CrC/a-C:H coatings for highly loaded, low friction applications under formulated oil lubrication

被引:26
|
作者
Keunecke, M. [1 ]
Bewilogua, K. [1 ]
Becker, J. [2 ]
Gies, A. [3 ]
Grischke, M. [3 ]
机构
[1] Fraunhofer Inst Surface Engn & Thin Films, D-38108 Braunschweig, Germany
[2] Oerlikon Balzers Coating Germany GmbH, D-55411 Bingen, Germany
[3] OC Oerlikon Balzers AG, FL-9495 Balzers, Liechtenstein
来源
关键词
Sputter; CrC/a-C:H; Friction coefficient; Wear; Oil lubrication; MoDTC additive; C-H COATINGS; DLC COATINGS; WEAR; COMPONENTS; ADDITIVES; TOOLS; FILMS;
D O I
10.1016/j.surfcoat.2012.06.085
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Diamond-like carbon (DLC) coatings, especially amorphous hydrogenated a-C:H and metal containing a-C:H: Me coatings are well established in the automotive industry as standard solutions to eliminate wear problems of highly loaded components due to their outstanding properties in terms of low friction coefficients under dry conditions. Under lubricated conditions the friction can be reduced once more by applying lubricants with special additives. For example the friction modifier MoDTC (molybdenum-dithio-carbamate) is used in many engine oils. Metal free a-C:H coatings were found to interact in a negative way with MoDTC in high concentrations. In order to overcome these problems CrC/a-C:H coatings with different Cr contents were prepared by reactive magnetron sputtering, and tested systematically under lubricated conditions with and without MoDTC. The results were compared with those obtained for pure a-C:H. Hardness and abrasive wear were determined as a function of the Cr content and coating structure. With an increasing Cr content the morphology of the coatings became denser and the surfaces smoother. The hydrogen content in the coatings decreased continuously with increasing Cr contents and reached values close to 3 at% for chromium to carbon (Cr:C) ratios close to 1. Taking into account these hydrogen contents and sub-stoichiometric chromium carbide phases, a nanocomposite-like structure with chromium carbide phases embedded in an a-C:H binder matrix can be assumed. CrC/a-C:H coatings with Cr:C ratios in the range of 1, but having a notable amount of an amorphous a-C:H phase, showed to be an optimum solution under lubricated conditions with MoDTC because they exhibit both low friction and extremely low wear rates. The wear mechanism, especially the interaction with the friction modifier MoDTC will be discussed. (c) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:270 / 278
页数:9
相关论文
共 50 条
  • [41] Evaluation of the friction and wear behavior of a-C:H coatings for lubricant-reduced sheet metal forming
    Reblitz, Jonas
    Zettl, Bastian
    Seynstaahl, Armin
    Orgeldinger, Christian
    Tremmel, Stephan
    Merklein, Marion
    20TH METAL FORMING INTERNATIONAL CONFERENCE, METAL FORMING 2024, 2024, 44 : 663 - 673
  • [42] Diamond-like nanocomposite coatings (a-C:H/a-Si:O) for tribological applications
    Bekaert Corp Rsch Ctr, N.V. Bekaert S.A., Bekaertstraat 2, Zwevegem 8550, Belgium
    Diamond Relat Mater, 2-5 (468-471):
  • [43] Diamond-like nanocomposite coatings (a-C:H/a-Si:O) for tribological applications
    Neerinck, D
    Persoone, P
    Sercu, M
    Goel, A
    Kester, D
    Bray, D
    DIAMOND AND RELATED MATERIALS, 1998, 7 (2-5) : 468 - 471
  • [44] Tribological characteristics of Cr/CrN/a-C:H:W/a-C:H coating under boundary lubrication conditions with glycerol mono-oleate (GMO) and molybdenum dithiocarbamate (MoDTC)
    Kim, Dong-Wook
    Kim, Kyung-Woong
    WEAR, 2015, 342 : 107 - 116
  • [45] Friction and wear behaviour of TiN/Au, TiN/MoS2 and TiN/TiCN/a-C:H coatings
    Ma, KJ
    Chao, CL
    Liu, DS
    Chen, YT
    Shieh, MB
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2002, 127 (02) : 182 - 186
  • [46] Deposition of a-C:H:SiOx Coatings Using Low-Frequency Inductively Coupled Plasma
    Grenadyorov, Alexander S.
    Semenov, Vyacheslav A.
    Oskirko, Vladimir O.
    Oskomov, Konstantin V.
    Solovyev, Andrey A.
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2024, 221 (11):
  • [47] Friction and wear behavior under oil lubrication conditions of amorphous-nanocrystalline composite coatings deposited via HVAS
    Xin, Wei
    Wang, YuJiang
    Wei, ShiCheng
    Liang, Yi
    Xia, XingChuan
    Chen, Xi
    Wang, Bo
    Xu, BinShi
    SURFACE & COATINGS TECHNOLOGY, 2022, 429
  • [48] Structural and environmental dependence of superlow friction in ion vapour-deposited a-C : H : Si films for solid lubrication application
    Chen, Xinchun
    Kato, Takahisa
    Kawaguchi, Masahiro
    Nosaka, Masataka
    Choi, Junho
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2013, 46 (25)
  • [49] Friction reduction of highly-loaded rolling-sliding contacts by surface modifications under elasto-hydrodynamic lubrication
    Bobzin, K.
    Broegelmann, T.
    Stahl, K.
    Michaelis, K.
    Mayer, J.
    Hinterstoisser, M.
    WEAR, 2015, 328 : 217 - 228
  • [50] Exploring the friction mechanism of a-C:H:Si:O film under water-lubricated condition
    Yin, Pingmei
    Dai, Renlong
    Yang, Lei
    Liu, Zhengyu
    Wei, Xubing
    Xu, Yifei
    Cheng, Wangjun
    Sun, Yaoning
    Zhang, Guangan
    DIAMOND AND RELATED MATERIALS, 2025, 154