Formation of perovskite type phases during the high temperature oxidation of stainless steels coated with reactive element oxides

被引:2
|
作者
Chevalier, S [1 ]
Larpin, JP [1 ]
机构
[1] Univ Bourgogne, CNRS UMR 5613, Lab Rech Reactivite Solides, F-21078 Dijon, France
关键词
reactive element effect; perovskite phases; X-ray diffraction; MOCVD coatings; Fe-30Cr alloys;
D O I
10.1016/s1359-6454(02)00106-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The beneficial effects of reactive elements (RE) on the high temperature (HT) oxidation behavior of stainless steels have previously been attributed to the formation of perovskite compounds on oxide grain boundaries. In order to verify the ability of Cr2O3 to form perovskite compounds with reactive element oxides RE2O3 (RE=La, Nd, Sm, Gd, Yb, Y), mixtures of Cr2O3 and RE2O3 powders were oxidized at 1000 degreesC in air, and characterized by X-ray diffraction. Results were compared to those obtained on RE2O3-coated Fe-30Cr samples (RE=Y, Nd, Sin, Yb) oxidized at 1000 degreesC under the same conditions. It was found that the most efficient reactive element oxide, Y2O3, was not this which was completely converted into perovskite structure. So, it is assumed that it is not the reaction rate of the perovskite formation, or the ability of the RE oxide to form a perovskite structure, but rather the intrinsic properties of the perovskite, which is the origin of the RE effect. (C) 2002 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:3105 / 3114
页数:10
相关论文
共 50 条
  • [31] INFLUENCE OF SURFACE PREPARATION ON OXIDATION OF STAINLESS-STEELS AT HIGH-TEMPERATURE
    GUILLAMET, R
    LENGLET, M
    GAZIN, L
    HANNOYER, B
    LOPITAUX, J
    SURFACE AND INTERFACE ANALYSIS, 1993, 20 (01) : 15 - 20
  • [32] HIGH TEMPERATURE OXIDATION OF AUSTENITIC STAINLESS STEELS IN REHEATING FURNACE ATMOSPHERE.
    Kinoshita, Yoshio
    Oguma, Susumu
    1600, (65):
  • [33] Glass coatings on stainless steels for high-temperature oxidation protection: Mechanisms
    Chen, Minghui
    Li, Wenbo
    Shen, Mingli
    Zhu, Shenglong
    Wang, Fuhui
    CORROSION SCIENCE, 2014, 82 : 316 - 327
  • [35] High-temperature oxidation inducing strain for the 2205 duplex stainless steels
    Lv, Jinlong
    Wang, Zhuqing
    MATERIALS RESEARCH EXPRESS, 2020, 7 (10)
  • [36] Preliminary study on the laser cleaning of stainless steels after high temperature oxidation
    Psyllaki, P
    Oltra, R
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 282 (1-2): : 145 - 152
  • [37] High temperature oxidation behavior of AISI 304 and AISI 430 stainless steels
    Departamento de Química, Universidade Federal de Ouro Preto, Campus Universitário, 35400 Ouro Preto - MG, Brazil
    不详
    不详
    Mater. Res., 2006, 4 (393-397):
  • [38] Evolution of the metal-oxide interface during the initial stage of the high temperature oxidation of ferritic stainless steels
    Issartel, Jerome
    Martoia, Sebastien
    Charlot, Frederic
    Parry, Valerie
    Wouters, Yves
    Galerie, Alain
    MATERIALS AT HIGH TEMPERATURES, 2011, 28 (04) : 274 - 278
  • [39] HYDROGEN ABSORPTION BY STEELS DURING HIGH-TEMPERATURE OXIDATION
    KIRILLOVA, VP
    MALYSHEV, VN
    ARCHAKOV, YI
    JOURNAL OF APPLIED CHEMISTRY OF THE USSR, 1982, 55 (03): : 542 - 545
  • [40] The mechanism of oxide film formation on austenitic stainless steels in high temperature water
    Stellwag, B
    CORROSION SCIENCE, 1998, 40 (2-3) : 337 - 370