Hydride Reorientation and Delayed Hydride Cracking of Spent Fuel Rods in Dry Storage

被引:4
|
作者
Kim, Young S. [1 ]
机构
[1] Korea Atom Energy Res Inst, Nucl Mat Res Div, Taejon 305353, South Korea
关键词
PRESSURE TUBE MATERIAL; ZIRCONIUM ALLOYS; TERMINAL SOLUBILITY; HYDROGEN; PRECIPITATION; TEMPERATURE; STRESS; DISSOLUTION; OXIDATION; BEHAVIOR;
D O I
10.1007/s11661-009-0044-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this work is to investigate the effect of thermal creep during vacuum drying of spent fuel rods on hydride reorientation and their delayed hydride cracking (DHC) susceptibility. To these ends, we analyzed Tsai's thermal creep results of irradiated Zircaloy-4 cladding segments from two pressurized water reactors and Simpson and Ells' observation where zirconium alloy cladding tube failed during long-term storage at room temperature. On cooling under 190 MPa, the spent fuel rods crept to 3.5 pct strain during vacuum drying showed large radial hydrides, while the ones crept to 0.35 pct strain had very fine radial hydrides. Thus, it is suggested that prior creep deformation promotes hydride reorientation in spent fuel rods on cooling after vacuum drying. Evidence for this suggestion is provided by a model experiment. Considering Kim's DHC model and experimental facts showing precipitation of hydrides even at room temperature at stress raisers, we suggest that spent fuel rods would fail by DHC in dry storage if stress raisers are present inside the cladding on cooling to below 180 degrees C, and then axial splits of the failed spent fuel rods would occur by DHC due to fuel expansion by UO2 oxidation.
引用
收藏
页码:2867 / 2875
页数:9
相关论文
共 50 条
  • [31] Numerical modeling of delayed hydride cracking in zirconium alloys
    Varias, AG
    Massih, AR
    ADVANCES IN MECHANICAL BEHAVIOUR, PLASTICITY AND DAMAGE, VOLS 1 AND 2, PROCEEDINGS, 2000, : 1219 - 1224
  • [32] Preventing Stress Corrosion Cracking of Spent Nuclear Fuel Dry Storage Canisters
    Hackel, Lloyd
    Rankin, Jon
    Walter, Matt
    Dane, C. Brent
    Neuman, William
    Oneid, Pierre
    Thomas, Garreth
    Bidrawn, Fred
    FATIGUE DESIGN 2019, INTERNATIONAL CONFERENCE ON FATIGUE DESIGN, 8TH EDITION, 2019, 19 : 346 - 361
  • [33] The critical length of the hydride cluster in delayed hydride cracking of Zr-2.5wt% Nb
    D. Yan
    R. L. Eadie
    Journal of Materials Science, 2000, 35 : 5667 - 5672
  • [34] Zirconium hydride phase mapping in Zircaloy-2 cladding after delayed hydride cracking
    Colldeweih, Aaron W.
    Makowska, Malgorzata G.
    Tabai, Omaia
    Sanchez, Dario Ferreira
    Bertsch, Johannes
    MATERIALIA, 2023, 27
  • [35] EFFECT OF STRESS ON HYDRIDE PRECIPITATION IN ZIRCONIUM-2.5-PERCENT NIOBIUM AND ON DELAYED HYDRIDE CRACKING
    EADIE, RL
    COLEMAN, CE
    SCRIPTA METALLURGICA, 1989, 23 (11): : 1865 - 1870
  • [36] The critical length of the hydride cluster in delayed hydride cracking of Zr-2.5wt% Nb
    Yan, D
    Eadie, RL
    JOURNAL OF MATERIALS SCIENCE, 2000, 35 (22) : 5667 - 5672
  • [37] Hydride morphology and striation formation during delayed hydride cracking in Zr-2.5% Nb
    Shek, GK
    Jovanovic, MT
    Seahra, H
    Ma, Y
    Li, D
    Eadie, RL
    JOURNAL OF NUCLEAR MATERIALS, 1996, 231 (03) : 221 - 230
  • [38] Investigation of resistance of nuclear fuel cladding to hydride cracking
    Makarevicius, V.
    Grybenas, A.
    Kriukiene, R.
    MECHANIKA, 2010, (05): : 25 - 30
  • [39] UNCERTAINTY QUANTIFICATION FOR THE DEVELOPMENT OF MECHANISTIC HYDRIDE BEHAVIOR MODEL FOR SPENT FUEL CLADDING STORAGE AND TRANSPORTATION
    Duchnowski, Edward M.
    Bin Seo, Seok
    Brown, Nicholas R.
    PROCEEDINGS OF THE 2020 INTERNATIONAL CONFERENCE ON NUCLEAR ENGINEERING (ICONE2020), VOL 3, 2020,
  • [40] Spent fuel dry storage in Hungary
    Takáts, F
    Buday, G