Changes in the adhesion strength between copper thin films and polyimide substrates after heat treatment

被引:17
|
作者
Iwamori, S
Miyashita, T
Fukuda, S
Nozaki, S
Sudoh, K
Fukuda, N
机构
[1] Central Research Institute, Mitsui Toatsu Chemicals, Inc., Yokohama, 247, 1190 Kasama-cho, Sakae-ku
关键词
copper; polyimide; adhesion strength; weak boundary layer;
D O I
10.1163/156856197X00912
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The adhesion strength between a copper (Cu) thin film and a polyimide [pyromellitic dianhydride-oxydianiline (PMDA-ODA)] substrate is reduced by heat treatment at 150 degrees C in air. In this work, we determined the changes in adhesion strength between Cu films and polyimide substrates using Auger electron spectroscopy (AES), attenuated total reflection Fourier-transform infrared spectroscopy Fm), and X-ray photoelectron spectroscopy (XPS). The analysis showed that the weak boundary layer (WBL) shifted towards the Cu interface as the hear treatment time was increased. To confirm this shift, we looked at two other polyimide substrates: biphenyl dianhydride-p-phenylene diamine (BPDA-PDA) and biphenyl dianhydride-oxydianiline (BPDA-ODA). Comparing the adhesion strength for the Cu thin film, the adhesion strength was high for the Cu/PMDA-ODA and Cu/BPDA-ODA laminates, but very low for the Cu/BPDA-PDA laminate. One of the possible reasons for this behavior could be that the ether moiety between the two benzene rings in ODA is related to the adhesion between a Cu film and an O-2-plasma-treated polyimide (PI) substrate. The relationship between the adhesion strength and chemical bonding states is also discussed. We conclude that a Cu thin film sputtered onto a PI substrate is apt to peel at the oxidized interface, due to the heat treatment.
引用
收藏
页码:783 / 795
页数:13
相关论文
共 50 条
  • [21] Adhesion of RF bias-sputtered Cr thin films onto photosensitive polyimide substrates
    Kim, SY
    Kim, YH
    Yoon, CS
    [J]. ADVANCES IN ELECTRONIC MATERIALS AND PACKAGING 2001, 2001, : 202 - 207
  • [22] Influence of the substrate position angle on the adhesion of ZnO thin films deposited on polyimide foil substrates
    Hu Changji
    Zhu Daoyun
    He Zhenhui
    Fu Weichun
    Zhong Qi
    [J]. APPLIED SURFACE SCIENCE, 2011, 257 (07) : 2801 - 2805
  • [23] Thermal contact resistance and adhesion studies on thin copper films on alumina substrates
    Sakami, D
    Lahmar, A
    Scudeller, Y
    Danes, F
    Bardon, JP
    [J]. JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2001, 15 (12) : 1403 - 1416
  • [24] Effects of current density on adhesion of copper electrodeposits to polyimide substrates
    G. A. Prentice
    K. S. Chen
    [J]. Journal of Applied Electrochemistry, 1998, 28 : 971 - 977
  • [25] Effects of current density on adhesion of copper electrodeposits to polyimide substrates
    Prentice, GA
    Chen, KS
    [J]. JOURNAL OF APPLIED ELECTROCHEMISTRY, 1998, 28 (09) : 971 - 977
  • [26] Correction to: Study on Aging Effect of Adhesion Strength Between Polyimide Film and Copper Layer
    Seok-Bon Koo
    Chang-Myeon Lee
    Sang-Jun Kwon
    Jun-Mi Jeon
    Jin-young Hur
    Hong-Kee Lee
    [J]. Metals and Materials International, 2019, 25 : 821 - 821
  • [27] Enhanced adhesion of plasma-sputtered copper films on polyimide substrates by oxygen glow discharge for microelectronics
    Lin, Y. -S.
    Liu, H. -M.
    [J]. THIN SOLID FILMS, 2008, 516 (08) : 1773 - 1780
  • [28] Improvement of the adhesion to polyimide substrates of copper films prepared by an ion beam and vapor deposition (IVD) method
    Ebe, A
    Takahashi, E
    Iwamoto, Y
    Kuratani, N
    Nishiyama, S
    Imai, O
    Ogata, K
    Setsuhara, Y
    Miyake, S
    [J]. THIN SOLID FILMS, 1996, 281 : 356 - 359
  • [29] An Assessment of Surface Treatments for Adhesion of Polyimide Thin Films
    Cen-Puc, Marco
    Schander, Andreas
    Gleason, Minerva G. Vargas
    Lang, Walter
    [J]. POLYMERS, 2021, 13 (12)
  • [30] EXPERIMENT PLANNING FOR EFFECTS OF HEAT-TREATMENT CONDITIONS ON STRENGTH OF POLYIMIDE FILMS
    SMIRNOVA, VE
    BESSONOV, MN
    KOTON, MM
    [J]. INDUSTRIAL LABORATORY, 1977, 43 (01): : 98 - 99