Effect of holding time on the self-joining of silicon nitride

被引:22
|
作者
Liu, C. F. [1 ]
Zhang, J. [1 ]
Zhou, Y. [1 ]
Yi, H. L. [1 ]
Naka, M. [2 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Inst Adv Ceram, Harbin 150001, Peoples R China
[2] Osaka Univ Ibaraki, Joining & Welding Res Inst, Osaka 5670047, Japan
关键词
Si3N4; ceramics; Brazing; Cu-Pd-Ti filler alloy; Microstructure; Bonding strength; MICROSTRUCTURE; SI3N4; INTERFACE; STRENGTH; JOINTS; AG; CU;
D O I
10.1016/j.jallcom.2008.03.059
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Reliable Si3N4/Si3N4 joints were obtained using Cu-Pd-Ti as filler alloy. The effect of holding time on interfacial microstructure and bonding strength of the joints was investigated. All the joints consist of continuous reaction layer (fine-grain TiN), discontinuous reaction layer (coarse-grain TiN), Cu-based solid solution and reaction products. Prolonged exposure to the elevated temperature causes the thickness of the discontinuous reaction layer to increase, due to the coarsening of TiN grains. And the amount of Pd-Si phase increases instead of Ti-Si phase. With the increase of holding time, the bonding strength of the joints decreases. The formation of a reaction layer with a suitable thickness promotes the improvement of bonding strength of joints. (C) 2008 Elsevier B. V. All rights reserved.
引用
收藏
页码:217 / 221
页数:5
相关论文
共 50 条
  • [11] Silicon nitride: From sintering to joining
    Gopal, M
    De Jonghe, LC
    Thomas, G
    ACTA MATERIALIA, 1998, 46 (07) : 2401 - 2405
  • [12] Joining silicon nitride to itself and to metals
    Peteves, SD
    Ceccone, G
    Paulasto, M
    Stamos, V
    Yvon, P
    JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1996, 48 (01): : 48 - +
  • [13] Seamless joining of silicon nitride ceramics
    Gopal, M
    Sixta, M
    De Jonghe, L
    Thomas, G
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2001, 84 (04) : 708 - 712
  • [14] JOINING OF SILICON NITRIDE BY SLURRY OR PASTE
    Kondo, Naoki
    Hyuga, Hideki
    Kita, Hideki
    ADVANCED PROCESSING AND MANUFACTURINGTECHNOLOGIES FOR STRUCTURAL AND MULTIFUNCTIONAL MATERIALS III, 2010, 30 (08): : 131 - 134
  • [15] On embeddability of automorphisms into measurable flows from the point of view of self-joining properties
    Kulaga-Przymus, Joanna
    FUNDAMENTA MATHEMATICAE, 2015, 230 (01) : 15 - 76
  • [16] Self-joining of Si3N4 using metal interlayers
    Lemus-Ruiz, J
    León-Patiño, CA
    Drew, RAL
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2006, 37A (01): : 69 - 75
  • [17] Microwave joining of ceramics, silicon nitride and silicon carbide
    Sato, Tadao
    Sugiura, Toshiharu
    Shimakage, Kazuyoshi
    Journal of the Ceramic Society of Japan. International ed., 1993, 101 (04): : 411 - 416
  • [18] Semi-homogeneous joining of silicon nitride with a silicon nitride powder insert
    Kondo, Naoki
    Hyuga, Hideki
    Hotta, Mikinori
    Kita, Hideki
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2011, 119 (1388) : 322 - 324
  • [19] Semi-homogeneous joining of silicon nitride with a silicon nitride powder insert
    National Institute of Advanced Industrial Science and Technology , 2266-98 Shimo-Shidami, Moriyama-ku, Nagoya 463-8560, Japan
    J Ceram Soc Jpn, 1388 (322-334):
  • [20] Effect of Temperature and Holding Time on Synthesized Silicon Oxynitride
    Nie Jianhua
    Wen Jin
    Qiu Wendong
    Zhao Wei
    Yin Guoheng
    Liang Yonghe
    Yin Yucheng
    Xu Chao
    RARE METAL MATERIALS AND ENGINEERING, 2015, 44 : 475 - 477