Plasma oxidation of bilayered Y/Zr films

被引:0
|
作者
Pranevicius, L. [1 ]
Milcius, D. [2 ]
Pranevicius, L. L. [1 ,2 ]
Orliukas, A. [3 ]
Dudonis, J. [4 ]
Laukaitis, G. [4 ]
机构
[1] Vytautas MAgnus Univ, LT-44404 Kaunas, Lithuania
[2] Lithuanian Energy Inst, LT-44403 Kaunas, Lithuania
[3] Vilnius State Univ, LT-10222 Vilnius, Lithuania
[4] Kaunas Univ Technol, LT-51368 Kaunas, Lithuania
关键词
YSZ films; oxidation; mixing; surface instabilities;
D O I
10.1016/j.ssi.2007.12.038
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The two-layered Y/Zr structures (0.1 mu m thick of Y film on 1.0 mu m thick of Zr film) have been deposited on silicon substrate and oxidized in Ar+O-2 plasma in temperature range 350-800 degrees C simultaneously under irradiation by ions extracted by 100 V bias. The characterization of coating structure was carried out by the X-ray diffraction, The secondary ion mass-spectrometry was used for the recording of depth profiles of the most important elements in film and at interface. The surface topography was monitored by atomic force and scanning electron microscopes. It is shown that the oxidation kinetics in complex way depends on parameters of irradiation and temperature. The homogeneous nanocrystalline YSZ films have been obtained after plasma oxidation for temperatures higher than 450 degrees C and ion current density 1 ma.cm(-2). The atomic mixing and oxidation mechanisms are discussed. The emphasis is made on the analysis of surface instabilities acting as possible driving force for the intermixing and restructuring of Y/Zr layers. (c) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:104 / 107
页数:4
相关论文
共 50 条
  • [41] Transition from internal to external oxidation in binary Ni-Zr and ternary Ni-Zr-Y alloys
    Fuhrmann, L.
    Konrad, C. H.
    Voelkl, R.
    Glatzel, U.
    CORROSION SCIENCE, 2015, 94 : 218 - 223
  • [42] Diffusion barrier performance of Zr-N/Zr bilayered film in Cu/Si contact system
    Wang, Ying
    Cao, Fei
    Ding, Ming-hui
    Liu, Yun-tao
    MICROELECTRONICS RELIABILITY, 2008, 48 (11-12) : 1800 - 1803
  • [43] Surface morphology, corrosion resistance and in vitro bioactivity of P containing ZrO2 films formed on Zr by plasma electrolytic oxidation
    Sandhyarani, M.
    Rameshbabu, N.
    Venkateswarlu, K.
    Sreekanth, D.
    Subrahmanyam, Ch
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 553 : 324 - 332
  • [44] Investigation of the hydrogenation properties of Zr films under unclean plasma conditions
    Shi, LQ
    Yan, GQ
    Zhou, JY
    Luo, SZ
    Peng, SM
    Ding, W
    Long, XG
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 2002, 20 (06): : 1840 - 1845
  • [45] Hydrogenation properties of Zr films under various conditions of hydrogen plasma
    Yan, GQ
    Shi, LQ
    Zhou, ZY
    Zhao, GQ
    Hu, PG
    Luo, SZ
    Peng, SM
    Ding, W
    Long, XG
    CHINESE PHYSICS LETTERS, 2002, 19 (06) : 775 - 778
  • [46] Isothermal Oxidation Behavior of Ternary Zr-Nb-Y Alloys at High Temperature
    Prajitno, Djoko Hadi
    Soepriyanto, Syoni
    Basuki, Eddy Agus
    Wiryolukito, Slameto
    4TH INTERNATIONAL CONFERENCE ON MATHEMATICS AND NATURAL SCIENCES (ICMNS 2012)L: SCIENCE FOR HEALTH, FOOD AND SUSTAINABLE ENERGY, 2014, 1589 : 182 - 186
  • [47] Fast internal oxidation of Ni-Zr-Y alloys at low oxygen pressure
    Kloss, B
    Wenderoth, M
    Glatzel, U
    Völkl, R
    OXIDATION OF METALS, 2004, 61 (3-4): : 239 - 251
  • [48] Enhanced electrical properties in bilayered ferroelectric thin films
    ZHANG Hao
    LONG WeiJie
    CHEN YaQing
    GUO DongJie
    Science China(Physics,Mechanics & Astronomy), 2013, Mechanics & Astronomy)2013 (03) : 551 - 555
  • [49] Plastic and elastic behavior of sputtered bilayered films by nanoindedtation
    Kikuchi, N
    Kusano, E
    Sawahira, Y
    Kinbara, A
    THIN FILMS-STRESSES AND MECHANICAL PROPERTIES VIII, 2000, 594 : 513 - 518
  • [50] Bilayered Pb(Zr,Ti)O3/(Bi,Nd)4Ti3O12 thin films
    Sim, Chow Hong
    Sen Gao, Xing
    Zhou, Zhao Hui
    Wang, John
    JOURNAL OF ELECTROCERAMICS, 2006, 16 (04) : 459 - 462