摘要
The chemical vapour deposition of MoSi2 on plane substrates (graphite or sintered-SiC) and ceramic fibres has been studied from MoCl4SiCl4-H-2-Ar gas mixtures at 900 < T < 1400 degrees C and 2 < P< 40 kPa, according to an experimental approach. MoSi2 is deposited as single phase coatings for 2.5 < alpha = PSiCl4/PMoCl4 < 10 and 10 < beta = P-H2/(P-MoCl4 + P-SiCl4) < 20. The deposition process appears to be thermally activated, the thermal variations of the growth rate obeying one or two Arrhenius law(s) depending on P. It seems to remain rate controlled by heterogeneous surface reactions as long as the gas flow-rate is high enough. Deposits with a smooth surface aspect and homogeneous in thickness are obtained at low T, low P and high H-2-dilution. Nicalon/MoSi2/SiC and C(T300)/MoSi2/SiC microcomposites are prepared and tested in tensile loading at ambient and high temperatures. They exhibit a brittle or quasi-brittle mechanical behaviour, with no (or almost no) matrix microcracking before failure. It is anticipated that dense MoSi2 deposited by CVD may not be a suitable interphase material for SiC/SiC and C/SiC composite materials. (C) 1998 Kluwer Academic Publishers.
引用
收藏
页码:4461 / 4473
页数:13
相关论文
共 50 条
  • [31] MoSi2与MoSi2-SiC的扫描电镜研究
    杨生荣
    吕晋军
    阎逢元
    林新华
    电子显微学报, 2000, (04) : 601 - 602
  • [32] WEIBULL ANALYSIS OF FLEXURAL STRENGTH OF A SIC/MOSI2 COMPOSITE
    TING, JM
    SCRIPTA METALLURGICA ET MATERIALIA, 1993, 29 (05): : 677 - 682
  • [33] Impression creep behavior of SiC particle MoSi2 composites
    Butt, DP
    Korzekwa, DA
    Maloy, SA
    Kung, H
    Petrovic, JJ
    JOURNAL OF MATERIALS RESEARCH, 1996, 11 (06) : 1528 - 1536
  • [34] Residual stress investigation in SiC/MOSi2(p) composites
    Sciti, Diletta
    Guicciardi, Stefano
    Celotti, Giancarlo
    Deluca, Marco
    Pezzotti, Giuseppe
    ADVANCED ENGINEERING MATERIALS, 2007, 9 (05) : 393 - 399
  • [35] SiC对MoSi2烧结行为的影响
    张厚安
    王德志
    刘心宇
    功能材料, 1999, (01) : 107 - 108
  • [36] SiC颗粒强韧MoSi2复合材料
    郑灵仪,金燕苹,李鹏兴,王本民,金璐
    无机材料学报, 1994, (02) : 232 - 238
  • [37] CONTACT STRENGTH AND CRACK FORMATION IN MONOLITHIC SiC AND MoSi2
    Hegeduesova, Lucia
    Ceniga, Ladislav
    Dusza, Jan
    CHEMICKE LISTY, 2011, 105 : S802 - S803
  • [38] Hardness and toughness of MoSi2 and MoSi2-SiC composite prepared by reactive sintering of powders
    Morris, DG
    Leboeuf, M
    Morris, MA
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 251 (1-2): : 262 - 268
  • [39] Preparation of MoSi2–SiC–ZrB2 Structural Ceramics by Free Sintering
    M. A. Markov
    S. S. Ordan’yan
    S. V. Vikhman
    S. N. Perevislov
    A. V. Krasikov
    A. D. Bykova
    M. V. Staritsyn
    Refractories and Industrial Ceramics, 2019, 60 : 385 - 388
  • [40] 原位合成MoSi2反应烧结SiC-MoSi2复合材料
    郜剑英
    蒋明学
    王刚
    江莞
    耐火材料, 2003, (05) : 259 - 261+266