Improvement of oxidation resistance of Ti-47Al-2W-0.5Si alloy modified by aluminizing method

被引:21
|
作者
Szkliniarz, Agnieszka [1 ]
Moskal, Grzegorz [1 ]
Szkliniarz, Wojciech [1 ]
Swadzba, Radoslaw [2 ]
机构
[1] Silesian Tech Univ, Dept Mat Sci & Met, PL-40019 Katowice, Poland
[2] Inst Ferrous Met, PL-44100 Gliwice, Poland
来源
关键词
Titanium aluminides; TiAl based alloy; Protective coatings; Oxidation; Out-of-pack method; CYCLIC OXIDATION; COATINGS; MICROSTRUCTURE; BEHAVIOR;
D O I
10.1016/j.surfcoat.2015.07.072
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The presented study defines the impact of aluminizing process by out-of-pack method on the oxidation resistance of cast Ti-47Al-2W-0.5Si alloy after homogenising and hot isostatic pressing. The surface condition was characterized, as well as chemical and phase composition of scale formed on examined alloy with and without protective coating, when subjected to cyclic oxidation at 950 degrees C. It was established that the generated hermetic and compact aluminium diffusion coating with a thickness of about 7.5 mu m, consisting mainly of TiAl2 phase, has a significant effect on the improvement of cyclic oxidation resistance in the case of investigated alloy. It was confirmed that the scale formed after the oxidation process on the surface of alloy with protective coating was composed mainly of Al2O3 oxide, contrary to the scale formed on the alloy without protective coating, which was mainly consisting of TiO2 oxide. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:270 / 277
页数:8
相关论文
共 50 条
  • [21] Precipitation of β particles in a fully lamellar Ti-47Al-2Nb-1Mn-0.5W-0.5Mo-0.2Si (at.%) alloy
    J. Beddoes
    W. R. Chen
    L. Zhao
    Journal of Materials Science, 2002, 37 : 621 - 627
  • [22] The effect of stress and temperature on primary creep of Ti-47Al-2Nb-1Mn-0.5W-0.5Mo-0.2Si alloy
    Seo, DY
    Bieler, TR
    Larsen, DE
    CREEP AND FRACTURE OF ENGINEERING MATERIALS AND STRUCTURES, 1996, : 577 - 586
  • [23] Changes in microstructure during primary creep of a Ti-47Al-2Nb-1Mn-0.5W-0.5Mo-0.2Si alloy
    D. Y. Seo
    T. R. Bieler
    S. U. An
    D. E. Larsen
    Metallurgical and Materials Transactions A, 1998, 29 : 89 - 98
  • [24] Improvement in the oxidation resistance of Nb-16Si-24Ti-2Al-2Cr alloy by hot pressing
    Liu, Tian
    Li, Tiejun
    Cao, Yuankui
    Fu, Ao
    Xie, Zhonghao
    Wang, Jian
    Liu, Bin
    Liu, Yong
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2024, 120
  • [25] Liquid-phase aluminizing and siliconizing at the surface of a Ti60 alloy and improvement in oxidation resistance
    Xiong, Hua-Ping
    Mao, Wei
    Ma, Wen-Li
    Xie, Yong-Hui
    Chen, Yun-Feng
    Yuan, Hong
    Li, Xiao-Hong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 433 (1-2): : 108 - 113
  • [26] Effect of growth rate on microstructures and microhardness in directionally solidified Ti-47Al-1.0W-0.5Si alloy
    Liu, Tong
    Luo, Liangshun
    Su, Yanqing
    Wang, Liang
    Li, Xinzhong
    Chen, Ruirun
    Guo, Jingjie
    Fu, Hengzhi
    JOURNAL OF MATERIALS RESEARCH, 2016, 31 (05) : 618 - 626
  • [27] Effect of growth rate on microstructures and microhardness in directionally solidified Ti-47Al-1.0W-0.5Si alloy
    Tong Liu
    Liangshun Luo
    Yanqing Su
    Liang Wang
    Xinzhong Li
    Ruirun Chen
    Jingjie Guo
    Hengzhi Fu
    Journal of Materials Research, 2016, 31 : 618 - 626
  • [28] Effect of surface aluminizing temperature on oxidation resistance of Ti2AlNb alloy
    Ren, Bei-Lei
    Miao, Qiang
    Liang, Wen-Ping
    Wang, Li
    Hu, Rong-Yao
    Lu, Hai-Feng
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2015, 36 (12): : 241 - 246
  • [29] Microstructural modification of investment cast Ti-47Al-2Nb-1Mn-0.5Mo-0.5W-0.2Si alloy by heat treatment
    Chen, WR
    Zhao, L
    Beddoes, J
    GAMMA TITANIUM ALUMINIDES 1999, 1999, : 323 - 330
  • [30] On the grain growth in a cast intermetallic Ti-46Al-2W-0.5Si alloy
    Lapin, J
    Klimová, A
    JOURNAL OF MATERIALS SCIENCE LETTERS, 2003, 22 (18) : 1275 - 1277