Mode I interlaminar fracture toughness of carbon-epoxy coupons with embedded ceramic sensors

被引:9
|
作者
Torres, Mauricio [1 ]
Tellez, Ricardo A. [2 ]
Hernandez, Hilario [3 ]
Camps, Thierry [4 ]
机构
[1] Natl Council Sci & Technol CONACYT, Ctr Engn & Ind Dev CIDESI, Queretaro, Mexico
[2] Cranfield Univ, Sch Aerosp, Cranfield, Beds, England
[3] Inst Politecn Nacl, ESIME UP Ticoman, Mexico City, DF, Mexico
[4] Univ Fed Toulouse Midi Pyrenees, LAAS, Toulouse, France
关键词
carbon fibers; delamination; fractography; fracture toughness; COMPOSITE STRUCTURES; MONITORING PATCH; PREDICTION; GROWTH; BEHAVIOR;
D O I
10.1002/adv.21905
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
This study analyses the mechanical and crack growth behavior of woven carbon fiber reinforced plastics (CPRF) with embedded ceramic sensors. The material studied here is 3K-70-P carbon fiber plain weave with EPOLAM 2015 (R) epoxy resin. The composite is manufactured with vacuum bagging procedure. Later on, the composite Mode I interlaminar fracture toughness (G(IC)) is calculated by means of double cantilever beam tests (DCB) for two layout configurations [0/90] and [+/- 45] with and without embedded sensors. Results give an initial approach of the fracture behavior of an instrumented composite facing an interlaminar crack. The interlaminar fracture toughness for the instrumented specimens is lower compared to the noninstrumented coupons. The presence of the sensor and its wire connection has a considerable impact on the damage tolerance of the woven composite, where the sensors surroundings seem to be the more likely region to be affected by an interlaminar fracture.
引用
收藏
页码:2294 / 2302
页数:9
相关论文
共 50 条
  • [1] Interlaminar Fracture Characterization of a Carbon-Epoxy Composite in Pure Mode II
    Campilho, R. D. S. G.
    de Moura, M. F. S. F.
    Pinto, A. M. G.
    Ramantani, D. A.
    ADVANCED MATERIALS FORUM V, PT 1 AND 2, 2010, 636-637 : 1518 - +
  • [2] Mode-II interlaminar fracture toughness of carbon/epoxy laminates
    Saidpour, H
    Barikani, M
    Sezen, M
    IRANIAN POLYMER JOURNAL, 2003, 12 (05) : 389 - 400
  • [3] Mode-I interlaminar fracture toughness in unidirectional carbon-fibre/epoxy composites
    Barikani, M
    Saidpour, H
    Sezen, M
    IRANIAN POLYMER JOURNAL, 2002, 11 (06) : 413 - 423
  • [4] Mode I Interlaminar Fracture Toughness of Nylon 66 Nanofibrilmat Interleaved Carbon/Epoxy Laminates
    Hamer, Shay
    Leibovich, Herman
    Green, Anthony
    Intrater, Ron
    Avrahami, Ron
    Zussman, Eyal
    Siegmann, Arnon
    Sherman, Dov
    POLYMER COMPOSITES, 2011, 32 (11) : 1781 - 1789
  • [5] Influence of femtosecond laser treated surfaces on the mode I fracture toughness of carbon-epoxy bonded joints
    Moreira, R. D. F.
    Oliveira, V.
    Silva, F. G. A.
    Vilar, R.
    de Moura, M. F. S. F.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2018, 82 : 108 - 113
  • [6] Mode I interlaminar fracture of carbon/epoxy multidirectional laminates
    Pereira, AB
    de Morais, AB
    COMPOSITES SCIENCE AND TECHNOLOGY, 2004, 64 (13-14) : 2261 - 2270
  • [7] Improvement of Mode I Interlaminar Fracture Toughness of Stitched Glass/Epoxy Composites
    Goektas, D.
    Kennon, W. R.
    Potluri, P.
    APPLIED COMPOSITE MATERIALS, 2017, 24 (02) : 351 - 375
  • [8] Improvement of Mode I Interlaminar Fracture Toughness of Stitched Glass/Epoxy Composites
    D. Göktaş
    W. R. Kennon
    P. Potluri
    Applied Composite Materials, 2017, 24 : 351 - 375
  • [9] Mode I interlaminar fracture toughness of composite
    Jiao, Guiqiong
    Gao, Jian
    Deng, Qiang
    Fuhe Cailiao Xuebao/Acta Materiae Compositae Sinica, 1994, 11 (01): : 113 - 118
  • [10] Effects of loading rates on mode I interlaminar fracture toughness of carbon/epoxy composite toughened by carbon nanotube films
    Li, Zhouyi
    Wang, Yu
    Cao, Junchao
    Meng, Xianghao
    Aamir, Raza Muhammad
    Lu, Weibang
    Suo, Tao
    COMPOSITES PART B-ENGINEERING, 2020, 200