Influence of sodium hypochlorite and EDTA on the microtensile bond strength of a self-etching adhesive system

被引:28
|
作者
Cechin, Doglas [1 ]
Farina, Ana Paula [2 ]
Galafassi, Daniel [3 ]
Baroni Barbizam, Joao Vicente [4 ]
Milori Corona, Silmara Aparecida [5 ]
Carlini-Junior, Bruno [4 ]
机构
[1] Univ Estadual Campinas, Endodont Div, Dept Restorat Dent, Piracicaba Dent Sch, Piracicaba, SP, Brazil
[2] Univ Estadual Campinas, Prosthodont Div, Dept Restorat Dent, Piracicaba Dent Sch, Piracicaba, SP, Brazil
[3] Univ Sao Paulo, Dept Restorat Dent, Ribeirao Preto Dent Sch, BR-14049 Ribeirao Preto, SP, Brazil
[4] Univ Passo Fundo, Dept Restorat Dent, Sch Dent, Passo Fundo, RS, Brazil
[5] Univ Sao Paulo, Dept Restorat Dent, Sch Dent, BR-14049 Ribeirao Preto, SP, Brazil
关键词
Dentin-bonding agents; EDTA; Sodium hypochlorite; SMEAR LAYER REMOVAL; ENDODONTIC IRRIGANTS; SURFACE-AREA; NAOCL; IRRIGATION; RESISTANCE; FRACTURE; AGENTS; TIME;
D O I
10.1590/S1678-77572010000400011
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Chemical substances used during biomechanical preparation of root canals can alter the composition of dentin surface and affect the interaction with restorative materials. Objective: The purpose of this study was to evaluate the microtensile bond strength (mu TBS) of a self-etching adhesive system to dentin irrigated with sodium hypochlorite (NaOCl) and ethylenediaminetetraacetic acid (EDTA). Material and Methods: Thirty human third molars were sectioned 3 mm below the occlusal surface, polished with 600- to 1200-grit silicon carbide papers, and randomly divided into 3 groups: G1 (control): no irrigating solution; G2: 1% NaOCl; and G3: 1% NaOCl followed by the application of 17% EDTA. The specimens received the self-etching adhesive system (XENO III - Dentsply), restored with microhybrid composite resin (Z250 - 3M ESPE), sectioned and trimmed to create 4 hourglass-shaped slabs of each tooth. The slabs were tested in microtensile strength in a universal testing machine (Emic DL 2000) at a crosshead speed of 0.5 mm/min until fracture. The results were analyzed statistically by ANOVA and Newman-Keuls test. Results: Mean mu TBS values and standard deviations in MPa were: G1 = 11.89 +/- 4.22; G2 = 19.41 +/- 5.32; G3 = 11.34 +/- 4.73. 1% NaOCl increased the adhesive resistance significantly (p<0.001/F = 22.5763). The application of 1% NaOCl/ 17% EDTA resulted in statistically similar mu TBS to the control group. Conclusions: None of the irrigants affected negatively the mu TBS of XENO III to dentin. The use of 1% NaOCl alone resulted in higher bond strength than the other treatments. The combination of 1% NaOCl and 17% EDTA produced similar bond strength to that of untreated dentin.
引用
收藏
页码:385 / 389
页数:5
相关论文
共 50 条
  • [41] Microtensile bond strength of a total-etching versus self-etching adhesive to caries-affected and intact dentin in primary teeth
    Nakornchai, S
    Harnirattisai, C
    Surarit, R
    Thiradilok, S
    JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 2005, 136 (04): : 477 - 483
  • [42] Microtensile dentin bond strength and interface morphology of different self-etching adhesives and universal adhesives applied in self-etching mode
    Fabiao, Amanda de Mello
    Fronza, Bruna Marin
    Andre, Carolina Bosso
    Cavalli, Vanessa
    Giannini, Marcelo
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2021, 35 (07) : 723 - 732
  • [44] Bond strength of composite to dentin using self-etching adhesive systems
    Naughton, WT
    Latta, MA
    QUINTESSENCE INTERNATIONAL, 2005, 36 (04): : 259 - 262
  • [45] Microtensile bond strength and sealing efficiency of all-in-one self-etching adhesives
    Tekce, Neslihan
    Demirci, Mustafa
    Tuncer, Safa
    Uysal, Omer
    BIOTECHNOLOGY & BIOTECHNOLOGICAL EQUIPMENT, 2015, 29 (03) : 570 - 578
  • [46] Shear bond strength of three self-etching adhesive systems.
    Brandt, PD
    De Wet, FA
    van der Vyver, PJ
    Botha, SJ
    JOURNAL OF DENTAL RESEARCH, 2000, 79 (05) : 1311 - 1311
  • [47] Tensile bond strength of self-etching adhesive systems to primary dentin
    Torres, CP
    Ciccone, JC
    Ramos, RP
    Corona, SAM
    Palma-Dibb, RG
    Borsatto, MC
    AMERICAN JOURNAL OF DENTISTRY, 2005, 18 (06): : 327 - 332
  • [48] Mechanical properties and bond strength of self-etching adhesive systems.
    Akimoto, N.
    Ohmori, K.
    Yokoyama, G.
    Cox, C. F.
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : B120 - B120
  • [49] Shear bond strength of a self-etching adhesive in primary and permanent dentition
    Cecilia, CG
    Ballesta, CG
    Lillo, OC
    Lajarín, LP
    AMERICAN JOURNAL OF DENTISTRY, 2005, 18 (05): : 331 - 334
  • [50] Enamel microtensile bond strengths of self-etching primers.
    Mallmann, A
    Perdigäo, J
    Cardoso, PEC
    Burmann, PA
    JOURNAL OF DENTAL RESEARCH, 2000, 79 : 442 - 442