Post examination of tungsten monoblocks subjected to high heat flux tests of ITER full-tungsten divertor qualification program

被引:37
|
作者
Sun, Zhaoxuan [1 ,2 ]
Li, Qiang [1 ]
Wang, Wanjing [1 ]
Wang, Ji-Chao [1 ,2 ]
Wang, Xingli [1 ,2 ]
Wei, Ran [1 ,2 ]
Xie, Chunyi [1 ]
Luo, Guang-nan [1 ,2 ,3 ,4 ]
Hirai, T. [5 ]
Escourbiac, F. [5 ]
Panayotis, S. [5 ]
机构
[1] Chinese Acad Sci, Inst Plasma Phys, Hefei 230031, Anhui, Peoples R China
[2] Univ Sci & Technol China, Grad Sch, Sci Isl Branch, Hefei 230031, Anhui, Peoples R China
[3] Hefei Ctr Phys Sci & Technol, Hefei 230022, Anhui, Peoples R China
[4] Chinese Acad Sci, Hefei Sci Ctr, Hefei 230027, Anhui, Peoples R China
[5] ITER Org, Route Vinon Sur Verdon,CS 90 046, F-13067 St Paul Les Durance, France
基金
中国国家自然科学基金;
关键词
ITER; Tungsten; Divertor; High heat flux; Monoblock; MOCK-UPS;
D O I
10.1016/j.fusengdes.2017.06.009
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
In 2015, as part of ITER Full-Tungsten Divertor Qualification Program, Institute of Plasma Physics Chinese Academy of Sciences (ASIPP) manufactured six small-scale Tungsten (W) monoblock mock-ups that were tested at the electron beam facility, ITER Divertor Test Facility (IDTF, St Petersburg, RF). The high heat flux (HHF) tests consisted of 5000 cycles at 10 MW/m(2), followed by 300 cycles at 20 MW/m(2) and additional 700 cycles at 20 MW/m(2). All mock-ups fulfilled the requirements of high heat flux performance successfully. One (WTC-5) of the six mock-ups was then selected to carry out critical heat flux (CHF) test with local heat flux up to 37-39 MW/m(2). After HHF test, ultrasonic test (UT) and destructive tests were performed to characterize the damages of monoblocks. The debonding of the Cu/CuCrZr interface was detected by both nondestructive and destructive tests. Intergranular rupture of W was observed by Scanning Electron Microscope (SEM). The recrystallization was found in the W monoblocks and the recrystallized depth were analyzed by metallography and Vickers hardness measurement. (C) 2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:60 / 69
页数:10
相关论文
共 49 条
  • [31] Manufacturing and High Heat Flux Testing of Tungsten-Brazed Mock-Ups for KSTAR Divertor
    Kim, K. M.
    Kim, H. T.
    Song, J. H.
    Kim, H. K.
    Park, S. H.
    Hong, S. H.
    Kim, B. C.
    Yang, H. L.
    Kim, Y. S.
    You, S. Y.
    IEEE TRANSACTIONS ON PLASMA SCIENCE, 2017, 45 (03) : 519 - 522
  • [32] Study on melting and solidification behaviors of tungsten loaded by high heat flux for divertor in tokamak fusion reactor
    Hoashi, Eiji
    Kuroyanagi, Shinpei
    Okita, Takafumi
    Maeji, Takeru
    Ibano, Kenzo
    Ueda, Yoshio
    FUSION ENGINEERING AND DESIGN, 2018, 136 : 350 - 356
  • [33] Ultrasonic analysis of tungsten monoblock divertor mock-ups after high heat flux test
    Dose, Giacomo
    Roccella, Selanna
    Richou, Marianne
    Gallay, Franklin
    Visca, Eliseo
    Greuner, Henri
    Romanelli, Francesco
    Hunger, Katja
    Barrett, Tom
    You, Jeong-Ha
    FUSION ENGINEERING AND DESIGN, 2019, 146 : 870 - 873
  • [34] High heat flux test of CVD-tungsten coated Cu heat sink divertor mock-up
    Sato, K
    Nakamura, K
    Suzuki, S
    Araki, M
    Dairaku, M
    Yokoyama, K
    Akiba, M
    FUSION TECHNOLOGY, 1996, 30 (03): : 769 - 773
  • [35] First thermal fatigue studies of tungsten armor for DEMO and ITER at the OLMAT High Heat Flux facility
    Alegre, D.
    Tafalla, D.
    De Castro, A.
    Gonzalez, M.
    Manchon, J. G.
    Tabares, F. L.
    Hernandez, T.
    Wirtz, M.
    Coenen, J. W.
    Mao, Y.
    Oyarzabal, E.
    NUCLEAR MATERIALS AND ENERGY, 2024, 38
  • [36] Comparative study of ITER conform tungsten grades exposed to high heat flux and neutron irradiation damage
    Terentyev, D.
    Wirtz, M.
    Morgan, T. W.
    Nozawa, T.
    Zinovev, A.
    Chang, C. C.
    Poleshchuk, K.
    Elenbaas, J.
    FUSION ENGINEERING AND DESIGN, 2024, 200
  • [37] High heat flux test of actively cooled tungsten-coated carbon divertor mock-ups
    Tokunaga, K
    Yoshida, N
    Kubota, Y
    Noda, N
    Imamura, Y
    Oku, T
    Kurumada, A
    Sogabe, T
    Kato, T
    Plöchl, L
    FUSION ENGINEERING AND DESIGN, 2000, 49-50 : 371 - 376
  • [38] Potential approach of IR-analysis for high heat flux quality assessment of divertor tungsten monoblock components
    Greuner, Henri
    Boeswirth, B.
    Maier, H.
    Hirai, T.
    Panayotis, S.
    Crescenzi, F.
    Roccella, S.
    Visca, E.
    Missirlian, M.
    Richou, M.
    FUSION ENGINEERING AND DESIGN, 2017, 124 : 202 - 206
  • [39] Manufacturing and high heat flux loading of tungsten coatings on fine grain graphite for the ASDEX-Upgrade divertor
    Deschka, S
    GarciaRosales, C
    Hohenauer, W
    Duwe, R
    Gauthier, E
    Linke, J
    Lochter, M
    Mallener, W
    Plochl, L
    Rodhammer, P
    Salito, A
    JOURNAL OF NUCLEAR MATERIALS, 1996, 233 : 645 - 649
  • [40] Observation of surface deformation of tungsten exposed to single pulsed high heat flux and magnetic field for divertor design
    Okita, Takafumi
    Matsuda, Yuki
    Saito, Sho
    Hoashi, Eiji
    Ibano, Kenzo
    Ueda, Yoshio
    FUSION ENGINEERING AND DESIGN, 2021, 171