摘要
The aim of this work is to investigate the effect of thermal creep during vacuum drying of spent fuel rods on hydride reorientation and their delayed hydride cracking (DHC) susceptibility. To these ends, we analyzed Tsai's thermal creep results of irradiated Zircaloy-4 cladding segments from two pressurized water reactors and Simpson and Ells' observation where zirconium alloy cladding tube failed during long-term storage at room temperature. On cooling under 190 MPa, the spent fuel rods crept to 3.5 pct strain during vacuum drying showed large radial hydrides, while the ones crept to 0.35 pct strain had very fine radial hydrides. Thus, it is suggested that prior creep deformation promotes hydride reorientation in spent fuel rods on cooling after vacuum drying. Evidence for this suggestion is provided by a model experiment. Considering Kim's DHC model and experimental facts showing precipitation of hydrides even at room temperature at stress raisers, we suggest that spent fuel rods would fail by DHC in dry storage if stress raisers are present inside the cladding on cooling to below 180 degrees C, and then axial splits of the failed spent fuel rods would occur by DHC due to fuel expansion by UO2 oxidation.
引用
收藏
页码:2867 / 2875
页数:9
相关论文
共 50 条
  • [1] Hydride Reorientation and Delayed Hydride Cracking of Spent Fuel Rods in Dry Storage
    Young S. Kim
    Metallurgical and Materials Transactions A, 2009, 40 : 2867 - 2875
  • [2] Delayed hydride cracking of spent fuel rods in dry storage
    Kim, Young Suk
    JOURNAL OF NUCLEAR MATERIALS, 2008, 378 (01) : 30 - 34
  • [3] Delayed hydride cracking assessment of PWR spent fuel during dry storage
    Hong, Jong-Dae
    Kim, Hyo-Chan
    Kim, Ju-Seong
    Yang, Yong-Sik
    Kook, Dong-Hak
    NUCLEAR ENGINEERING AND DESIGN, 2017, 322 : 324 - 330
  • [4] Rupture of spent fuel Zircaloy cladding in dry storage due to delayed hydride cracking
    Chao, C. K.
    Yang, K. C.
    Tseng, C. C.
    NUCLEAR ENGINEERING AND DESIGN, 2008, 238 (01) : 124 - 129
  • [5] Improvement of delayed hydride cracking assessment of PWR spent fuel during dry storage
    Hong, Jong-Dae
    Yang, Yong-Sik
    Kook, Donghak
    NUCLEAR ENGINEERING AND TECHNOLOGY, 2020, 52 (03) : 614 - 620
  • [6] Is Spent Nuclear Fuel Immune from Delayed Hydride Cracking during Dry Storage? An IAEA Coordinated Research Project
    Coleman, Christopher E.
    Markelov, Vladimir A.
    Roth, Maria
    Makarevicius, Vidas
    He, Zhang
    Chakravartty, Jayanta Kumar
    Alvarez-Holston, Anna-Maria
    Ali, Liaqat
    Ramanathan, Lalgudi
    Inozemtsev, Victor
    ZIRCONIUM IN THE NUCLEAR INDUSTRY: 18TH INTERNATIONAL SYMPOSIUM, 2018, 1597 : 1224 - 1251
  • [7] Delayed-hydride cracking (DHC) of cladding materials: An analysis for storage and disposal of spent nuclear fuel
    Ahn, Tae M.
    NUCLEAR ENGINEERING AND DESIGN, 2019, 350 : 128 - 136
  • [8] THE EFFECTS OF CREEP AND HYDRIDE ON SPENT FUEL INTEGRITY DURING INTERIM DRY STORAGE
    Kim, Hyun-Gil
    Jeong, Yong-Hwan
    Kim, Kyu-Tae
    NUCLEAR ENGINEERING AND TECHNOLOGY, 2010, 42 (03) : 249 - 258
  • [9] Characteristics of hydride precipitation and reorientation in spent-fuel cladding
    Chung, HM
    Daum, RS
    Hiller, JM
    Billone, MC
    ZIRCONIUM IN THE NUCLEAR INDUSTRY: THIRTEENTH INTERNATIONAL SYMPOSIUM, 2002, 1423 : 561 - 580
  • [10] Stress-induced Hydride Reorientation and Cracking in Fuel Cladding Tube
    Grybenas, Albertas
    Makarevicius, Vidas
    Kaliatka, Tadas
    Dundulis, Gintautas
    Kriukiene, Rita
    MATERIALS SCIENCE-MEDZIAGOTYRA, 2014, 20 (04): : 403 - 408