Interfacial Bond Behavior of High Strength Concrete Filled Steel Tube after Exposure to Elevated Temperatures and Cooled by Fire Hydrant

被引:8
|
作者
Chen, Zongping [1 ,2 ]
Tang, Jiyu [1 ]
Zhou, Xingyu [1 ]
Zhou, Ji [1 ]
Chen, Jianjia [1 ]
机构
[1] Guangxi Univ, Coll Civil Engn & Architecture, Nanning 530004, Peoples R China
[2] Guangxi Univ, Key Lab Disaster Prevent & Struct Safety, Chinese Minist Educ, Nanning 530004, Peoples R China
基金
中国国家自然科学基金;
关键词
elevated temperatures and water-cooling exposure; high-strength concrete; circular steel tube; bond strength; slip behavior;
D O I
10.3390/ma13010150
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
For the engineering structure in case of fire, a fire hydrant is generally used for extinguishing the fire. This paper presents an experimental investigation on interfacial bond behavior of high-strength concrete-filled steel tube (HSCFST) after exposure to elevated temperatures and cooled by fire hydrant using the pull-out test of 22 specimens. According to the experimental study, the failure mechanism of HSCFST exposed to elevated temperatures and water-cooling (ETWC) was revealed, the influence of various parameters on the bond behavior was analyzed, and the calculation formula of the bond strength of HSCFST subjected to ETWC was put forward. The results show that the load-slip curves of the loading end and the free end of the specimen are basically similar, and can be divided into three types of typical curves. In the push out test, the strain on the outer surface of the steel tube is exponentially distributed with its distance from the loading end. After ETWC exposure, the bond strength of the specimen is less affected by the concrete strength, which is inversely proportional to the anchorage length, and it is basically stable after the constant temperature duration is longer than 60 min. With the increase of the maximum temperature, the ultimate bond strength increases first, then decreases and then increases, and the residual bond strength increases first and then decreases. Besides, the study indicate that cooling method has significant influence on the bond behavior, compared with natural cooling specimens, the ultimate bond strength, residual bond strength, and shear bond stiffness of water-cooling specimens are smaller, and the interfacial energy dissipation capacity is larger.
引用
收藏
页数:23
相关论文
共 50 条
  • [1] Residual bond behavior of high strength concrete-filled square steel tube after elevated temperatures
    Chen, Zongping
    Liu, Xiang
    Zhou, Wenxiang
    STEEL AND COMPOSITE STRUCTURES, 2018, 27 (04): : 509 - 523
  • [2] Bond behavior between circular steel tube and high-strength concrete after elevated temperatures
    Zhou, Ji
    Chen, Zongpin
    Ban, Maogen
    Pang, Yunsheng
    STRUCTURAL ENGINEERING AND MECHANICS, 2022, 84 (05) : 575 - 590
  • [3] Bond behavior of recycled aggregate concrete-filled steel tube after elevated temperatures
    Chen, Zongping
    Jia, Hengrui
    Li, Shengxin
    CONSTRUCTION AND BUILDING MATERIALS, 2022, 325
  • [4] Experimental Study on Interface Bond Behavior of High Strength Concrete Filled Circle Steel Tube after Elevated Temperatures and Water Cooling
    Chen Z.
    Zhou J.
    Chen J.
    Ban M.
    Hunan Daxue Xuebao/Journal of Hunan University Natural Sciences, 2021, 48 (03): : 75 - 87
  • [5] Axial compression behavior of rubberized concrete filled steel tube columns after exposure to elevated temperatures
    Xiang, Yong
    Liang, Jiongfeng
    Wang, Caisen
    Wangliu, Haoxiang
    Li, Wei
    SCIENTIFIC REPORTS, 2025, 15 (01):
  • [6] Research on interfacial bond behavior and constitutive equation of recycled aggregate concrete filled circle steel tube after exposure to high temperature
    Jia H.-R.
    Chen Z.-P.
    Chen J.-R.
    Gongcheng Lixue/Engineering Mechanics, 2021, 38 (10): : 119 - 133
  • [7] Bond Behavior of Concrete-Filled Steel Tubes at Elevated Temperatures
    Song, Tian-Yi
    Tao, Zhong
    Han, Lin-Hai
    Uy, Brian
    JOURNAL OF STRUCTURAL ENGINEERING, 2017, 143 (11)
  • [8] Experiment Study on Interfacial Normal Bond Strength of Concrete Filled Steel Tube
    Liu, Zhen-yu
    ADVANCES IN INDUSTRIAL AND CIVIL ENGINEERING, PTS 1-4, 2012, 594-597 : 947 - 954
  • [9] Mechanical behavior of recycled aggregate concrete-filled steel tube stub columns after exposure to elevated temperatures
    Li, Wengui
    Luo, Zhiyu
    Tao, Zhong
    Duan, Wen Hui
    Shah, Surendra P.
    CONSTRUCTION AND BUILDING MATERIALS, 2017, 146 : 571 - 581
  • [10] Bond Behavior between Steel Rebar and RCA Concrete after Exposure to Elevated Temperatures
    Zou, Wanjie
    Liang, Jiongfeng
    Liu, Dawei
    Zhang, Guangwu
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2020, 2020