摘要
The chemical vapour deposition of MoSi2 on plane substrates (graphite or sintered-SiC) and ceramic fibres has been studied from MoCl4SiCl4-H-2-Ar gas mixtures at 900 < T < 1400 degrees C and 2 < P< 40 kPa, according to an experimental approach. MoSi2 is deposited as single phase coatings for 2.5 < alpha = PSiCl4/PMoCl4 < 10 and 10 < beta = P-H2/(P-MoCl4 + P-SiCl4) < 20. The deposition process appears to be thermally activated, the thermal variations of the growth rate obeying one or two Arrhenius law(s) depending on P. It seems to remain rate controlled by heterogeneous surface reactions as long as the gas flow-rate is high enough. Deposits with a smooth surface aspect and homogeneous in thickness are obtained at low T, low P and high H-2-dilution. Nicalon/MoSi2/SiC and C(T300)/MoSi2/SiC microcomposites are prepared and tested in tensile loading at ambient and high temperatures. They exhibit a brittle or quasi-brittle mechanical behaviour, with no (or almost no) matrix microcracking before failure. It is anticipated that dense MoSi2 deposited by CVD may not be a suitable interphase material for SiC/SiC and C/SiC composite materials. (C) 1998 Kluwer Academic Publishers.
引用
收藏
页码:4461 / 4473
页数:13
相关论文
共 50 条
  • [1] On the CVD of MoSi2: an experimental study from the MoCl4–SiCl4–H2–Ar precursor with a view to the preparation of C/MoSi2/SiC and SiC/MoSi2/SiC microcomposites
    J. L. Bobet
    G. Vignoles
    F. Langlais
    R. Naslain
    Journal of Materials Science, 1998, 33 : 4461 - 4473
  • [2] Creep behavior of MoSi2 and MoSi2 + SiC composite
    P. Hvizdoš
    J. Dusza
    W. Steinkellner
    K. Kromp
    Journal of Materials Science, 2004, 39 : 4073 - 4077
  • [3] Diffusion boronizing of SiC and MoSi2
    Dzyadykevich, YV
    Bochar, II
    INORGANIC MATERIALS, 1998, 34 (05) : 448 - 451
  • [4] THERMAL-PROPERTIES OF MOSI2 AND SIC WHISKER-REINFORCED MOSI2
    BOSE, S
    HECHT, RJ
    JOURNAL OF MATERIALS SCIENCE, 1992, 27 (10) : 2749 - 2752
  • [5] ABRASIVE WEAR BEHAVIOR OF MOSI2/SIC AND MOSI2/ZRO2 COMPOSITES
    ALMAN, DE
    HAWK, JA
    PETROVIC, JJ
    SCRIPTA METALLURGICA ET MATERIALIA, 1995, 32 (11): : 1765 - 1770
  • [6] Fracture and mechanical properties of MoSi2 and MoSi2+SiC
    Dusza, J
    Kromp, K
    ADVANCES IN FRACTURE AND DAMAGE MECHANICS, 2003, 251-2 : 13 - 18
  • [7] SiC/Si - MoSi2/MoSi2 oxidation protective coating for carbon material at 1700 °C
    Zhao, Juan
    MATERIALS SCIENCE AND ENGINEERING APPLICATIONS, PTS 1-3, 2011, 160-162 : 1 - 6
  • [8] Fracture and mechanical properties of MoSi2 and MoSi2+SiC
    Dusza, J.
    Hvizdos, P.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2006, 44 (05): : 251 - 258
  • [9] Creep behavior of MoSi2 and MoSi2+SiC composite
    Hvizdos, P
    Dusza, J
    Steinkellner, W
    Kromp, K
    JOURNAL OF MATERIALS SCIENCE, 2004, 39 (12) : 4073 - 4077
  • [10] 微波烧结制备MoSi2及SiC/MoSi2纳米复合陶瓷
    刘长虹
    艾云龙
    何文
    宇航材料工艺, 2012, 42 (03) : 54 - 58