Crack-healing behavior of Si3N4/SiC ceramics under cyclic stress and resultant fatigue strength at the healing temperature

被引:76
|
作者
Ando, K
Takahashi, K
Nakayama, S
Saito, S
机构
[1] Yokohama Natl Univ, Dept Energy & Safety Engn, Yokohama, Kanagawa, Japan
[2] Yokohama Natl Univ, Yokohama, Kanagawa, Japan
[3] NHK Spring Co Ltd, Yokohama, Kanagawa, Japan
关键词
Cyclic stresses;
D O I
10.1111/j.1151-2916.2002.tb00446.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Si3N4/SiC composite ceramics were sintered and subjected to three-point bending. A semi-elliptical surface crack of 100 mum surface length was made on each specimen. The crack-healing behavior under cyclic stress of 5 Hz, and resultant cyclic fatigue strengths at healing temperatures of 1100degrees and 1200degreesC, were systematically investigated. The main conclusions are as follows: (1) Si3N4/SiC composite ceramics have an excellent ability to heal a crack at 1100degrees and 1200degreesC. (2) This sample could heal a crack even under cyclic stress at a frequency of 5 Hz. (3) The crack-healed sample exhibited quite high cyclic fatigue strength at each crack-healing temperature, 1100degrees and 1200degreesC.
引用
收藏
页码:2268 / 2272
页数:5
相关论文
共 50 条
  • [1] Threshold stress for crack-healing of Si3N4/SiC and resultant cyclic fatigue strength at the healing temperature
    Takahashi, K
    Ando, K
    Murase, H
    Nakayama, S
    Saito, S
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2005, 88 (03) : 645 - 651
  • [2] Crack-healing under cyclic stress and improvement of the resultant fatigue strength of Si3N4/SiC
    Takahashi, Koji
    Ando, Kotoji
    Saito, Shinji
    SCIENCE OF ENGINEERING CERAMICS III, 2006, 317-318 : 453 - 456
  • [3] Crack-healing behavior of Si3N4/SiC ceramics under stress and fatigue strength at the temperature of healing (1000°C)
    Ando, K
    Houjyou, K
    Chu, MC
    Takeshita, S
    Takahashi, K
    Sakamoto, S
    Sato, S
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (08) : 1339 - 1346
  • [4] Crack-healing behavior under stress and fatigue strength at elevated temperature of crack-healed Si3N4/SiC composite ceramics
    Ando, K
    Houjyou, K
    Chu, MC
    Takahashi, K
    Yao, F
    Sato, S
    EURO CERAMICS VII, PT 1-3, 2002, 206-2 : 819 - 822
  • [5] Crack-healing behavior and static fatigue strength of Si3N4/SiC ceramics held under stress at temperature (800, 900, 1000 °C)
    Takahashi, K
    Kim, BS
    Chu, MC
    Sato, S
    Ando, K
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2003, 23 (11) : 1971 - 1978
  • [6] Effects of frequency on the crack-healing behavior of Si3N4/SiC composite under cyclic stress
    Takahashi, Koji
    Mizobe, Yuuta
    Ando, Kotoji
    Saito, Shinji
    JSME INTERNATIONAL JOURNAL SERIES A-SOLID MECHANICS AND MATERIAL ENGINEERING, 2006, 49 (03) : 307 - 313
  • [7] Effect of crack-healing process on fatigue strength of Si3N4/SiC ceramics at 1000°C
    Hojo, K
    Ando, K
    Chu, MC
    Sato, S
    ADVANCED CERAMICS AND COMPOSITES, 2003, 247 : 271 - 274
  • [8] Crack-healing behaviour and resultant high-temperature fatigue strength of machined Si3N4/SiC composite ceramic
    Jung, Y. -S.
    Guo, Y.
    Nakao, W.
    Takahashi, K.
    Ando, K.
    Saito, S.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2008, 31 (01) : 2 - 11
  • [9] Crack-healing behavior of silicon nitride ceramics under cyclic stress and resultant strength at crack-healed temperature
    Takahashi, K
    Ando, K
    Nakayama, S
    Murase, H
    Saito, S
    ADVANCED CERAMICS AND COMPOSITES, 2003, 247 : 275 - 278
  • [10] Crack-healing behavior under stress of mullite/silicon carbide ceramics and the resultant fatigue strength
    Ando, K
    Furusawa, K
    Chu, MC
    Hanagata, T
    Tuji, K
    Sato, S
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2001, 84 (09) : 2073 - 2078