Deuterium adsorption on (and desorption from) SiC(0001)-(3 x 3), (√3 x √3) R30°, (6√3 x 6√3) R30° and quasi-free-standing graphene obtained by hydrogen intercalation

被引:9
|
作者
Bocquet, F. C. [1 ]
Bisson, R. [2 ]
Themlin, J-M [3 ,4 ]
Layet, J-M [2 ]
Angot, T. [2 ]
机构
[1] Forschungszentrum Julich, Peter Grunberg Inst PGI 3, D-52425 Julich, Germany
[2] Aix Marseille Univ, CNRS, PIIM, UMR 7345, F-13013 Marseille, France
[3] Aix Marseille Univ, IM2NP, F-13397 Marseille, France
[4] CNRS, UMR 7334, F-13397 Marseille, France
关键词
ENERGY-LOSS SPECTROSCOPY; 3X3 SURFACE RECONSTRUCTION; EPITAXIAL GRAPHENE; POLYCRYSTALLINE DIAMOND; 6H-SIC(0001) SURFACE; SILICON-CARBIDE; SIC SURFACES; ABSTRACTION; GRAPHITIZATION; 4H-SIC(0001);
D O I
10.1088/0022-3727/47/9/094014
中图分类号
O59 [应用物理学];
学科分类号
摘要
We present a comparative high-resolution electron energy-loss spectroscopy study on the interaction of atomic hydrogen and deuterium with various reconstructions of SiC(0 0 0 1). We first show that on both the (3 x 3) and (root 3 x root 3) R30 degrees reconstructions, deuterium atoms only bind to silicon atoms, thereby confirming the silicon-rich appellation of these reconstructions. Deuterium passivation of the (3 x 3) is only reversible when exposed to atomic deuterium at a surface temperature of 700K since tri- and dideuterides, necessary precursors for silicon etching, are not stable. On the other hand, we show that the deuteration of the (root 3 x root 3) R30 degrees is always reversible because precursors to silicon etching are scarce on the surface. Then, we demonstrate that hydrogen (deuterium) adsorption at 300K on both the (6 root 3 x 6 root 3) R30 degrees (buffer-layer) and the quasi-free-standing graphene occurs on carbon atoms justifying their carbon-rich appellation. Comparison of the deuterium binding in the intercalation layer of quasi-free-standing graphene with the deuterated (root 3 x root 3) R30 degrees surface provides some indication on the bonding structure at the substrate intercalation layer. Finally, by measuring C-H (C-D) vibrational frequencies and hydrogen (deuterium) desorption temperatures we suggest that partial sp(2)-to-sp(3) rehybridization occurs for the carbon atoms of the buffer-layer because of the corrugation related to covalent bonding to the SiC substrate. In contrast, on quasi-free-standing graphene hydrogen (deuterium) atoms adsorb similarly to what is observed on graphite, i.e. without preferential sticking related to the underlying SiC substrate.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] Scanning tunneling microscopy study of pentacene adsorption on Ag/Si(111)-(√3 x √3)R30°
    Guaino, P
    Carty, D
    Hughes, G
    Moriarty, P
    Cafolla, AA
    APPLIED SURFACE SCIENCE, 2003, 212 : 537 - 541
  • [42] A scanning tunneling microscopy observation of (√3 x √3) R30° reconstructed Ni2P(0001)
    Kinoshita, Kumiko
    Simon, Georg Hermann
    Koenig, Thomas
    Heyde, Markus
    Freund, Hans-Joachim
    Nakagawa, Yuta
    Suzuki, Shushi
    Chun, Wan-Jae
    Oyama, Shiaeo Ted
    Otani, Shigeki
    Asakura, Kiyotaka
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2008, 47 (07) : 6088 - 6091
  • [43] A structural model of Si(111)(2√3 x 2√3)R30°-Sn
    Ichikawa, T
    Cho, K
    Onodera, T
    Mizoguchi, A
    Ohkoshi, T
    PROCEEDINGS OF THE 25TH INTERNATIONAL CONFERENCE ON THE PHYSICS OF SEMICONDUCTORS, PTS I AND II, 2001, 87 : 291 - 292
  • [44] Insulating ground state of Sn/Si(111)-(√3x√3)R30°
    Modesti, S.
    Petaccia, L.
    Ceballos, G.
    Vobornik, I.
    Panaccione, G.
    Rossi, G.
    Ottaviano, L.
    Larciprete, R.
    Lizzit, S.
    Goldoni, A.
    PHYSICAL REVIEW LETTERS, 2007, 98 (12)
  • [45] Observation of a (√3 x √3)R30° reconstruction on O-polar ZnO surfaces
    King, S. T.
    Parihar, S. S.
    Pradhan, K.
    Johnson-Steigelman, H. T.
    Lyman, P. F.
    SURFACE SCIENCE, 2008, 602 (22) : L131 - L134
  • [46] Electronic and crystal structure of the Pt(111)-(√3 x √3)R30°-K system
    Koroteev, Yu. M.
    Chulkov, E. V.
    SURFACE SCIENCE, 2018, 678 : 99 - 105
  • [47] Simultaneous noncontact AFM and STM of Ag:Si(111)-(√3 x √3)R30°
    Sweetman, Adam
    Stannard, Andrew
    Sugimoto, Yoshiaki
    Abe, Masayuki
    Morita, Seizo
    Moriarty, Philip
    PHYSICAL REVIEW B, 2013, 87 (07)
  • [48] The model of the magnesium silicide phase (2/3√3 x 2/3√3)-R30° on Si(111)
    Galkin, Konstantin N.
    Kumar, Mahesh
    Shivaprasad, S. M.
    Galkin, Nikolay G.
    ASIA-PACIFIC CONFERENCE ON SEMICONDUCTING SILICIDES SCIENCE AND TECHNOLOGY TOWARDS SUSTAINABLE OPTOELECTRONICS (APAC-SILICIDE 2010), 2011, 11 : 47 - 50
  • [49] LEED structure determination of the Ni(111)(√3 x √3)R30°-Sn surface
    Soares, EA
    Bittencourt, C
    Lopes, EL
    de Carvalho, VE
    Woodruff, DP
    SURFACE SCIENCE, 2004, 550 (1-3) : 127 - 132
  • [50] THERMODYNAMIC PROPERTIES OF THE METALLIC SYSTEM Au(111)-(√3 x √3)R30°-Pd
    Chadli, R.
    Kheffache, S.
    Khater, A.
    SURFACE REVIEW AND LETTERS, 2016, 23 (03)