Evolution of micro-arc oxidation behaviors of the hot-dipping aluminum coatings on Q235 steel substrate

被引:31
|
作者
Lu Lihong [1 ,2 ]
Shen Dejiu [2 ]
Zhang Jingwu [2 ]
Song Jian [3 ]
Li Liang [3 ]
机构
[1] Chinese Peoples Armed Police Acad, Res Dept, Langfang 065000, Peoples R China
[2] Yanshan Univ, Coll Mat Sci & Engn, State Key Lab Metastable Mat Sci & Technol, Qinhuangdao 066004, Peoples R China
[3] Tsinghua Univ, State Key Lab Automot Safety & Energy, Beijing 100084, Peoples R China
关键词
Evolution; Q235; steel; Hot-dipping aluminum; Micro-arc oxidation; Ceramic coatings; PLASMA ELECTROLYTIC OXIDATION; CERAMIC COATINGS; WEAR-RESISTANCE; GROWTH; ALLOY;
D O I
10.1016/j.apsusc.2010.11.187
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Micro-arc oxidation (MAO) is not applicable to prepare ceramic coatings on the surface of steel directly. In this work, hybrid method of MAO and hot-dipping aluminum (HDA) were employed to fabricate composite ceramic coatings on the surface of Q235 steel. The evolution of MAO coatings, such as growth rate, thickness of the total coatings, ingrown and outgrown coatings, cross section and surface morphologies and phase composition of the ceramic coatings were studied. The results indicate that both the current density and the processing time can affect the total thickness, the growth rate and the ratio of ingrown and outgrown thickness of the ceramic coatings. The total thickness, outgrown thickness and growth rate have maximum values with the processing time prolonged. The time when the maximum value appears decreases and the ingrown dominant turns to outgrown dominant little by little with the current density increasing. The composite coatings obtained by this hybrid method consists of three layers from inside to outside, i.e. Fe-Al alloy layer next to the substrate, aluminum layer between the Fe-Al layer and the ceramic coatings which is as the top exterior layer. Metallurgical bonding was observed between every of the two layers. There are many micro-pores and micro-cracks, which act as discharge channels and result of quick and non-uniform cooling of melted sections in the MAO coatings. The phase composition of the ceramic coatings is mainly composed of amorphous phase and crystal Al2O3 oxides. The crystal Al2O3 phase includes kappa-Al2O3, 0-Al2O3 and beta-Al2O3. Compared with the others, the beta-Al2O3 content is the least. The MAO process can be divided into three periods, namely the common anodic oxidation stage, the stable MAO stage and the ceramic coatings destroyed stage. The exterior loose part of the ceramic coatings was destroyed badly in the last period which should be avoided during the MAO process. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:4144 / 4150
页数:7
相关论文
共 50 条
  • [1] Structures of ceramics coatings on steel fabricated by hot-dipping and micro-arc oxidation
    Shen, DJ
    Wang, YL
    Gu, WC
    Xing, GZ
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2004, 14 : 170 - 172
  • [2] TEM analysis and wear resistance of the ceramic coatings on Q235 steel prepared by hybrid method of hot-dipping aluminum and plasma electrolytic oxidation
    Lu Lihong
    Zhang Jingwu
    Shen Dejiu
    Wu Lailei
    Jiang Guirong
    Li Liang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 512 (01) : 57 - 62
  • [3] TEM analysis and corrosion resistance of the ceramic coatings on Q235 steel prepared by hybrid method of hot-dipping aluminum and plasma electrolytic oxidation
    Lu Lihong
    Shen Dejiu
    Zhang Jingwu
    Guo Changhong
    MECHANICAL ENGINEERING AND MATERIALS, PTS 1-3, 2012, 152-154 : 40 - +
  • [4] Influence of micro-arc oxidation process on phase structure and properties of electroplating aluminum coating on Q235 steel
    College of Materials Science and Engineering, Dalian Jiaotong University, Dalian 116028, China
    不详
    Cailiao Rechuli Xuebao, 2008, 5 (169-172):
  • [5] Abrasive wear performance of hot-dipping Al-Mn alloy coatings on Q235
    Dong, Xiaofeng
    Li, Xinmei
    Dong, X. (249166004@qq.com), 2012, Trans Tech Publications Ltd (522) : 13 - 16
  • [6] Effect of current density on micro-arc oxidation of Q235 steel and corrosion resistance in liquid Pb-Bi
    Zhu, Qiang
    He, Ning
    Zhang, Yanchao
    Lei, Yucheng
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2019, 70 (07): : 1171 - 1178
  • [7] Micrographic Properties of Composite Coatings Prepared on TA2 Substrate by Hot-Dipping in Al-Si Alloy and Using Micro-Arc Oxidation Technologies (MAO)
    Wang, Shaopeng
    Zhou, Lian
    Li, Changjiu
    Li, Zhengxian
    Li, Hongzhan
    Yang, Lijing
    COATINGS, 2020, 10 (04)
  • [8] Preparation of Compact Micro-Arc Oxidation Coatings on Aluminum Alloys
    Wu, P. N.
    Xi, J. J.
    Zhao, J.
    Wang, T. J.
    ADVANCES IN FUNCTIONAL MANUFACTURING TECHNOLOGIES, 2010, 33 : 492 - +
  • [9] Process Parameters Optimization for Micro-arc Oxidation of Hot-dip Aluminum Coating on Stainless Steel
    Niu, Zongwei
    Li, Zhiyong
    Li, Li
    Zhang, Jiayou
    Wang, Aihong
    SURFACE FINISHING TECHNOLOGY AND SURFACE ENGINEERING II, 2010, 135 : 190 - +
  • [10] Role of Substrates in the Corrosion Behaviors of Micro-Arc Oxidation Coatings on Magnesium Alloys
    Liu, Cancan
    Yuan, Junwen
    Li, Hongtao
    Jiang, Bailing
    METALS, 2019, 9 (10)