The light-induced hydrogen evolution (LIHE) from amorphous (a-) Si:H by the order of at. % is observed during white light soaking (WLS) of 100-400 mW/cm(2) at 350-500K or ultra violet light soaking (UVLS) of 30-120 mW/cm(2) at 305-320K in a vacuum. The thermal desorption spectroscopy indicates that LIHE originated from bonded hydrogen takes place through the diffusion of light-induced mobile hydrogen (LIMH) with the activation energy of 0.5 eV. LIMH is assigned to bond centered hydrogen and the hydrogen diffusion process becomes prominent when LIMH can leave from a-Si:H such under light soaking in a vacuum above room temperature. For H-2 in microvoids, the hydrogen evolution rate is governed by the surface barrier and its activation energy of 1.0 eV in dark decreases to 0.4 eV under WLS or UVLS. (C) 2014 AIP Publishing LLC.