Formation of perovskite type phases during the high temperature oxidation of stainless steels coated with reactive element oxides

被引:2
|
作者
Chevalier, S [1 ]
Larpin, JP [1 ]
机构
[1] Univ Bourgogne, CNRS UMR 5613, Lab Rech Reactivite Solides, F-21078 Dijon, France
关键词
reactive element effect; perovskite phases; X-ray diffraction; MOCVD coatings; Fe-30Cr alloys;
D O I
10.1016/s1359-6454(02)00106-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The beneficial effects of reactive elements (RE) on the high temperature (HT) oxidation behavior of stainless steels have previously been attributed to the formation of perovskite compounds on oxide grain boundaries. In order to verify the ability of Cr2O3 to form perovskite compounds with reactive element oxides RE2O3 (RE=La, Nd, Sm, Gd, Yb, Y), mixtures of Cr2O3 and RE2O3 powders were oxidized at 1000 degreesC in air, and characterized by X-ray diffraction. Results were compared to those obtained on RE2O3-coated Fe-30Cr samples (RE=Y, Nd, Sin, Yb) oxidized at 1000 degreesC under the same conditions. It was found that the most efficient reactive element oxide, Y2O3, was not this which was completely converted into perovskite structure. So, it is assumed that it is not the reaction rate of the perovskite formation, or the ability of the RE oxide to form a perovskite structure, but rather the intrinsic properties of the perovskite, which is the origin of the RE effect. (C) 2002 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:3105 / 3114
页数:10
相关论文
共 50 条
  • [41] Grain growth of iron oxides during high temperature oxidation
    Kim, BK
    Szpunar, JA
    RECRYSTALLIZATION AND GRAIN GROWTH, VOLS 1 AND 2, 2001, : 489 - 494
  • [42] Oxidation After Breakdown of the Chromium-Rich Scale on Stainless Steels at High Temperature: Internal Oxidation
    T. Jonsson
    S. Karlsson
    H. Hooshyar
    M. Sattari
    J. Liske
    J.-E. Svensson
    L.-G. Johansson
    Oxidation of Metals, 2016, 85 : 509 - 536
  • [43] Oxidation After Breakdown of the Chromium-Rich Scale on Stainless Steels at High Temperature: Internal Oxidation
    Jonsson, T.
    Karlsson, S.
    Hooshyar, H.
    Sattari, M.
    Liske, J.
    Svensson, J. -E.
    Johansson, L. -G.
    OXIDATION OF METALS, 2016, 85 (5-6): : 509 - 536
  • [44] Influences of carbon and silicon on blister formation in scale surface during high temperature oxidation of carbon steels
    Deuk-Jung Kim
    Jae-Sang Lee
    Yang-Mo Koo
    Metals and Materials International, 2017, 23 : 715 - 719
  • [45] Influences of Carbon and Silicon on Blister Formation in Scale Surface During High Temperature Oxidation of Carbon Steels
    Kim, Deuk-Jung
    Lee, Jae-Sang
    Koo, Yang-Mo
    METALS AND MATERIALS INTERNATIONAL, 2017, 23 (04) : 715 - 719
  • [46] Review of Several Studies on High Temperature Oxidation Behaviour and Mechanism of Austenitic Stainless Steels
    Fujikawa, H.
    DIFFUSION IN SOLIDS AND LIQUIDS VI, PTS 1 AND 2, 2011, 312-315 : 1097 - 1105
  • [47] Perovskite-type oxides for high-temperature oxygen separation membranes
    Kharton, VV
    Yaremchenko, AA
    Kovalevsky, AV
    Viskup, AP
    Naumovich, EN
    Kerko, PF
    JOURNAL OF MEMBRANE SCIENCE, 1999, 163 (02) : 307 - 317
  • [48] High temperature sorption of carbon dioxide on perovskite-type metal oxides
    Lin, Y. S.
    Yang, Qing
    Ida, Junichi
    JOURNAL OF THE TAIWAN INSTITUTE OF CHEMICAL ENGINEERS, 2009, 40 (03) : 276 - 280
  • [49] Texture evolution during high temperature gas nitriding of duplex stainless steels
    Tschiptschin, AP
    Garzón, CM
    De Lima, NB
    TEXTURES OF MATERIALS, PTS 1 AND 2, 2002, 408-4 : 1347 - 1352
  • [50] Multi layered Surface Oxides within Crevices of Type 316L Stainless Steels in High-Temperature Pure Water
    Soma, Y.
    Kato, C.
    Yamamoto, M.
    CORROSION, 2014, 70 (04) : 366 - 374