 90 (12) : 241S - 248S
  • [2] Characterization of fiber laser welds in X100 pipeline steel
    Miranda, R.
    Costa, A.
    Quintino, L.
    Yapp, D.
    Iordachescu, D.
    [J]. MATERIALS & DESIGN, 2009, 30 (07) : 2701 - 2707
  • [3] Recrystallization behavior of X100 pipeline steel
    Zhou, Feng
    Wu, Kai-Ming
    Kang, Yong-Lin
    Chen, Jian-Xin
    [J]. Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2015, 36 (06): : 121 - 125
  • [4] Assessment of properties and microstructure of X100 pipeline girth welds
    Gianetto J.A.
    Bowker J.T.
    Dorling D.V.
    [J]. Welding in the World, 2005, 49 (11-12) : 77 - 89
  • [5] Anisotropic Behavior of X100 Pipeline Steel
    Treinen, J. Matthew
    Luecke, William E.
    McColskey, J. David
    Darcis, Philippe P.
    Wang, Yong-Yi
    [J]. PROCEEDINGS OF THE EIGHTEENTH (2008) INTERNATIONAL OFFSHORE AND POLAR ENGINEERING CONFERENCE, VOL 4, 2008, : 131 - +
  • [6] CTOA Results for X65 and X100 Pipeline Steels: Influence of Displacement Rate
    Reuven, R.
    McCowan, C.
    Drexler, E.
    Shtechman, A.
    Darcis, Ph.
    Treinen, M.
    Smith, R.
    Merritt, J.
    Siewert, T.
    McColskey, J. D.
    [J]. IPC2008: PROCEEDINGS OF THE ASME INTERNATIONAL PIPELINE CONFERENCE - 2008, VOL 3, 2009, : 279 - 286
  • [7] Microstructure and precipitates of X100 pipeline steel
    Ruan, Hong-Zhi
    Zhao, Zheng-Zhi
    Zhao, Ai-Min
    Gao, Xu-Tao
    Qi, Liang
    [J]. Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2013, 34 (01): : 43 - 48
  • [8] Study on the weldability of X100 pipeline steel on scene
    Wang Pinyi
    Mou Zongyuan
    [J]. MATERIALS PROCESSING AND MANUFACTURING III, PTS 1-4, 2013, 753-755 : 343 - 352
  • [9] Cold cracking susceptibility of X100 pipeline steel
    严春妍
    姜心怡
    元媛
    纪秀林
    张可召
    [J]. China Welding, 2019, 28 (03) : 25 - 33
  • [10] Acicular ferrite nucleation mechanism in laser-MAG hybrid welds of X100 pipeline steel
    Qi, Xiaonan
    Wang, Xiaonan
    Di, Hongshuang
    Shen, Xinjun
    Huan, Pengcheng
    He, Jingrui
    Chen, Long
    [J]. MATERIALS LETTERS, 2021, 304