摘要
Mullite/SiC composite ceramics were sintered and subjected to three-point bending of specimens made according to the appropriate JIS standard. A semicircular surface crack 100 to 250 Rm in diameter was made on each specimen. We systematically studied crack-healing behavior and cyclic- and static-fatigue strengths at room temperature and 1000 degreesC (crack-healing temperature) by using three types of specimens (smooth, cracked, and crack-healed). The main conclusions are as follows: (i) mullite/SiC composite ceramics have the ability to heal after cracking; (ii) crack-healed specimens exhibited higher static and fatigue strengths than those of smooth specimens, which was caused by crack-healing; (iii) a sample crack-healed at 1000 degreesC had a high fatigue strength at 1000 degreesC; and (iv) mullite/SiC ceramics can heal a crack under stress at 1000 degreesC, and this behavior was considered using crack-driving force and crack-healing force, qualitatively.
引用
收藏
页码:2073 / 2078
页数:6
相关论文
共 50 条
  • [41] Crack-healing behaviour and resultant high-temperature fatigue strength of machined Si3N4/SiC composite ceramic
    Jung, Y. -S.
    Guo, Y.
    Nakao, W.
    Takahashi, K.
    Ando, K.
    Saito, S.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2008, 31 (01) : 2 - 11
  • [42] CRACK-HEALING BEHAVIOR AND BENDING STRENGTH PROPERTIES OF SiC CERAMICS BASED ON THE TYPE OF ADDITIVE SiO2 EMPLOYED
    Nam, Ki Woo
    Kim, Jong Soon
    Park, Seung Won
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2010, 24 (15-16): : 2869 - 2874
  • [43] Strength recovery behavior of machined alumina/SiC whisker composite by crack-healing
    Osada, Toshio
    Nakao, Wataru
    Takahashi, Koji
    Ando, Kotoji
    Saito, Shinji
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2007, 115 (1340) : 278 - 284
  • [44] Strength recovery behavior of machined Al2O3/SiC nano-composite ceramics by crack-healing
    Osada, Toshio
    Nakao, Wataru
    Takahashi, Koji
    Ando, Kotoji
    Saito, Shinji
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (10) : 3261 - 3267
  • [45] Critical crack-healing condition for SiC whisker reinforced alumina under stress
    Nakao, W
    Ono, M
    Lee, SK
    Takahashi, K
    Ando, K
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2005, 25 (16) : 3649 - 3655
  • [46] Crack healing behaviour and high-temperature strength of mullite/SiC composite ceramics
    Ando, K
    Chu, MC
    Tsuji, K
    Hirasawa, T
    Kobayashi, Y
    Sato, S
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (08) : 1313 - 1319
  • [47] Gas permeability behavior of mullite-bonded porous silicon carbide ceramics
    Ding, Shuqiang
    Zeng, Yu-Ping
    Jiang, Dongliang
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (17) : 7171 - 7175
  • [48] Gas permeability behavior of mullite-bonded porous silicon carbide ceramics
    Shuqiang Ding
    Yu-Ping Zeng
    Dongliang Jiang
    Journal of Materials Science, 2007, 42 : 7171 - 7175
  • [49] Crack-healing behavior and strength recovery of hot-pressed TZ3Y20A-MoSi2 ceramics
    Zhang, Xiu-Ping
    Ouyang, Jia-Hu
    Liu, Zhan-Guo
    Wang, Yu-Jin
    Wang, Ya-Ming
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 648 : 299 - 304
  • [50] Strength properties of crack-healed silicon-carbide ceramics
    Lee, Sangkee
    Ishida, Wataru
    Ando, Kotoji
    Zairyo/Journal of the Society of Materials Science, Japan, 2003, 52 (06) : 674 - 680