摘要
C/C-SiC composites, namely carbon fiber reinforced silicon carbide and pyrocarbon matrices, were fabricated in two steps in this study. Firstly, C/C composites were prepared by a rapid economical densification process of chemical liquid-vaporized infiltration. PAN based felt and 2-Dimensional carbon fibers were chosen as preform, respectively. A liquid hydrocarbon, kerosene, was used as a precursor. The C/C composites were processed in a temperature range of 900-1100 degrees C for 150 minutes. Subsequently, C/C-SiC composites were fabricated from the C/C composites and silicon powder by reactive melt infiltration method. Densities, open porosities of the C/C and the C/C-SiC composites were investigated. Structural properties of the C/C-SiC composites were studied by optical microscopy. X-ray diffraction was used to identify the element and the crystal phase of the composites. It was shown that the density of C/C composite reached to 1.72 g/cm(3) based on the 2D carbon fibers by CLVI method. Microstructure observation of the C/C composite revealed that the pyrocarbon is layer concentric around the fibers. It was found that during the RMI processing beta-SiC was formed through the reaction only between liquid silicon and pyrocarbon, while carbon fiber was not damaged. Free silicon remains in the C/C-SiC composites because of insufficient reaction with the pyrocarbon.
引用
收藏
页码:159 / 162
页数:4
相关论文
共 50 条
  • [21] Friction and wear properties of C/C-SiC braking composites
    Zhou, Xuan
    Zhu, Dongmei
    Xie, Qiao
    Luo, Fa
    Zhou, Wancheng
    CERAMICS INTERNATIONAL, 2012, 38 (03) : 2467 - 2473
  • [22] Effect of damage on flexural modulus of C/C-SiC composites
    Srivastava, VK
    Maile, K
    Bothe, K
    Udoh, A
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 354 (1-2): : 292 - 297
  • [23] Preparation and properties of C/C-SiC nano-composites
    Krnel, Kristoffer
    Stadler, Zmago
    Kosmac, Tomaz
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (2-3) : 1211 - 1216
  • [24] Tribological behaviour of C/C-SiC composites-A review
    Kumar, Parshant
    Srivastava, V. K.
    JOURNAL OF ADVANCED CERAMICS, 2016, 5 (01) : 1 - 12
  • [25] OXIDATION BEHAVIOUR OF C/C-SiC COMPOSITES IN OPEN ATMOSPHERE
    Srivastava, V. K.
    Singh, Shraddha
    ADVANCED PROCESSING AND MANUFACTURING TECHNOLOGIES FOR STRUCTURAL AND MULTIFUNCTIONAL MATERIALS II, 2009, 29 (09): : 33 - 41
  • [26] Tribological Properties of C/C-SiC Composites for Brake Discs
    Jang, G. H.
    Cho, K. H.
    Park, S. B.
    Lee, W. G.
    Hong, U. S.
    Jang, H.
    METALS AND MATERIALS INTERNATIONAL, 2010, 16 (01) : 61 - 66
  • [27] Impulse excitation nondestructive mapping of C/C-SiC composites
    Srivastava, VK
    Maile, K
    HIGH TEMPERATURE CERAMIC MATRIX COMPOSITES 5, 2005, : 569 - 573
  • [28] Mechanical properties and morphological studies of C/C-SiC composites
    Singh, Shraddha
    Srivastava, V. K.
    Prakash, Rajiv
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 534 : 707 - 710
  • [29] Oxidation behavior of C/C-SiC gradient matrix composites
    Deng, Jingyi
    Liu, Wenchuan
    Du, Haifeng
    Cheng, Huiming
    Li, Yiyi
    Journal of Materials Science and Technology, 2001, 17 (05): : 543 - 546
  • [30] Oxidation Behavior of C/C-SiC Gradient Matrix Composites
    Jingyi DENG
    Journal of Materials Science & Technology, 2001, (05) : 543 - 546