摘要
This in vitro study assessed the adherence of glass-ionomer cement (GIC) root canal sealers to dentin conditioned by three endodontic intracanal medications. Three GIC sealers were used: (i) Ketac-Endo; (ii) KT-308, an experimental GIC sealer; and (iii) ZUT, a combination of KT-308 and a silver-containing zeolite (0.2% by weight). Superficial dentin of 120 bovine incisor crowns was used as a substrate. The dentin was irrigated with 2.6% NaOCl for 30 s and then blotted dry. One of the following conditioning media (n = 30) was maintained in contact with the dentin for 7 days: (i) Ca(OH), paste; (ii) chlorhexidine gluconate (CHX) liquid 0.12%; (iii) formocresol (FML) liquid; (iv) distilled water (dH(2)O) used as control. The GIC sealers were applied to the conditioned dentin, bench set for 90 min, stored in 100% humidity at 37 degreesC for 48 h, then tested to failure for shear bond strength (MPa) in an Instron machine. In the ZUT specimens, the shear bond strength did not differ significantly among those conditioned with Ca(OH)(2), CHX, FML, and dH(2)O. For KT-308, the mean scores were significantly lower (p < 0.05) after conditioning with CHX than with dH(2)O. For Ketac-Endo, the mean scores were significantly lower after conditioning with Ca(OH)(2) and FML than with dH(2)O (p < 0.05). Furthermore Ketac-Endo demonstrated significantly lower (p < 0.05) shear bond strength than KT-308 or ZUT to the dentin conditioned with Ca(OH)(2) or FML. The results suggest that intracanal medications differentially influence the adhesion of various GIC sealers to root canal dentin.
引用
收藏
页码:85 / 88
页数:4
相关论文
共 50 条
  • [21] INCREASED BONDING OF A GLASS-IONOMER CEMENT TO DENTIN BY MEANS OF FECL3
    SHALABI, HS
    ASMUSSEN, E
    JORGENSEN, KD
    SCANDINAVIAN JOURNAL OF DENTAL RESEARCH, 1981, 89 (04): : 348 - 353
  • [22] EFFECT OF DENTINAL PRETREATMENT ON BOND STRENGTH BETWEEN GLASS-IONOMER CEMENT AND DENTIN
    JOYNT, RB
    DAVIS, EL
    WIECZKOWSKI, G
    PIERCE, L
    OPERATIVE DENTISTRY, 1990, 15 (05) : 173 - 177
  • [23] Bioactive glass-ionomer cement with potential therapeutic function to dentin capping mineralization
    Xie, Dong
    Zhao, Jun
    Weng, Yiming
    Park, Jong-Gu
    Jiang, Hui
    Platt, Jeffrey A.
    EUROPEAN JOURNAL OF ORAL SCIENCES, 2008, 116 (05) : 479 - 487
  • [24] THE CLINICAL DISINTEGRATION OF A GLASS-IONOMER CEMENT
    EARL, MSA
    IBBETSON, RJ
    BRITISH DENTAL JOURNAL, 1986, 161 (08) : 287 - 291
  • [25] THE CLINICAL DISINTEGRATION OF A GLASS-IONOMER CEMENT
    SIGRIST, J
    BRITISH DENTAL JOURNAL, 1987, 162 (03) : 92 - 92
  • [26] THE CLINICAL DISINTEGRATION OF A GLASS-IONOMER CEMENT
    EARL, M
    BRITISH DENTAL JOURNAL, 1987, 162 (06) : 209 - 210
  • [27] THE CLINICAL DISINTEGRATION OF A GLASS-IONOMER CEMENT
    IBBETSON, RJ
    BRITISH DENTAL JOURNAL, 1987, 162 (05) : 175 - 176
  • [28] DOWEL RETENTION WITH GLASS-IONOMER CEMENT
    KRUPP, JD
    CAPUTO, AA
    TRABERT, KC
    STANDLEE, JP
    JOURNAL OF PROSTHETIC DENTISTRY, 1979, 41 (02): : 163 - 166
  • [29] THE BIOCOMPATIBILITY OF A RADIOPAQUE GLASS-IONOMER CEMENT
    JONCK, LM
    FERREIRA, MR
    SCHERMAN, B
    JOURNAL OF DENTAL RESEARCH, 1987, 66 (04) : 945 - 945
  • [30] Development of glass-ionomer cement systems
    Smith, DC
    BIOMATERIALS, 1998, 19 (06) : 467 - 478