Hydride Reorientation and Delayed Hydride Cracking of Spent Fuel Rods in Dry Storage

被引:4
|
作者
Kim, Young S. [1 ]
机构
[1] Korea Atom Energy Res Inst, Nucl Mat Res Div, Taejon 305353, South Korea
关键词
PRESSURE TUBE MATERIAL; ZIRCONIUM ALLOYS; TERMINAL SOLUBILITY; HYDROGEN; PRECIPITATION; TEMPERATURE; STRESS; DISSOLUTION; OXIDATION; BEHAVIOR;
D O I
10.1007/s11661-009-0044-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this work is to investigate the effect of thermal creep during vacuum drying of spent fuel rods on hydride reorientation and their delayed hydride cracking (DHC) susceptibility. To these ends, we analyzed Tsai's thermal creep results of irradiated Zircaloy-4 cladding segments from two pressurized water reactors and Simpson and Ells' observation where zirconium alloy cladding tube failed during long-term storage at room temperature. On cooling under 190 MPa, the spent fuel rods crept to 3.5 pct strain during vacuum drying showed large radial hydrides, while the ones crept to 0.35 pct strain had very fine radial hydrides. Thus, it is suggested that prior creep deformation promotes hydride reorientation in spent fuel rods on cooling after vacuum drying. Evidence for this suggestion is provided by a model experiment. Considering Kim's DHC model and experimental facts showing precipitation of hydrides even at room temperature at stress raisers, we suggest that spent fuel rods would fail by DHC in dry storage if stress raisers are present inside the cladding on cooling to below 180 degrees C, and then axial splits of the failed spent fuel rods would occur by DHC due to fuel expansion by UO2 oxidation.
引用
收藏
页码:2867 / 2875
页数:9
相关论文
共 50 条
  • [41] Evolution of Spent Fuel Dry Storage
    Standring, Paul Nicholas
    Takats, Ferenc
    ATW-INTERNATIONAL JOURNAL FOR NUCLEAR POWER, 2016, 61 (11): : 673 - 678
  • [42] SALINE HYDRIDE VEHICULAR FUEL STORAGE SYSTEMS
    RUDMAN, PS
    ENERGY CONVERSION, 1975, 14 (3-4): : 97 - 102
  • [43] DRY STORAGE OF DIORIT SPENT FUEL
    OSPINA, C
    ATOMWIRTSCHAFT-ATOMTECHNIK, 1983, 28 (11): : 569 - 570
  • [44] DRY CASK STORAGE OF SPENT FUEL
    ARITOMI, M
    AOKI, S
    SAEGUSA, T
    KAWASAKI, R
    JOURNAL OF THE ATOMIC ENERGY SOCIETY OF JAPAN, 1989, 31 (03): : 331 - 346
  • [45] Effect of specimen pre-cracking method on Delayed Hydride Cracking Rate
    Mieza, J. I.
    De Las Heras, E.
    Arias, M. I.
    Domizzi, G.
    JOURNAL OF NUCLEAR MATERIALS, 2012, 420 (1-3) : 273 - 277
  • [46] PRIMARY HYDRIDE FAILURE OF ZIRCALOY-CLAD FUEL RODS
    JOON, K
    TRANSACTIONS OF THE AMERICAN NUCLEAR SOCIETY, 1972, 15 (01): : 186 - &
  • [47] MODULAR DRY STORAGE OF SPENT FUEL
    BAXTER, JW
    TRANSACTIONS OF THE AMERICAN NUCLEAR SOCIETY, 1982, 41 : 130 - 131
  • [48] EFFECTS OF CRACK TIP STRESS STATES AND HYDRIDE-MATRIX INTERACTION STRESSES ON DELAYED HYDRIDE CRACKING
    PULS, MP
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1990, 21 (11): : 2905 - 2917
  • [49] Effects of δ-hydride precipitation at a crack tip on crack propagation in delayed hydride cracking of Zircaloy-2
    Kubo, T.
    Kobayashi, Y.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 439 (1-3) : 202 - 211
  • [50] DELAYED HYDRIDE CRACKING BEHAVIOR FOR ZIRCALOY-2 PLATE
    MILLS, JW
    HUANG, FH
    ENGINEERING FRACTURE MECHANICS, 1991, 39 (02) : 241 - 257