Deposition of ferroelectric Pb(Zr0.52Ti0.48)O-3 films on platinized silicon using Nd:YAG laser

被引:0
|
作者
Im, HS
Kim, SH
Choi, YK
Lee, KH
Jung, KW
机构
[1] WONKWANG UNIV,MED RESOURCES RES CTR,IKSAN 570749,SOUTH KOREA
[2] WONKWANG UNIV,DEPT CHEM,IKSAN,SOUTH KOREA
关键词
D O I
暂无
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Lead zirconate titanate (PZT) thin films were deposited onto the Pt/Ti/SiO2/Si substrate by the pulsed laser deposition with the second harmonic wavelength (532 nm) of Nd:YAG laser. In order to determine the optimum conditions for the film deposition, the phase of the films were investigated as functions of ambient oxygen pressure, substrate temperature, and laser fluence. Also the chemical composition analysis was conducted for the PZT films deposited under various ambient oxygen pressure. When the distance between substrate and bulk PZT target is set to 20 mm, the optimum conditions have been determined to be 3 torr of oxygen pressure, 1.5 J/cm(2) of laser fluence, and 823-848(+/-10) K range of substrate temperature. At these conditions, perovskite phase PZT films were obtained on platinized silicon. The chemical composition of the films is very similar to that of PZT bulk target. The physical structure of the deposited films analyzed by scanning electron microscopy shows a columnar morphology perpendicular to the substrate surface. Capacitance-Voltage hysteresis loop measurements show also a typical characteristics of ferroelectric thin film. The dielectric constant is found to be 528 for the 0.48 mu m thickness of PZT thin film.
引用
收藏
页码:56 / 61
页数:6
相关论文
共 50 条
  • [31] Microstructure and electrical properties of Pb(Zr0.52Ti0.48)O3 ferroelectric films on different bottom electrodes
    Li, JK
    Yao, X
    MATERIALS LETTERS, 2004, 58 (27-28) : 3447 - 3450
  • [32] Nano-indentation fracture test of Pb(Zr0.52Ti0.48)O3 ferroelectric thin films
    Zheng, XJ
    Zhou, YC
    Li, JY
    ACTA MATERIALIA, 2003, 51 (14) : 3985 - 3997
  • [33] In situ laser annealing during growth of Pb(Zr0.52Ti0.48)O3 thin films
    Rajashekhar, Adarsh
    Fox, Austin
    Bharadwaja, S. S. N.
    Trolier-McKinstry, Susan
    APPLIED PHYSICS LETTERS, 2013, 103 (03)
  • [34] Polarization fatigue and photoinduced current in (Pb0.72La0.28)Ti0.93O3 buffered Pb(Zr0.52Ti0.48)O3 films on platinized silicon
    Zheng, Fengang
    Shen, Mingrong
    Fang, Liang
    Wu, Xinglong
    Cao, Wenwu
    MATERIALS RESEARCH BULLETIN, 2009, 44 (04) : 803 - 806
  • [35] Coercive field of ultrathin Pb(Zr0.52Ti0.48)O3 epitaxial films
    Pertsev, NA
    Contreras, JR
    Kukhar, VG
    Hermanns, B
    Kohlstedt, H
    Waser, R
    APPLIED PHYSICS LETTERS, 2003, 83 (16) : 3356 - 3358
  • [36] Nanocrystalline Pb(Zr0.52Ti0.48)O3 Ferroelectric Ceramics: Mechanical and Electrical Properties
    Ramana, M. Venkata
    Reddy, M. Penchal
    Reddy, N. Ramamanohar
    Kumar, K. V. Siva
    Murthy, V. R. K.
    Murty, B. S.
    JOURNAL OF NANOMATERIALS, 2010, 2010
  • [37] Ferroelectric properties of the flexible Pb(Zr0.52Ti0.48)O3 thin film on mica
    Qi, Hongyan
    Xia, Xin
    Zhou, Changlin
    Xiao, Pengcheng
    Wang, Yun
    Deng, Yongju
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2020, 31 (04) : 3042 - 3047
  • [38] Dielectric Properties of Lanthanum Doped Pb(Zr0.52Ti0.48)O3 Ferroelectric Nanoceramics
    Prabu, M.
    Jeniffa, R.
    Gobalakrishnan, S.
    Praseetha, P. K.
    Arun, T.
    NANOSCIENCE AND NANOTECHNOLOGY LETTERS, 2016, 8 (09) : 723 - 728
  • [39] Fatigue and refresh characteristics of Pb(Zr0.52Ti0.48)O3 thin films
    Chae, BG
    Lee, SJ
    Yang, YS
    Kim, SH
    Jang, MS
    JOURNAL OF THE KOREAN PHYSICAL SOCIETY, 1997, 31 (06) : 874 - 878
  • [40] Ferroelectric properties of the flexible Pb(Zr0.52Ti0.48)O3 thin film on mica
    Hongyan Qi
    Xin Xia
    Changlin Zhou
    Pengcheng Xiao
    Yun Wang
    Yongju Deng
    Journal of Materials Science: Materials in Electronics, 2020, 31 : 3042 - 3047