Microstructural evolution and mechanical properties of the AA2219/TiC nanocomposite manufactured by ultrasonic solidification

被引:45
|
作者
Yang, Yilong [1 ]
Liu, Zhilin [1 ,2 ]
Jiang, Ripeng [1 ]
Li, Ruiqing [1 ]
Li, Xiaoqian [1 ,2 ]
机构
[1] Cent South Univ, Light Alloy Res Inst, Changsha 410083, Hunan, Peoples R China
[2] Cent South Univ, Coll Mech & Elect Engn, State Key Lab High Performance Complex Mfg, Changsha 410083, Hunan, Peoples R China
基金
中国国家自然科学基金;
关键词
AA2219/TiC nanocomposite; Ultrasonic casting; Structure-property relationship; Strengthening mechanisms; Grain refinement; METAL-MATRIX COMPOSITES; GRAIN-REFINEMENT; PLASTIC RELAXATION; CAVITATION EROSION; TENSILE PROPERTIES; ALUMINUM-ALLOYS; BEHAVIOR; NANO; NUCLEATION; DISPERSION;
D O I
10.1016/j.jallcom.2019.151991
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The mechanical properties of metallic matrix composites can be tailored through the microstructural modification between metal matrix and reinforcing particles. In this work, the AA2219/TiC nano-composite containing 0, 0.5, 0.9, 1.3 and 1.7 wt.% TiC nanoparticles were individually manufactured using the ultrasound-assisted solidification technique. There existed an optimal addition level of TiC nanoparticles (0.9 wt.%) beyond which grain coarsening occurred. TiC nanoparticles were observed to reduce the average grain sizes of alpha-Al matrix alloy by 61%. Meanwhile, 0.9 wt.% TiC nanoparticles corresponded to the maximum tensile strength and hardness. When the addition level reached over 0.9 wt.% in the 2219 Al alloy matrix melt, the TiC nanoparticles tended to agglomerate in a form of condensed clusters, which cannot be well dispersed by ultrasonication due to the increasing viscosity. Such agglomerating TiC nanoparticles deteriorated the tensile strain and hardness of AA2219/TiC nanocomposite. Then, five major potential strengthening mechanisms in AA2219/TiC nanocomposite was quantitatively analysed, including grain refinement, Orowan strengthening, load transfer effect, mismatch of thermal expansion, and mismatch of elastic modulus. Analysis shows that Orowan strengthening acts as the most dominant strengthening mechanism, followed by another comparable strengthening mechanism from the mismatch between the thermal expansion of alpha-Al matrix and TiC nanoparticles. The other three strengthening mechanisms induced very limited improvement in mechanical properties. Besides acting as reinforcing agents, the TiC nanoparticles also possess very high potency as heterogeneous nucleation sites. The relevant nucleation potency was validated by crystallographic investigation using the edge-to-edge matching model. Finally, the grain refining mechanism of alpha-Al matrix alloy was unraveled in terms of the nucleation crystallography and the ultrasonic cavitation. (C) 2019 Elsevier B.V. All rights reserved.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Microstructural and Mechanical Characterization of as Weld and Aged Conditions of AA2219 Aluminium Alloy by Gas Tungsten Arc Welding Process
    Arunkumar, S.
    Sathiya, P.
    Devakumaran, K.
    Kumar, S. Ramesh
    RUSSIAN JOURNAL OF NON-FERROUS METALS, 2018, 59 (01) : 93 - 101
  • [32] Analysis on exceptional cryogenic mechanical properties of AA2219 alloy FSW joints in multi-scale
    Hao, Yong-gang
    Liu, Wei
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 850
  • [33] Effect of welding processes on AA2219 aluminium alloy joint properties
    Malarvizhi, S.
    Balasubramanian, V.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2011, 21 (05) : 962 - 973
  • [34] Microstructure Evolution during Friction Stir Welding of Aluminum Alloy AA2219
    K.S.Arora
    S.Pandey
    M.Schaper
    R.Kumar
    JournalofMaterialsScience&Technology, 2010, 26 (08) : 747 - 753
  • [35] Influence of protrusion geometry on the microstructure and mechanical properties of AA2219 fabricated by additive friction stir deposition
    Zhang, Ming
    Lai, Ruilin
    Li, Yidi
    Wang, Hui
    Yang, Biaobiao
    Li, Yunping
    PROGRESS IN ADDITIVE MANUFACTURING, 2025,
  • [36] Mechanical properties of cryo-rolled aluminium alloy AA2219 at 300, 77 and 20 K
    Nayan, Niraj
    Singh, Gaurav
    Baunthiyal, Davinder
    Murty, S. V. S. Narayana
    Prabhu, T. Antony
    Singh, Satish K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 881
  • [37] Analysis on exceptional cryogenic mechanical properties of AA2219 alloy FSW joints in multi-scale
    Hao, Yong-gang
    Liu, Wei
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 850
  • [38] Improvement of mechanical properties of aluminium-copper alloy (AA2219) GTA welds by Sc addition
    Seshagiri, P. C.
    Nair, B. S.
    Reddy, G. M.
    Rao, K. S.
    Bhattacharya, S. S.
    Rao, K. P.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2008, 13 (02) : 146 - 158
  • [39] Microstructure Evolution during Friction Stir Welding of Aluminum Alloy AA2219
    Arora, K. S.
    Pandey, S.
    Schaper, M.
    Kumar, R.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2010, 26 (08) : 747 - 753
  • [40] Refilling friction stir welding of 20 mm thick AA2219 and analysis of microstructure and mechanical properties
    Ji P.
    Liu X.
    Zhang Y.
    Hong L.
    Hao Y.
    Hao, Yunfei (haoyunfei1234@163.com), 1600, Harbin Research Institute of Welding (42): : 86 - 91