Interfacial Bond Behavior of High Strength Concrete Filled Steel Tube after Exposure to Elevated Temperatures and Cooled by Fire Hydrant

被引:8
|
作者
Chen, Zongping [1 ,2 ]
Tang, Jiyu [1 ]
Zhou, Xingyu [1 ]
Zhou, Ji [1 ]
Chen, Jianjia [1 ]
机构
[1] Guangxi Univ, Coll Civil Engn & Architecture, Nanning 530004, Peoples R China
[2] Guangxi Univ, Key Lab Disaster Prevent & Struct Safety, Chinese Minist Educ, Nanning 530004, Peoples R China
基金
中国国家自然科学基金;
关键词
elevated temperatures and water-cooling exposure; high-strength concrete; circular steel tube; bond strength; slip behavior;
D O I
10.3390/ma13010150
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
For the engineering structure in case of fire, a fire hydrant is generally used for extinguishing the fire. This paper presents an experimental investigation on interfacial bond behavior of high-strength concrete-filled steel tube (HSCFST) after exposure to elevated temperatures and cooled by fire hydrant using the pull-out test of 22 specimens. According to the experimental study, the failure mechanism of HSCFST exposed to elevated temperatures and water-cooling (ETWC) was revealed, the influence of various parameters on the bond behavior was analyzed, and the calculation formula of the bond strength of HSCFST subjected to ETWC was put forward. The results show that the load-slip curves of the loading end and the free end of the specimen are basically similar, and can be divided into three types of typical curves. In the push out test, the strain on the outer surface of the steel tube is exponentially distributed with its distance from the loading end. After ETWC exposure, the bond strength of the specimen is less affected by the concrete strength, which is inversely proportional to the anchorage length, and it is basically stable after the constant temperature duration is longer than 60 min. With the increase of the maximum temperature, the ultimate bond strength increases first, then decreases and then increases, and the residual bond strength increases first and then decreases. Besides, the study indicate that cooling method has significant influence on the bond behavior, compared with natural cooling specimens, the ultimate bond strength, residual bond strength, and shear bond stiffness of water-cooling specimens are smaller, and the interfacial energy dissipation capacity is larger.
引用
收藏
页数:23
相关论文
共 50 条
  • [21] Performance of high strength concrete filled steel columns at ambient and elevated temperatures
    Kodur, VKR
    Wang, YC
    TUBULAR STRUCTURES IX, 2001, : 445 - 451
  • [22] Impact tests on dynamic behavior of concrete-filled steel tube at elevated temperatures
    He, Yuan-Ming
    Huo, Jing-Si
    Chen, Bai-Sheng
    Gongcheng Lixue/Engineering Mechanics, 2013, 30 (01): : 52 - 58
  • [23] Mechanical behaviour of ultra-high strength concrete at elevated temperatures and fire resistance of ultra-high strength concrete filled steel tubes
    Xiong, Ming-Xiang
    Liew, J. Y. Richard
    MATERIALS & DESIGN, 2016, 104 : 414 - 427
  • [24] Research on the residual strength of concrete-filled circular steel tube stub columns after exposure to fire
    College of Civil Engineering, Fuzhou Univ, Fuzhou
    Fujian
    350108, China
    Hunan Daxue Xuebao, 9 (42-51):
  • [25] Residual bond strength between steel bars and concrete after elevated temperatures
    Bingol, A. Ferhat
    Gul, Ruestem
    FIRE SAFETY JOURNAL, 2009, 44 (06) : 854 - 859
  • [26] Interface mechanical behavior test and bond strength calculation of high-strength concrete filled circular steel tube
    Ke, Xiaojun
    Sun, Haiyang
    Chen, Zongping
    Su, Yisheng
    Ying, Wudang
    Jianzhu Jiegou Xuebao/Journal of Building Structures, 2015, 36 : 401 - 406
  • [27] Bond behavior of lightweight concrete-filled steel tubes containing rock wool waste after exposure to high temperatures
    Bahrami, Amirreza
    Nematzadeh, Mahdi
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 300
  • [28] Bond behavior between high-strength grout and rebar after exposure to elevated temperatures
    Liu, Lianglin
    Sun, Wenjuan
    Xiao, Jianzhuang
    Li, Weihua
    Jian, Luying
    Zhang, Qing
    STRUCTURES, 2024, 69
  • [29] Tests on the Steel–Concrete Bond Strength in Steel Reinforced Concrete (SRC) Columns After Fire Exposure
    Wei-Hua Wang
    Lin-Hai Han
    Qing-Hua Tan
    Zhong Tao
    Fire Technology, 2017, 53 : 917 - 945
  • [30] Residual bond strength in steel reinforced concrete columns after fire exposure
    Tao, Zhong
    Yu, Qing
    FIRE SAFETY JOURNAL, 2012, 53 : 19 - 27