Fabrication of copper clad aluminum wire(CCAW) by indirect extrusion and drawing

被引:14
|
作者
Kwon, HC
Jung, TK
Lim, SC
Kim, MS
机构
[1] Korea Inst Ind Technol, Inchon 404254, South Korea
[2] Inha Univ, Sch Mat Sci & Engn, Inchon 402751, South Korea
关键词
indirect extrusion; copper clad aluminum wire(CCAW);
D O I
10.4028/www.scientific.net/MSF.449-452.317
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The optimized extrusion conditions from the present research were the extrusion temperature of 573similar to623K and the extrusion ratio(A(0)/A) of 21.39. Above the extrusion temperature of 623K, the fracture of sheath material was observed. It is due to the difference of flow stress between the sheath material and the core material during extrusion process. The bonding strength increased with increasing the extrusion temperature and the extrusion ratio. The bonding strength increased with increasing the annealing temperature. However, over 573K, it decreased abruptly since the thick and brittle intermetallic compounds of larger than 3 mum were formed. The electrical conductivity of copper clad aluminum wire was about 70%IACS without annealing.
引用
收藏
页码:317 / 320
页数:4
相关论文
共 50 条
  • [21] Formation of ultra-fine copper grains in copper-clad aluminum wire
    Sasaki, T. T.
    Morris, R. A.
    Thompson, G. B.
    Syarif, Y.
    Fox, D.
    SCRIPTA MATERIALIA, 2010, 63 (05) : 488 - 491
  • [22] Multi-billet extrusion of aluminum-clad copper alloy rods
    General Research Inst for, Non-ferrous Metals, Beijing, China
    Jixie Gongcheng Xuebao, 4 (107-110):
  • [23] Fabrication of Aluminum Clad Copper Tube by Planet Schrage Walzwerk Process
    Zhang Xiao-li
    Tian Fusheng
    PROGRESS IN MATERIALS AND PROCESSES, PTS 1-3, 2013, 602-604 : 1855 - 1859
  • [24] Drawing lubricants for copper wire drawing
    Hofmann, H.
    Tribologie und Schmierungstechnik, 1600, 56 (02): : 35 - 38
  • [25] FABRICATION OF NB3SN SUPERCONDUCTING WIRE BY THE CLAD-CHIP EXTRUSION METHOD
    SAITO, S
    WACHI, T
    ADACHI, K
    HANADA, S
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1992, 56 (08) : 960 - 964
  • [26] On the production of aluminum clad steel wire
    Song, B.Y.
    Gao, F.
    Dai, H.H.
    Yu, X.
    Zhongguo Jixie Gongcheng/China Mechanical Engineering, 2001, 12 (03):
  • [27] Microstructure of aluminum/copper clad composite fabricated by casting-cold extrusion forming
    Luo Jun-ting
    Zhao Shuang-jing
    Zhang Chun-xiang
    JOURNAL OF CENTRAL SOUTH UNIVERSITY OF TECHNOLOGY, 2011, 18 (04): : 1013 - 1017
  • [28] Microstructure of aluminum/copper clad composite fabricated by casting-cold extrusion forming
    Jun-ting Luo
    Shuang-jing Zhao
    Chun-xiang Zhang
    Journal of Central South University of Technology, 2011, 18 : 1013 - 1017
  • [29] Microstructure of aluminum/copper clad composite fabricated by casting-cold extrusion forming
    骆俊廷
    赵双敬
    张春祥
    Journal of Central South University of Technology, 2011, 18 (04) : 1013 - 1017
  • [30] ALUMINUM EXTRUSION BY THE INDIRECT PROCESS
    不详
    METALLURGIA, 1979, 46 (05): : 362 - 362