摘要
This in vitro study assessed the adherence of glass-ionomer cement (GIC) root canal sealers to dentin conditioned by three endodontic intracanal medications. Three GIC sealers were used: (i) Ketac-Endo; (ii) KT-308, an experimental GIC sealer; and (iii) ZUT, a combination of KT-308 and a silver-containing zeolite (0.2% by weight). Superficial dentin of 120 bovine incisor crowns was used as a substrate. The dentin was irrigated with 2.6% NaOCl for 30 s and then blotted dry. One of the following conditioning media (n = 30) was maintained in contact with the dentin for 7 days: (i) Ca(OH), paste; (ii) chlorhexidine gluconate (CHX) liquid 0.12%; (iii) formocresol (FML) liquid; (iv) distilled water (dH(2)O) used as control. The GIC sealers were applied to the conditioned dentin, bench set for 90 min, stored in 100% humidity at 37 degreesC for 48 h, then tested to failure for shear bond strength (MPa) in an Instron machine. In the ZUT specimens, the shear bond strength did not differ significantly among those conditioned with Ca(OH)(2), CHX, FML, and dH(2)O. For KT-308, the mean scores were significantly lower (p < 0.05) after conditioning with CHX than with dH(2)O. For Ketac-Endo, the mean scores were significantly lower after conditioning with Ca(OH)(2) and FML than with dH(2)O (p < 0.05). Furthermore Ketac-Endo demonstrated significantly lower (p < 0.05) shear bond strength than KT-308 or ZUT to the dentin conditioned with Ca(OH)(2) or FML. The results suggest that intracanal medications differentially influence the adhesion of various GIC sealers to root canal dentin.
引用
收藏
页码:85 / 88
页数:4
相关论文
共 50 条
  • [41] Interaction of glass-ionomer cements with moist dentin
    Yiu, CKY
    Tay, FR
    King, NM
    Pashley, DH
    Sidhu, SK
    Neo, JCL
    Toledano, M
    Wong, SL
    JOURNAL OF DENTAL RESEARCH, 2004, 83 (04) : 283 - 289
  • [42] ADHESION OF A GLASS-IONOMER SEALANT TO ENAMEL
    CLARK, N
    SHEN, C
    MJOR, IA
    JOURNAL OF DENTAL RESEARCH, 1995, 74 : 247 - 247
  • [43] TOXICITY TO THE PULP OF A GLASS-IONOMER CEMENT
    BURKE, FJT
    BRITISH DENTAL JOURNAL, 1987, 163 (06) : 180 - 180
  • [44] TOXICITY TO THE PULP OF A GLASS-IONOMER CEMENT
    KNIBBS, PJ
    BRITISH DENTAL JOURNAL, 1987, 163 (02) : 40 - 40
  • [45] Milestones in adhesion: Glass-ionomer cements
    Tyas, MJ
    JOURNAL OF ADHESIVE DENTISTRY, 2003, 5 (04): : 259 - 266
  • [46] SHEAR BOND STRENGTH AND MARGINAL MICROLEAKAGE OF GLASS-IONOMER CEMENT AFTER DENTIN TREATMENT
    PRATI, C
    NUCCI, C
    MONTANARI, G
    JOURNAL OF DENTAL RESEARCH, 1989, 68 (04) : 627 - 627
  • [47] Comparative Evaluation of Osteogenic Potential of Conventional Glass-ionomer Cement with Chitosan-modified Glass-ionomer and Bioactive Glass-modified Glass-ionomer Cement - An In vitro Study
    Ranjani, Muthukrishnan Sudharshana
    Kavitha, Mahendran
    Venkatesh, Srinivasan
    CONTEMPORARY CLINICAL DENTISTRY, 2021, 12 (01) : 32 - 36
  • [48] Effect of saliva contamination on the bond of dentin to resin-modified glass-ionomer cement
    Safar, JA
    Davis, RD
    Overton, JD
    OPERATIVE DENTISTRY, 1999, 24 (06) : 351 - 357
  • [49] Effect of Dentin Sealers on Postoperative Sensitivity of Complete Cast Crowns Cemented with Glass Ionomer Cement
    Maghrabi, Abdulhamaid A.
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2011, 20 (05): : 385 - 390
  • [50] Adhesion evaluation of a glass ionomer cement compared with different root canal sealers.
    Najar, AL
    Vansan, LP
    Neto, MDS
    Saquy, PC
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : A250 - A250