Fracture toughness of thick plates of Ti-6Al-4V weldments

被引:0
|
作者
Eizaguirre, I [1 ]
Santamaria, F [1 ]
Irisarri, AM [1 ]
Plaza, LM [1 ]
机构
[1] INASMET, San Sebastian 20009, Spain
关键词
D O I
暂无
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The fracture behaviour of thick plates of Ti-6Al-4V alloy joined by means of plasma are welding (PAW) and two different electron beam welding (EBW) procedures. In the whole temperature range PAW weld metal specimens exhibited higher toughness than base material. This behaviour has been attributed to the acicular microstructure of the weld metal compared to the equiaxic of parent alloy. EBW welded metals also showed higher toughness than base material although no so high as PAW ones. These results could be associated with the presence of a small volume fraction of brittle alpha prime martensite due to the higher cooling rate.
引用
收藏
页码:895 / 900
页数:6
相关论文
共 50 条
  • [21] DYNAMIC FRACTURE-TOUGHNESS OF TI-6AL-4V ALLOYS AND ITS DEPENDENCE ON MICROSTRUCTURES
    YAMADA, T
    KIM, KH
    KIM, BN
    TAKEDA, N
    KISHI, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1990, 54 (10) : 1065 - 1071
  • [22] Fracture toughness and fatigue crack growth in Ti-6Al-4V friction stir welds
    Edwards, P.
    Ramulu, M.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2015, 38 (08) : 970 - 982
  • [23] EFFECT OF HEAT-TREATMENT AND MICROSTRUCTURE ON FRACTURE-TOUGHNESS OF TI-6AL-4V
    RHODES, CG
    JOURNAL OF METALS, 1979, 31 (12): : 109 - 109
  • [24] Influence of the heat treatment and notch orientation on the fracture toughness of a Ti-6Al-4V plate
    Plaza, LM
    Zapirain, F
    deSeoane, AV
    Irisarri, AM
    ECF 11 - MECHANISMS AND MECHANICS OF DAMAGE AND FAILURE, VOLS I-III, 1996, : 553 - 558
  • [25] Microstructural Characterization of Ti-6Al-4V Alloy Fiber Laser Weldments
    Kumar, Chandan
    Das, Manas
    ADVANCES IN MECHANICAL ENGINEERING, ICRIDME 2018, 2020, : 475 - 486
  • [26] ELECTRON-BEAM WELDING STUDIES ON 6.5 MM THICK TI-6AL-4V PLATES
    THOMAS, G
    RAMACHANDRA, V
    NAIR, MJ
    NAGARAJAN, KV
    SARKAR, BK
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 1982, 35 (01): : 25 - &
  • [27] Fracture toughness of laser-based powder bed fusion produced Ti-6Al-4V
    Louw, D. F.
    Neaves, M.
    Mcduling, C.
    Becker, T. H.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 931
  • [28] The Effect of Microstructural Features and Thickness on Fracture Toughness of Ti-6Al-4V ELI Thin Sheets
    Aliakbari, Saeed
    Yegaie, Yaser Salehi
    ARABIAN JOURNAL FOR SCIENCE AND ENGINEERING, 2018, 43 (03) : 1247 - 1255
  • [29] Adiabatic shear fracture in Ti-6Al-4V alloy
    Zhang Jing
    Tan Cheng-wen
    Ren Yu
    Yu Xiao-dong
    Ma Hong-lei
    Wang Fu-chi
    Cai Hong-nian
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2011, 21 (11) : 2396 - 2401
  • [30] DIFFUSION BONDING OF SIC/TI-6AL-4V COMPOSITE TO TI-6AL-4V ALLOY AND FRACTURE-BEHAVIOR OF JOINT
    FUKUMOTO, S
    HIROSE, A
    KOBAYASHI, KF
    MATERIALS SCIENCE AND TECHNOLOGY, 1993, 9 (06) : 520 - 527