摘要
Mullite/SiC composite ceramics were sintered and subjected to three-point bending of specimens made according to the appropriate JIS standard. A semicircular surface crack 100 to 250 Rm in diameter was made on each specimen. We systematically studied crack-healing behavior and cyclic- and static-fatigue strengths at room temperature and 1000 degreesC (crack-healing temperature) by using three types of specimens (smooth, cracked, and crack-healed). The main conclusions are as follows: (i) mullite/SiC composite ceramics have the ability to heal after cracking; (ii) crack-healed specimens exhibited higher static and fatigue strengths than those of smooth specimens, which was caused by crack-healing; (iii) a sample crack-healed at 1000 degreesC had a high fatigue strength at 1000 degreesC; and (iv) mullite/SiC ceramics can heal a crack under stress at 1000 degreesC, and this behavior was considered using crack-driving force and crack-healing force, qualitatively.
引用
收藏
页码:2073 / 2078
页数:6
相关论文
共 50 条
  • [1] Crack-healing behavior and resultant strength properties of silicon carbide ceramic
    Lee, SK
    Ishida, W
    Lee, SY
    Nam, KW
    Ando, K
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2005, 25 (05) : 569 - 576
  • [2] Self crack-healing behavior under stress of silicon nitride ceramics and resultant strength at the crack-healed temperature
    Takahashi, Koji
    Kim, Byung-Soo
    Chu, Min-Cheol
    Sato, Shigemi
    Ando, Kotoji
    Nippon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A, 2002, 68 (07): : 1063 - 1070
  • [3] Crack-healing behavior of silicon nitride ceramics under cyclic stress and resultant strength at crack-healed temperature
    Takahashi, K
    Ando, K
    Nakayama, S
    Murase, H
    Saito, S
    ADVANCED CERAMICS AND COMPOSITES, 2003, 247 : 275 - 278
  • [4] Crack-healing behavior of Si3N4/SiC ceramics under cyclic stress and resultant fatigue strength at the healing temperature
    Ando, K
    Takahashi, K
    Nakayama, S
    Saito, S
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (09) : 2268 - 2272
  • [5] Crack-healing behavior of liquid-phase-sintered silicon carbide ceramics
    Kim, YW
    Ando, K
    Chu, MC
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2003, 86 (03) : 465 - 470
  • [6] Crack-healing behavior of CVD grown silicon carbide
    Lee, Pete Sihyun
    Lee, Hee-Jun
    Kim, Hyun Mi
    Kim, Seong Hoon
    Park, Jae Hwa
    Shim, Kwang Bo
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2016, 17 (07): : 782 - 788
  • [7] Crack-healing and oxidation behavior of silicon nitride ceramics
    Houjou, K
    Ando, K
    Liu, SP
    Sato, S
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2004, 24 (08) : 2329 - 2338
  • [8] Effect of difference in crack-healing ability on fatigue behavior of alumina/silicon carbide composites
    Sugiyama, Ryo
    Yamane, Kazuya
    Nakao, Wataru
    Takahashi, Koji
    Ando, Kotoji
    JOURNAL OF INTELLIGENT MATERIAL SYSTEMS AND STRUCTURES, 2008, 19 (03) : 411 - 415
  • [9] Crack-healing under cyclic stress and improvement of the resultant fatigue strength of Si3N4/SiC
    Takahashi, Koji
    Ando, Kotoji
    Saito, Shinji
    SCIENCE OF ENGINEERING CERAMICS III, 2006, 317-318 : 453 - 456
  • [10] Crack-healing behavior of Si3N4/SiC ceramics under stress and fatigue strength at the temperature of healing (1000°C)
    Ando, K
    Houjyou, K
    Chu, MC
    Takeshita, S
    Takahashi, K
    Sakamoto, S
    Sato, S
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (08) : 1339 - 1346