On the CVD of MoSi2:: an experimental study from the MoCl4-SiCl4-H2-Ar precursor with a view to the preparation of C/MoSi2/SiC and SiC/MoSi2/SiC microcomposites

被引:1
|
作者
Bobet, JL [1 ]
Vignoles, G [1 ]
Langlais, F [1 ]
Naslain, R [1 ]
机构
[1] Lab Composites Thermostruct, CNRS, UMR 47, UB1, F-33600 Pessac, France
关键词
Brittle; Chemical Vapour Deposition; Surface Reaction; Phase Coating; Heterogeneous Surface;
D O I
10.1023/A:1004560232166
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The chemical vapour deposition of MoSi2 on plane substrates (graphite or sintered-SiC) and ceramic fibres has been studied from MoCl4SiCl4-H-2-Ar gas mixtures at 900 < T < 1400 degrees C and 2 < P< 40 kPa, according to an experimental approach. MoSi2 is deposited as single phase coatings for 2.5 < alpha = PSiCl4/PMoCl4 < 10 and 10 < beta = P-H2/(P-MoCl4 + P-SiCl4) < 20. The deposition process appears to be thermally activated, the thermal variations of the growth rate obeying one or two Arrhenius law(s) depending on P. It seems to remain rate controlled by heterogeneous surface reactions as long as the gas flow-rate is high enough. Deposits with a smooth surface aspect and homogeneous in thickness are obtained at low T, low P and high H-2-dilution. Nicalon/MoSi2/SiC and C(T300)/MoSi2/SiC microcomposites are prepared and tested in tensile loading at ambient and high temperatures. They exhibit a brittle or quasi-brittle mechanical behaviour, with no (or almost no) matrix microcracking before failure. It is anticipated that dense MoSi2 deposited by CVD may not be a suitable interphase material for SiC/SiC and C/SiC composite materials. (C) 1998 Kluwer Academic Publishers.
引用
收藏
页码:4461 / 4473
页数:13
相关论文
共 50 条
  • [41] Preparation of SiC/MoSi2 composites by mechanical alloying and its fracture properties
    Wu, Hsin-Ming
    Hu, Chia-Jung
    Chou, Ya-Hui
    THERMEC 2006, PTS 1-5, 2007, 539-543 : 1047 - +
  • [42] Comparative study on high-temperature oxidation behavior of MoSi2 and MoSi2/SiC-Mo2C composite coatings on Mo substrates at 1300 °C
    Huang, Yan
    Zhai, Ruixiong
    Huang, Taihong
    Pei, Hezhong
    He, Xuan
    Wan, Fayang
    Song, Peng
    SURFACE & COATINGS TECHNOLOGY, 2023, 458
  • [43] Instability of Si3N4/, SiC/, and MoSi2/ethanol suspensions
    Yoko Fukada
    Patrick S. Nicholson
    Journal of Materials Research, 2003, 18 : 45 - 52
  • [44] Instability of Si3N4/, SiC/, and MoSi2/ethanol suspensions
    Fukada, Y
    Nicholson, PS
    JOURNAL OF MATERIALS RESEARCH, 2003, 18 (01) : 45 - 52
  • [45] Influence of Nowonty phase on the fracture toughness of SiC/MoSi2 composites
    Kang, Pengchao
    Wu, Gaohui
    Yin, Zhongda
    PROGRESSES IN FRACTURE AND STRENGTH OF MATERIALS AND STRUCTURES, 1-4, 2007, 353-358 : 1326 - 1329
  • [46] Hardness and fracture toughness of SiC-preforms infiltrated with MoSi2
    Pánek, Z
    FRACTOGRAPHY OF ADVANCED CERAMICS, 2002, 223 : 215 - 219
  • [47] Tensile creep and creep rupture of SiC-reinforced MoSi2
    French, Jonathan D.
    Wiederhorn, Sheldon M.
    Petrovic, John J.
    Ceramic Engineering and Science Proceedings, 1995, 16 (04): : 129 - 136
  • [48] SiC颗粒强韧化MoSi2复合材料
    刘伯威
    潘进
    樊毅
    张金生
    复合材料学报, 2002, (01) : 59 - 63
  • [49] Synthesis of SiC/MOSi2 composite by mechanical alloying and reactive sintering
    Kang, PC
    Yin, ZD
    Li, MW
    Jiang, Y
    RARE METAL MATERIALS AND ENGINEERING, 2005, 34 (12) : 1974 - 1977
  • [50] Oxidation of SiOC/MoSi2/SiC composites prepared by polymer pyrolysis
    Lee, DB
    Kim, DJ
    OXIDATION OF METALS, 2004, 61 (5-6): : 423 - 437